Features of cold-resistant rubbers on the basis of different unvulcanized rubbers

Chaykun A.М., Еliseev O.A., Naumov I.S., Venediktova M.A.
Chaykun A.М., Еliseev O.A., Naumov I.S., Venediktova M.A. Features of cold-resistant rubbers on the basis of different unvulcanized rubbers // Proceedings of VIAM. 2013. No. 12. URL: https://viam-works.ru/en/journal/2013/12/4
Abstract

In article features of application of cold-resistant curing rubbers compounds on the basis of different rubbers in aircraft and astronautics are provided. At operation of low-temperature rubbers in products for aircraft and astronautics it is required along with high it is elastic-deformation characteristics and combination of frost resistance with high ozone and resistant to atmosphere influence, operation in all-weather conditions, and number of cases, resistance to influence of hostile environment is necessary also. In provided article features of application of the cold-resistant rubbers used in aircraft and astronautics are systematized, on basis interest to systematize features of application of the cold-resistant rubbers used in aircraft and astronautics, on the basis of different rubbers interest to systematize features of application of the cold-resistant rubbers used in aircraft and astronautics, on the basis of rubbers of different types. In the carried-out research the fa

Reference list
  1. Bol'shoy spravochnik rezinschika [Great handbook of rubber workers]: V 2 ch. M.: OOO «Tehinform». 2012. 1385 s.
  2. Nudel'man Z.N. Ftorkauchuki: osnovy, pererabotka, primenenie [Fluoroelastomers: Fundamentals. Processing. Applications]. M.: OOO «PIF RIAS». 2007. 383 s.
  3. Kablov E.N. Strategicheskie napravleniya razvitiya materialov i tehnologiy ih pererabotki do 2030 goda [Strategic directions of the development of materials and technologies of their processing for the period until 2030] //Aviatsionnye materialy i tehnologii. 2012. №S. S. 7–17.
  4. Kablov E.N. Himiya v aviatsionnom materialovedenii [Chemistry in the aviation materials science] //Rossiyskiy himicheskiy zhurnal. 2010. T. LIV. №1. S. 3–4.
  5. Eliseev O.A., Krasnov L.L., Zaytseva E.I., Savenkova A.V. Razrabotka i modifitsirovanie elastomernyh materialov dlya primeneniya vo vseklimaticheskih usloviyah [Development and Modification of Elastomeric Materials for Application under All-Climatic Conditions] //Aviatsionnye materialy i tehnologii. 2012. №S. S. 309–314.
  6. Graschenkov D.V., Chursova L.V. Strategiya razvitiya kompozitsionnyh i funktsional'nyh materialov [Development strategy of composite and functional materials] //Aviatsionnye materialy i tehnologii. 2012. №S. S. 231–242.
  7. Mahlis F.A., Fedyukin D.L. Terminologicheskiy spravochnik po rezine [Terminological handbook of rubber]. M.: Himiya. 1989. 400 s.
  8. Tehnologiya reziny: Retsepturostroenie i ispytaniya [Rubber technology: Compounding and testing]: Per. s angl. /Pod red. Dzh.S. Dika. SPb.: Nauchnye osnovy i tehnologii. 2010. 620 s.
  9. Shveytser F.A. Korroziya plastmass i rezin [Corrosion of plastics and rubbers]. SPb.: Nauchnye osnovy i tehnologii. 2010. 637 s.
  10. Chaykun A.M., Eliseev O.A., Naumov I.S., Venediktova M.A. Osobennosti postroeniya retseptur morozostoykih rezin [Compounding principles in the field of frost-resistant rubbers] //Aviatsionnye materialy i tehnologii. 2013. №3. S. 53–55.
