Perspective reinforcing high-temperature fibres for metal and ceramic composite materials
Kablov E.N., Schetanov B. V., Ivakhnenko Yu.A., Balinova Yu.A. Perspective reinforcing high-temperature fibres for metal and ceramic composite materials // Proceedings of VIAM. 2013. No. 2. URL: https://viam-works.ru/en/journal/2013/2/5
Abstract
Current state of production and prospect of application reinforcing fibers for metal and ceramic composite materials (CM) are considered. Properties of various matrix composites and fibers for each type of CM are described. Fields of application of ceramic and metal composites are given.