Study of cured hot melt adhesive epoxy binders by sclero- and microhardness methods
Salakhova R.K., Veshkin E.A, Apalkova A.V., Simirgina N.D. Study of cured hot melt adhesive epoxy binders by sclero- and microhardness methods // Proceedings of VIAM. 2025. No. 12. DOI: 10.18577/2307-6046-2025-0-12-12-24. URL: https://viam-works.ru/en/journal/2025/12/2
Keywords
hot melt adhesives, floor panel sheetings, microhardness, sclerometry, scratch resistance force, degree of curing, degree of conversion, volumetric anisotropy coefficient
Abstract
The results of cross-sectional microhardness measurements grade binders (compositions I–VII) are presented. Volumetric anisotropy coefficients are calculated, and the correlation between polymer matrix microhardness and the indenter scratch resistance parameter is studied. A comparative analysis of microhardness changes in the height direction of the samples and sclerograms obtained using an ST-01 laboratory scratch tester is conducted. For the low-flammability hot melt adhesive binder (composition VII), the optimal two-stage curing mode is selected, and the degree of polymer conversion is determined.
Reference list
- Kablov E.N. New Generation Materials – the Basis for Innovation, Technological Leadership, and National Security of Russia. Intellekt i tekhnologii, 2016, no. 2 (14), pp. 16–21.
- Kablov E.N. Science as a Branch of the Economy. Nauka i zhizn, 2009, no. 10, pp. 6–10.
- Kablov E.N. Composites: Today and Tomorrow. Metally Evrazii, 2015, no. 1, pp. 36–39.
- Startsev V.O., Antipov V.V., Slavin A.V., Gorbovets M.A. Modern domestic polymer composite materials for aviation industry (review). Aviation materials and technologies, 2023, no. 2 (71), paper no. 10. Available at: http://www.journal.viam.ru (accessed: September 23, 2025). DOI: 10.18577/2713-0193-2023-0-2-122-144.
- Mishkin S.I. Application of carbon fiber plastics in constructions of pilotless devices (review). Trudy VIAM, 2022, no. 5 (111), paper no. 08. Available at: http://www.viam-works.ru (accessed: September 30, 2025). DOI: 10.18577/2307-6046-2022-0-5-87-95.
- Raskutin A.E. Development strategy of polymer composite materials. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 344–348. DOI: 10.18577/2071-9140-2017-0-S-344-348.
- Isaev A.Yu., Rubtsova E.V., Kotova E.V., Sutyagin M.N. Research of properties of glues and glue binding, made with use of modern domestic component base. Trudy VIAM, 2021, no. 3 (97), paper no. 05. Available at: http://www.viam-works.ru (accessed: April 09, 2025). DOI: 10.18577/2307-6046-2021-0-3-58-67.
- Kutsevich K.E., Dementeva L.A., Lukina N.F., Tyumeneva T.Yu. Adhesive prepregs as promising materials for parts and assemblies from polymeric composite materials. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 379–387. DOI: 10.18577/2071-9140-2017-0-S-379-387.
- Chursova L.V., Tsybin A.I., Grebeneva T.A. Binders for polymer composite and functional materials. Previous experience, current status and development prospects. Novosti materialovedeniya. Nauka i tekhnika, 2017, no. 2 (26), pp. 34–46. Available at: http://www.materialsnews.ru (accessed: April 09, 2025).
- Sopotov R.I., Gorbunova I.Yu., Onuchin D.V. et al. Effect of polysulfone and polyethersulfone modifiers on the thermomechanical properties of epoxyamine binder. Uspekhi v khimii i khimicheskoy tekhnologii, 2015, vol. 29, no. 10, pp. 62–64.
- Kablov E.N., Chursova L.V., Babin A.N. et al. Developments of FSUE VIAM in the field of melt binders for polymer composite materials. Polimernye materialy i tekhnologii, 2016, vol. 2, no. 2, pp. 37–42.
- Kopitsyna M.N., Bessonov I.V., Kotomin S.V. Crack resistance of epoxy binders modified with thermoplastic polysulfone and furfural acetone resin. Inzhenernyy zhurnal: nauka i innovatsii, 2016, no. 12, pp. 1–9.
- Khasbulatova Z.S. Aromatic polysulfones. Plasticheskiye massy, 2009, no. 4, pp. 20–23.
- Kostromina N.V., Olikhova Yu.V., Malakhovsky S.S., Gorbunova I.Yu. Development of epoxy binders modified with heat-resistant thermoplastics for the creation of reinforced composite materials. Plasticheskiye massy, 2022, no. 9–10, pp. 17–19.
- Borodulin A.S. Plasticizers for epoxy adhesives and binders. Klei. Germetiki. Tekhnologii, 2012, no. 7, pp. 31–35.
- Malysheva G.V., Marakhovskiy P.S., Barinov D.Ya., Nikolaev E.V. Optimization of the curing modes of fiber-glass based on epoxy binder. Aviation materials and technologies, 2023, no. 2 (71), paper no. 08. Available at: http://www.journal.viam.ru (accessed: October 06, 2025). DOI: 10.18577/2713-0193-2023-0-2-94-103.
- Bolshakov V.A., Antyufeeva N.V. Evaluation of the curing process model of the adhesive binder in prepreg. Aviation materials and technologies, 2023, no. 4 (73), paper no. 07. Available at: http://www.journal.viam.ru (accessed: October 08, 2025). DOI: 10.18577/2713-0193-2023-0-4-66-77.
- Medvedeva K.A., Cherezova E.N. Study of new aminophenolic compounds as hardeners for epoxy oligomers. Fundamentalnye issledovaniya, 2013, no. 6, part 5, pp. 1085–1088.
- Semenychev V.V., Salakhova R.K. Device for assessing coating properties. Zavodskaya laboratoriya. Diagnostika materialov, 2017, vol. 83, no. 2, pp. 60–65.
- Salakhova R.K., Kirilin S.G., Tikhoobrazov A.B., Smirnova T.B. Scratch testing of electrolytic nickel coatings on a carbon fiber substrate. Vestnik Samarskogo universiteta. Aerokosmicheskaya tekhnika, tekhnologii i mashinostroyenie, 2021, vol. 20, no. 4, pp. 100–114.
- Zabolotnov A.S., Gostev S.S., Maklakova I.A. et al. Influence of Crystalline Structure on a Set of Physicomechanical Characteristics of Composite Materials Based on Ultra-High Molecular Weight Polyethylene. Vysokomolekulyarnye soyedineniya. Ser.: B, 2023, vol. 65, no. 5, pp. 341–346.
- Matveeva L.Yu., Yastrebinskaya A.V. Relationship between Supramolecular Structure and Properties of Polymer Composite Materials Based on Thermosetting Binders. Vestnik BGTU im. V.G. Shukhova, 2017, no. 12, pp. 49–54.
- Veshkin E.A., Slavin A.V., Postnova M.V., Apalkova A.V. The role of temperature-time curing conditions in the formation of unidirectional and equally strong carbon fiber plastics properties. Aviation materials and technologies, 2025, no. 2 (79), paper no. 05. Available at: http://www.journal.viam.ru (accessed: October 16, 2025). DOI: 10.18577/2713-0193-2025-0-2-59-71.