Investigation of electroplating of corrosion-resistant steels to prevent contact corrosion
Zakirova L.I., Sibileva S.V., Dyomin S.A., Duyunova V.A. Investigation of electroplating of corrosion-resistant steels to prevent contact corrosion // Proceedings of VIAM. 2024. No. 9. DOI: 10.18577/2307-6046-2024-0-9-42-53. URL: https://viam-works.ru/en/journal/2024/9/5
Keywords
aluminum alloy, electroplating, electrodeposition, zinc coating, cadmium coating, alloy coating, galvanothermal coating, accelerated corrosion tests, structurally similar sample.
Abstract
Electroplating coatings of corrosion-resistant steels have been studied to prevent contact corrosion of aluminum alloys: methods of surface preparation have been selected, optimal modes of coating application and heat treatment have been determined. Based on the results of accelerated corrosion tests of structurally similar samples in the salt mist chamber, galvanic coatings of corrosion-resistant steels with high protective ability under conditions of occurrence of a corrosion-resistant steel/aluminum contact pair were determined.
Reference list
- Kablov E.N., Kutyrev A.E., Vdovin A.I., Kozlov I.A., Afanasyev-Khodykin A.N. The research of possibility of galvanic corrosion in brazed connections used in aviation engine construction. Aviation materials and technologies, 2021, no. 4 (65), paper no. 01. Available at: http://www.journal.viam.ru (accessed: July 09, 2024). DOI: 10.18577/2713-0193-2021-0-4-3-13.
- Illarionov E.I., Kolobnev N.I., Gorbunov P.Z., Kablov E.N. Aluminum alloys in aerospace engineering. Ed. E.N. Kablov. Moscow: Nauka, 2001, 192 p.
- Kablov E.N., Antipov V.V., Girsh R.I., Serebrennikova N.Yu., Konovalov A.N. Constructed layered materials based on sheets of aluminum-lithium alloys and fiberglass in the structures of new generation aircraft. Vestnik mashinostroeniya, 2020, no. 12, pp. 46–52.
- Kablov E.N., Antipov V.V., Oglodkova Yu.S., Oglodkov M.S. Experience and prospects for the use of aluminum-lithium alloys in aviation and space technology. Metallurg, 2021, no. 1, pp. 62–70.
- Kablov E.N., Antipov V.V., Chesnokov D.V., Kutyrev A.E. Application of Al–Mg–Si–Cu system aluminum alloy combined anodic dissolution for prognosis of tensile strength loss during natural exposure testing. Aviacionnye materialy i tehnologii, 2020, no. 2 (59), pp. 63–73. DOI: 10.18577/2071-9140-2020-0-2-63-73.
- Sinyavskiy V.S., Kalinin V.D. Corrosion durability of aluminum alloys and corrosion-resistant steels in substructures of ventilated facades. Stroyprofil, 2011, no. 6, pp. 27–28.
- Zhirnov A.D., Karimova S.A., Golovina V.M. Corrosion resistance and protection of aluminum alloys in building structures. Stroyprofil, 2010, no. 2, pp. 30–31.
- Stogniy G.V. Prospects for studying contact corrosion of metals in modern shipbuilding and shipbuilding. Vodnyy transport, 2013, no. 2, pp. 43–51.
- GOST 9.005–72. Unified system of protection against corrosion and aging. Metals, alloys, metallic and non-metallic inorganic coatings. Permissible and unacceptable contacts with metals and non-metals. Moscow: Standartinform, 2008, 28 p.
- Navinsek B., Panjan P., Milosev I. PVD coatings as an environmentally clean alternative to electroplating and electroless processes. Surface and Coatings Technology, 1999, vol. 116–119, pp. 476–487.
- The Sigal process for electrodeposition of aluminium. Anti-Corrosion Methods and Materials. MCB UP Ltd, 1985, vol. 32, no. 7, р. 13. DOI: 10.1108/eb020360.