  11. Govorova O.A., Vishnitskiy A.S., Chubarova G.V., Morozov Yu.L. Razrabotka atmosferostoykih rezin s uluchshennymi nizkotemperaturnymi i adgezionnymi svoystvami [Development of weather-resistant rubbers with improved low-temperature and adhesion properties] //Kauchuk i rezina. 1999. №2. S. 18–20.
  12. Maskulyuinate O.E., Morozov Yu.L., Suhinin N.S. i dr. Vliyanie sposoba vvedeniya plastifikatora na svoystva parafinatnyh kauchukov BNKS i standartnye reziny na ih osnove [An influence of the plasticizing method on properties of paraffinate butadiene-nitrile raw rubbers and standard rubbers based on them] //Kauchuk i rezina. 2006. №3. S. 14–17.
  13. Petrova N.N. Osobennosti sozdaniya rezin uplotnitel'nogo naznacheniya dlya ekspluatatsii v usloviyah holodnogo klimata [Features of the production of seal-purpose rubbers for operation under cold weather conditions] //Kauchuk i rezina. 2005. №6. S. 27–29.
  14. Petrova N.N., Portnyagina V.V. Reziny na osnove smesey propilenoksidnogo kauchuka i politetraftoretilena [Rubbers based on mixtures of propylene oxide rubber and polytetrafluorethylene] //Kauchuk i rezina. 2007. №4. S. 8–11.
  15. Kucherskiy A.M., Varaksin M.E., Gleyzer L.B. Vliyanie plotnosti sshivaniya rezin na ih morozostoykost' [An effect of rubber crosslink density on their frost resistance] //Kauchuk i rezina. 1987. №11. S. 18–20.
  16. Kuznetsova O.V., Donskoy A.A., Markin E.A. Reziny na osnove ftorsiloksanovyh elastomerov: Sostoyanie i perspektivy razvitiya [Rubbers based on fluoro-silicone elas-tomers: Current state and development trends] //Kauchuk i rezina. 2007. №3. S. 37–43.
  17. Chaykun A.M., Naumov I.S., Eliseev O.A. Ftorsiloksanovye reziny: nekotorye aspekty primeneniya [Fluoro-silicone rubbers: some aspects of application] //Aviatsionnye ma-terialy i tehnologii. 2013. №2. S. 35–36.
  18. Anisimov B.Yu., Dybman A.S., Imyanitov L.S., Polyakov S.A. Gidrirovanie butadien-nitril'nyh kauchukov [Hydrogenation of nitrile butadiene rubbers] //Kauchuk i rezina. 2007. №2. S. 32–38.
  19. Kornev Yu.V., Yanovskiy Yu.G., Boyko O.V. i dr. Nanodispersnyj mineral shungit – novyj usilivayuschiy napolnitel' dlya elastomernyh kompozitsiy [Nanodispersed mineral shungite is a new reinforcing filler for elastomeric compositions] //Promyshlennoe pro-izvodstvo i ispol'zovanie elastomerov. 2011. №4. S. 36–41.
  20. Petrova N.N., Portnyagina V.V. Morozostoykie reziny novogo pokoleniya [Frost-resistant rubbers of new generation] /V sb. tru-dov Mezhdunarodnoy nauch.-tehnich. konf. «Forum gornyakov–2012». Dnepropetrovsk. 2012. S. 219–226.
  21. Kryukova A.B., Kuznetsova M.N., Kanauzova A.A., Amatina T.S., Mitina E.L., Vra-cheva R.A. Sravnitel'nye svoystva rezin na osnove etilen-propilenovyh kauchukov otechestvennogo i zarubezhnogo proizvodstva dlya primeneniya v aviatsionnoy tehnike [Comparative properties of rubbers based on ethylene-propylene raw rubbers of domestic and foreign production for the use in aeronautical engineering] /V sb. trudov II Vse-rossiyskoy nauch.-tehnich. konf. «Kauchuk i rezina–2010». M. 2010. S. 363–364.
  22. Shuvaeva A.V. Rezinotkanevye membrannye materialy na osnove gidrirovannyh butadien-nitril'nyh kauchukov [Rubber-fabric membrane materials based on hydrogenated nitrile butadiene rubbers]: Avtoref. dis. k.t.n. M. 2011. 23 s.
  23. Kotova S.V., Mihaylov S.I., Fomina A.A. Osobennosti sovremennogo rynka butadien-nitril'nyh kauchukov [Features of the modern market of nitrile butadiene rubbers] //Kauchuk i rezina. 2012. №6. S. 33–35.