Efficiency evaluation of the composition for low-temperature filling of sulfuric acid anodic-oxide coating and methods of its alternative application
Zakharov К.Е., Fomina M.A., Vdovin A.I., Chumakova E.S. Efficiency evaluation of the composition for low-temperature filling of sulfuric acid anodic-oxide coating and methods of its alternative application // Proceedings of VIAM. 2025. No. 4. DOI: 10.18577/2307-6046-2025-0-4-81-95. URL: https://viam-works.ru/en/journal/2025/4/7
Keywords
anodic-oxide coatings, filling, corrosion protection, corrosion inhibitors
Abstract
The most known method of protection against corrosion of aluminum and its alloys is sulfuric acid anodic oxidation. The oxidized surface has a significant ability to resist aggressive external factors, high adhesion properties. However, the coating requires an additional treatment consisting of soaking in hot solutions, called filling. The article presents the results of research aimed at the development of the composition and a new method of filling anodic-oxide coating, the possibility of using this composition as a corrosion inhibitor is evaluated.
Reference list
- Kablov E.N. Main directions of development of materials for aerospace engineering of the XXI century. Perspektivnye materialy, 2000, no. 3, pp. 27–36.
- Kablov E.N., Petrova A.P., Narsky A.R. Alexey Tikhonovich Tumanov – the founder of new scientific directions in materials science. Vse materialy. Entsiklopedicheskiy spravochnik, 2009, no. 1, pp. 2–5.
- Kablov E.N. Chemistry in aviation materials science. Rossiyskiy khimicheskiy zhurnal, 2010, vol. LIV, no. 1, pp. 3–4.
- Duyunova V.A., Leonov A.A., Molodtsov S.V. VIAM's contribution to the development of light alloys and the corrosion control of rocket and space technology products. Trudy VIAM, 2020, no. 2 (86), paper no. 03. Available at: http://www.viam-works.ru (accessed: March 22, 2024). DOI: 10.18577/2307-6046-2020-0-2-22-30.
- Duyunova V.A., Kozlov I.A., Oglodkov M.S., Kozlova A.A. Modern trends in the anodic oxidation of aluminum-lithium and aluminum alloys (review). Trudy VIAM, 2019, no. 8 (80), paper no. 09. Available at: http://www.viam-works.ru (accessed: March 22, 2024). DOI: 10.18577/2307-6046-2019-0-8-79-89.
- Kablov E.N. Quality control of materials – a guarantee of safety of operation of aviation equipment. Aviacionnye materialy i tehnologii, 2001, no. 1, pp. 3–8.
- Fomina M.A., Volkov I.A., Vdovin A.I., Yamshchikov E.I. Study of protective capacity anodic oxide coating with environmental friendly improved filling technology. Aviation materials and technologies, 2023, no. 4 (73), paper no. 10. Available at: http://www.journal.viam.ru (accessed: January 15, 2024). DOI: 10.18577/2713-0193-2023-0-4-101-110.
- Vinogradov S.S., Nikiforov A.A., Zakirova L.I. Cadmium replacement. Stage 2 – final. Galvanic thermal coating of zinc–tin system – real alternative to cadmium plating. Aviacionnye materialy i tehnologii, 2019, no. 3 (56), pp. 59–66. DOI: 10.18577/2071-9140-2019-0-3-59-66.
- Polyakova M.A., Mustafina V.G. Theory of corrosion and methods of corrosion protection: textbook. Magnitogorsk, 2008, 139 p.
- Agafonkina M.O., Andreeva N.P., Kuznetsov Yu.I., Timashev S.F. Substituted benzotriazoles ‒ copper corrosion inhibitors in a buffered borate corrosion solution. Zhurnal fizicheskoy khimii, 2017, vol. 91, no. 8, pp. 1294–1301.
- Solop G.R. Development and application of corrosion inhibitors based on petrochemical products: thesis abstract, Cand. Sc. (Tech.). Ufa, 2016, 24 p.
- Gazizova E.I., Bondar M.A. Efficiency of organic compounds as corrosion inhibitors. Actual problems of corrosion protection of oil and gas equipment and pipelines (Corrosion–2023): collection of materials of the I Int. scientific and technical. conf., dedicated to the 75th anniversary of the Federal State Budgetary Educational Institution of Higher Education «USPTU». Ufa, 2023, pp. 25–26.
- Posunko I.A. Technology of creating atmospheric corrosion inhibitors. Scientific research: theory, methodology and practice: collection of materials of the II Int. scientific and practical. conf. Cheboksary, 2017, pp. 149–156.
- Kadnikova O.Yu., Toretaev M.O., Akmalova O.A., Nurmukhambetova B.T., Kozhabergenova K.D. Development of environmentally friendly corrosion inhibitors for the protection of textile equipment. Vestnik Almatinskogo tekhnologicheskogo universiteta, 2020, no. 4, pp. 38–46.
- Mukhametzyanov M.I., Shakirova A.I. Study of corrosion of aluminum alloys and possible methods of their protection. Modern technologies in the oil and gas industry – 2016: collection of works. International scientific and technical conf., dedicated to the 60th anniversary of the branch. Ufa, 2016, pp. 475–482.
- Abramova M.G. Full-scale accelerated tests of aluminum alloys at continental and marine type stations. Aviacionnye materialy i tehnologii, 2020, no. 3 (60), pp. 57–65. DOI: 10.18577/2071-9140-2020-0-3-57-65.
- Vetrova E.Yu., Shchekin V.K., Kurs M.G. Comparative evaluation of methods for the determination of corrosion aggressivity of the atmosphere. Aviacionnye materialy i tehnologii, 2019, no. 1 (54), pp. 74–81. DOI: 10.18577/2071-9140-2019-0-1-74-81.
- Kablov E.N., Antipov V.V., Chesnokov D.V., Kutyrev A.E. Application of Al–Mg–Si–Cu system aluminum alloy combined anodic dissolution for prognosis of tensile strength loss during natural exposure testing. Aviacionnye materialy i tehnologii, 2020, no. 2 (59), pp. 63–73. DOI: 10.18577/2071-9140-2020-0-2-63-73.
- Antipov V.V., Medvedev I.M., Kutyrev A.E., Volkov I.A. Rapid assessment of hot water sealed anodic oxide coatings protective properties during NaCl immersion testing. Trudy VIAM, 2019, no. 8 (80), paper no. 08. Available at: http://www.viam-works.ru (accessed: October 15, 2020). DOI: 10.18577/2307-6046-2018-0-9-71-82.
- Duyunova V.A., Kutyrev A.E., Serebrennikova N.Yu., Vdovin A.I., Somov A.V. Examination of the impact of aggressive environmental factors on the development of corrosion damage on samples of laminated glass-reinforced plastic of SIAL class. Aviation materials and technologies, 2021, no. 4 (65), paper no. 09. Available at: http://www.journal.viam.ru (accessed: January 15, 2024). DOI: 10.18577/2713-0193-2021-0-4-81-90.