Influence of alloying elements and production technology on the properties of sintered magnets Pr(Nd)–Dy(M)–Fe–Co–B (M: Tb, Ce, Sm)
UDC
669.046.516.2
DOI
10.18577/2307-6046-2024-0-6-69-79
Article PDF (Russian)
(774.91 KB)
How to cite
Buzenkov A.V., Burkanov M.V., Valeev R.A., Piskorsky V.P. Influence of alloying elements and production technology on the properties of sintered magnets Pr(Nd)–Dy(M)–Fe–Co–B (M: Tb, Ce, Sm) // Proceedings of VIAM. 2024. No. 6. DOI: 10.18577/2307-6046-2024-0-6-69-79. URL: https://viam-works.ru/en/journal/2024/6/7
Keywords
dynamically adjustable gyroscope, rare earth metals, coercive force, residual induction, rectangularity of the demagnetization curve, sintering temperature, heat treatment modes, powder grinding duration
Abstract
The effect of alloying elements (Tb, Ce, Sm) on the properties of sintered magnets Pr(Nd)–Dy(M)–Fe–Co–B(М: Tb, Ce, Sm) as well as sintering temperature, grinding time and various heat treatment modes on the main magnetic characteristics and phase composition of magnets is investigated. It is shown that heat treatment does not significantly affect the magnetic properties. It was found that the admixture of samarium negatively affects the magnetic characteristics of materials. It has been established that the most effective materials are based on praseodymium (without admixture of neodymium).
Reference list
- Martynenko Yu.G. Trends in the development of modern gyroscopy. Sorosovskiy obrazovatelniy zhurnal, 1997, no. 11, pp. 120–127.
- Matveev V.V., Raspopov V.Ya. Fundamentals of constructing strapdown inertial navigation systems. St. Petersburg: Concern «Central Research Institute «Electropribor», 2009, 280 p.
- Mahony R., Kumar V., Corke P. Multirotor Aerial Vehicle Dynamics, Stability and Control: Towards a Full Estimation. Springer, 2012, pp. 20–32.
- Lavoie F. Di Li, Landry R. Development of an inertial navigation system based on MEMS sensors. Giroskopiya i navigatsiya, 2009, no. 1 (64), pp. 75–85.
- Chirkin D.S., Roslovets P.V., Tatarinov F.V., Novikov L.Z. Reducing the drift of a dynamically tuned gyroscope from launch to launch. Inzhenernyy zhurnal: nauka i innovatsii, 2017, no. 1, pp. 1–14. DOI: 10.18698/2308-6033-2017-01-1579.
- Topilskaya S.V., Borodulin D.S., Kornyukhin A.V. Experimental assessment of permissible mechanical influences on a dynamically adjustable gyroscope. Vestnik MGTU im. N.E. Baumana. Ser.: Priborostroyenie, 2018, no. 4, pp. 69–79.
- Moscovskaya T.E. Definition of density of bodies hydrostatic weighing: methodical recommendations. Irkutsk: Irkutsk state univ., 2003, pp. 1–9.
- Valeev R.A., Korolev D.V., Morgunov R.B., Piskorsky V.P. The effect of high concentrations of cobalt on the properties of magnets Pr–Dy–Fe–Co–B and Nd–Dy–Fe–Co–B. Trudy VIAM, 2022, no. 10 (116), paper no. 06. Available at: http://www.viam-works.ru (accessed: January 25, 2023). DOI: 10.18577/2307-6046-2022-0-10-66-75.
- Kablov E.N., Antipov V.V. The role of new generation materials in ensuring the technological sovereignty of the Russian Federation. Vestnik Rossiyskoy akademii nauk, 2023, vol. 93, no. 10, pp. 907–916.
- Lapteva K.A., Tolmachev I.I. Calculation of the demagnetizing factor during longitudinal magnetization in magnetic particle flaw detection. Izvestiya Tomskogo politekhnicheskogo universiteta, 2012, vol. 321, no. 2, pp. 140–144.
- Sato M., Ishii Y. Simple and approximate expressions of demagnetizing factors of uniformly magnetized rectangular rod and cylinder. Journal of Applied Physics, 1989, vol. 66, nо. 2, pp. 983–985.
- Chen Du-Xing, Brug J.A., Goldfarb R.B. Demagnetizing factor for cylinder. IEEE Transactions on Magnetics, 1991, vol. 27, nо. 4, pp. 3601–3619.
- Sinnema S., Franse J.J.J., Radwanski R.J. et al. Magnetic measurements on R2Fe14B and R2Co14B compounds in high fields. Le Journal de Physique Colloques, 1985, vol. 46, pp. C6-301–C6-304.
- Herbst J.F. R2Fe14B materials: intrinsic properties and technological properties and technological aspects. Reviews of Modern Physics, 1991, vol. 63, no. 4, pp. 819–898.
