Abstract

The development of modern equipment, in particular aviation, allows creation of new composite materials on the basis of the traditional materials used in different designs. Analysis of such constructional materials on the basis of metal composite materials with a hybrid reinforcing of fibers allows to make a conclusion about corrosion attacks on the boundary of metal-fiber, which is the cathode in relation to alloys, which can result in the conditions of corrosive environment to the destruction of the composite material. Schemes for providing surface protection of metal composite materials are chosen.

Reference list
  1. Kondrashov E.K., Kuznetsova V.A., Semenova L.V., Lebedeva T.A., Malova N.E. Razvitie aviatsionnyh lakokrasochnyh materialov [Development of aircraft lacquer-and-paint coatings] //Vse materialy. Entsiklopedicheskiy spravochnik. 2012. №5. S. 49–54.
  2. Kablov E.N. Sovremennye materialy – osnova innovatsionnoy modernizatsii Rossii [Modern materials – the basis for innovative modernization of Russia] //Metally Evrazii. 2012. №3. S. 10–15.
  3. Graschenkov D.V., Chursova L.V. Strategiya razvitiya kompozitsionnyh i funktsional'nyh materialov [Development strategy of composite and functional materials] //Aviatsionnye materialy i tehnologii. 2012. №S. S. 231–242.
  4. Kablov E.N., Schetanov B.V., Ivahnenko Yu.A., Balinova Yu.A. Perspektivnye armiruyuschie vysokotemperaturnye volokna dlya metallicheskih i keramicheskih kompozitsionnyh materialov [Advanced high-temperature reinforcing fibers for metal and ceramic composite materials] //Trudy VIAM. 2013. №2 (elektronnyj zhurnal).
  5. Migunov V.P., Farafonov D.P., Degovets M.L. Poristovoloknistyj material sverhnizkoy plotnosti na osnove metallicheskih volokon [Superlow-density porous-fibrous material based on metallic fibers] //Aviatsionnye materialy i tehnologii. 2012. №4. S. 38–41.
  6. Chebotarevskiy V.V., Kondrashov E.K. Tehnologiya lakokrasochnyh pokrytiy v mashinostroenii [Technology of lacquer-and-paint coatings in the mechanical engineering]. M.: Mashinostroenie. 1978. 295 s.
  7. Kablov E.N. Strategicheskie napravleniya razvitiya materialov i tehnologiy ih pererabotki na period do 2030 goda [Strategic directions of the development of materials and technolo-gies of their processing for the period until 2030] //Aviatsionnye materialy i tehnologii. 2012. №S. S. 7–17.
  8. Kablov E.N., Schetanov B.V., Ivahnenko Yu.A., Balinova Yu.A. Perspektivnye armiruyuschie vysokotemperaturnye volokna dlya metallicheskih i keramicheskih kompozitsionnyh materialov [Advanced high-temperature reinforcing fibers for metal and ceramic composite materials] //Trudy VIAM. 2013. №2 (elektronnyj zhurnal).
  9. Hohlatova L.B., Kolobnev N.I., Antipov V.V., Karimova S.A. i dr. Vliyanie korrozionnoy sredy na skorost' rosta treschiny ustalosti v alyuminievyh splavah [An effect of a corrosive environment on the fatigue crack growth rate in aluminium alloys] //Trudy VIAM. 2013. №3 (elektronnyj zhurnal).
  10. Akatenkov R.V., Kondrashov S.V., Fokin A.S., Marahovskiy P.S. Osobennosti formirovaniya polimernyh setok pri otverzhdenii epoksidnyh oligomerov s funktsializovannymi nanotrubkami [Polymer network formation features during the curing processes of epoxy oligomers with functionalized nanotubes] //Aviatsionnye materialy i tehnologii. 2011. №2. S. 31–37.
  11. Semenova L.V., Malova N.E., Kuznetsova V.A., Pozhoga A.A. Lakokrasochnye materialy i pokrytiya [Lacquer-and-paint materials and coatings] //Aviatsionnye materialy i tehnologii. 2012. №S. S. 315–327.
  12. Kablov E.N., Kondrashov S.V., Yurkov G.Yu. Perspektivy ispol'zovaniya uglerodsoderzhaschih nanochastits v svyazuyuschih dlya polimernyh kompozitsionnyh materialov [Application potential of carbon-bearing nanoparticles in binders for polymer composite materials] //Rossiyskie nanotehnologii. 2013. T. 8. №3–4. S. 28–46.
  13. Semenova L.V., Rodina N.D., Nefedov N.I. Vliyanie sherohovatosti sistem lakokrasochnyh pokrytiy na ekspluatatsionnye svoystva samoletov [An effect of roughness of lacquer-and-paint coating systems on service properties of aircraft] //Aviatsionnye materialy i tehnologii. 2013. №2. S. 37–40.
  14. Kondrashov E.K., Kuznetsova V.A., Semenova L.V., Lebedeva T.A. Osnovnye napravleniya povysheniya ekspluatatsionnyh, tehnologicheskih i ekologicheskih harakteristik lakokrasochnyh pokrytiy dlya aviatsionnoy tehniki [Main directions for an improvement of operational, processing and environmental characteristics of lacquer-and-paint coatings for aeronautical engineering] //Rossiyskiy himicheskiy zhurnal. 2010. T. LIV. №1. S. 96–102.
  15. Solntsev St.S., Rozenenkova V.A., Mironova N.A., Gavrilov S.V. Vysokotemperaturnye tonkoplenochnye pokrytiya dlya uplotnitel'nyh materialov iz metallicheskih volokon [High-temperature thin-film coatings for sealing materials made from metal fibers] //Aviatsionnye materialy i tehnologii. 2012. №1. S. 30–37.