- Enders B., KrauB S., Wolf G.K. Corrosion properties of aluminum based alloys deposited by ion beam assisted deposition. Surface and Coatings Technology, 1994, vol. 65, pp. 203–207.
- Jianming X., Weijianga Z., Wolf G.K. The corrosion properties of Al/Al2O3 multilayered coatings on CK45 steel deposited by IBAD. Surface and Coatings Technology, 2004, vol. 187, pp. 194–198.
- Matys V.G., Poplavsky V.V. Resistance of aluminum and its alloy to contact corrosion in galvanic couples with steels with metallic coatings. Trudy BGTU: Khimiya i tekhnologiya neorganicheskikh veshchestv, 2015, no. 3, pp. 85–92.
- Vyacheslavov P.M. Electrolytic deposition of alloys. Leningrad: Mashinostroenie, 1977, 34 p.
- Averkin V.A. Electrolytic deposition of alloys. Moscow: Mashgiz, 1961, 120 p.
- Kudryavtsev N.T. Electrolytic coatings with metals. Moscow: Khimiya, 1979, 352 p.
- Zakirova L.I., Laptev A.B. Properties of protective electroplating coatings for replacement of cadmium on steel fixing parts (review). Part 1. Morphology and corrosion resistance. Aviaсionnye materialy i tehnologii, 2020, no. 3 (60), pp. 37–46. DOI: 10.18577/2071-9140-2020-0-3-37-46.
- Laptev A.B., Zakirova L.I., Degovets M.L. Properties of protective galvanic coatings for replacement of cadmium on steel fixing parts (review). Part 2. Hydrogen embrittlement and frictional characteristics. Aviacionnye materialy i tehnologii, 2020, no. 4 (61), pp. 35–40. DOI: 10.18577/2071-9140-2020-0-4-35-40.
- Kablov E.N., Nikiforov A.A., Demin S.A., Chesnokov D.V., Vinogradov S.S. Promising coatings for corrosion protection of carbon steels. Stal, 2016, no. 6, pp. 70–81.
- Vinogradov S.S., Nikiforov A.A., Zakirova L.I. Cadmium replacement. Stage 2 – final. Galvanic thermal coating of zinc–tin system – real alternative to cadmium plating. Aviacionnye materialy i tehnologii, 2019, no. 3 (56), pp. 59–66. DOI: 10.18577/2071-9140-2019-0-3-59-66.
- Method for preparing the surface of articles made of easily oxidized metals: pat. 368762 Japan; appl. 26.08.70; publ. 26.01.73.
- State Standard 9.305–84. Unified system of protection against corrosion and aging. Metallic and non-metallic inorganic coatings. Operations of technological processes for obtaining coatings. Moscow: Publ. House of Standards, 2003, 105 p.
- Method for preparing the surface of stainless steel articles before galvanic nickel plating: pat. 2201478 Rus. Federation; appl. 18.02.00; publ. 27.03.03.
- Davlatyan T.A., Konarev A.A., Kruglov V.S. et al. Electrodeposition of copper on composite tapes «silver-stainless steel». Coatings and surface treatment: Abstracts of reports. 10th Int. Conf. Moscow, 2013, pp. 30–31.
- Method of surface preparation of stainless steel products before galvanic copper plating: patent. 2549037 Rus. Federation; appl. 03.07.13; publ. 20.04.15.
- State Standard 9.402–2004. Unified system of corrosion and aging protection. Paint and varnish coatings. Preparation of metal surfaces for painting. Moscow: Standartinform, 2006, 43 p.
- State Standard 9.302–88. Unified system of corrosion and aging protection (USCAP). Metallic and non-metallic inorganic coatings. Control methods. Moscow: Publ. House of Standards, 2001, 40 p.
- State Standard 9.308–85. Unified System of Protection against Corrosion and Aging (USPA). Metallic and non-metallic inorganic coatings. Methods of accelerated corrosion testing. Moscow: Publ. House of Standards, 1990, 21 p.