- Szytula A., Ivanov V., Vinokurova L. Magnetic properties of the RT2X2, RTX2 and RTX compounds in high magnetic field. Acta Physica Polonica A, 1994, vol. 85, pp. 293–296.
- Koichi Niihara, Toetu Shishido, Selshi Yajima. The crystal data of ternary rare earth borides RCo2B2. Bulletin of the Chemical Society of Japan, 1979, vol. 46, pp. 1137–1140.
- Aby S.N., Hadjipanayis G.C. Magnetic properties of amorphous and crystallized RT4B alloys. Journal of Applied Physics, 1987, vol. 61, no. 8, pp. 3757–3759.
- Drzazga Z., Winiarska A., Stein F. Magnetic properties of RCo4‒x Fex B compounds (R=Gd, Dy). Journal of the Less-Common Metals, 1989, vol. 153, pp. L21–L24.
- Gros F., Hartman-Boutron D.F., Meyer C. et al. Mossbauer study of compounds RCo4‒xFexB and RFe4B. Journal de Physique, 1988, vol. 49, no. 12, pp. C8-547–C8-548.
- Nguyen Minh Hong. Ferromagnetism in CeCo3B2. Communications in Physics, 2007, vol. 17, no. 4, pp. 241–245.
- De Cunha J.B.M., Viccaro P.J., Vasquez A. A Mossbauer study of the spin-reorientation in the pseudobinary intermetallic compounds (Er10xGdx)Fe3. Hyperfine Interactions, 1983, vol. 15/16, pp. 697–700.
- de Grood C.H., Buschow K.H.J., de Boer F.R. Re-entrant ferromagnetism in the ThFe3‒xAlx system. Journal of Magnetism and Magnetic Materials, 1996, vol. 157/158, pp. 641–642.
- Primavesi G.J., Taylor K.N.R., Harris L.R. Structural and magnetic studies of the pseudo-binary compounds (Gd1‒xNdx) Co2. Journal de Physique, 1971, vol. 32, pp. C1-661–C1-662.
- Ren W.J., Zhang Z.D., Markosyan A.S. et al. The beneficial effect of the boron substitution on the magnetostrictostrictive compound Tb0,7Pr0,3Fe2. Journal of Physics D: Applied Physics, 2001, vol. 54, pp. 3024–3027.
- Umkhaeva Z.S. Structural and magnetic phase transformations and hyperfine interactions on the 57Fe nucleus in high-pressure phases of alloys of quasi-binary systems RΙ1‒xRΙΙxM2 and R(Fe1‒xMx)2 (R-REM), M-3d-metal: thesis, Cand. Sc. (Tech.). Grozny, 2013, 339 p.
- Perigo E.A., Takiishi H., Motta C.C., Faria R.N. On the squareness factor behavior of RE-FeB (RE=Nd or Pr) magnets above room temperature. IEEE Transaction Magnetic, 2009, vol. 45, nо. 3, pp. 4431–4434.
- Takiishi H., Lima L.F.C.P., Costa I., Faria R.N. The influence of process parameters and alloy structure on the magnetic properties of NdDyFeB HD sintered magnets. Journal of Materials Processing Technology, 2004, vol. 152, pp. 1–8.
- Faria R.N., Davies B.E., Brown D.N., Harris I.R. Microstructural and magnetic studies of cast and annealed Nd and PrFeCoBZr alloys and HDDR materials. Journal of Alloys and Compounds, 2000, vol. 296, pp. 223–228.
- Morgunov R.B., Piskorskiy V.P., Valeev R.A., Korolev D.V. The thermal stability of rare-earth magnets supported by means of the magnetocaloric effect. Aviacionnye materialy i tehnologii, 2019, no. 1 (54), pp. 88–94. DOI: 10.18577/2071-9140-2019-0-1-88-94.
- Buzenkov A.V., Valeev R.A., Piskorsky V.P., Morgunov R.B. The effect of the content of yttrium on the properties of the sintered Magnets Nd–Dy–Y–Fe–Co–B. Trudy VIAM, 2022, no. 4 (110), paper no. 11. Available at: http://www.viam-works.ru (accessed: January 23, 2023). DOI: 10.18577/2307-6046-2022-0-4-108-117.
- Piskorskiy V.P., Valeev R.A., Korolev D.V., Stolyankov Yu.V., Morgunov R.B. Technologies of magneto-optical information recording in thin films of rare-earth magnetically soft alloys. Part II. Ultrafast all optical switching of magnetization. Trudy VIAM, 2020, no. 2 (86), paper no. 03. Available at: http://www.viam-works.ru (accessed: January 26, 2023). DOI: 10.18577/2307-6046-2020-0-2-10-21.