Development and researching of thermostable sol-gel coatings in Y2O3–AL2O3–SIO2 system for SiC-based materials

Lebedeva Yu.E., Grachshencov D.V., Popovich N.V., Orlova L.A., Chaynikova A.S.
Lebedeva Yu.E., Grachshencov D.V., Popovich N.V., Orlova L.A., Chaynikova A.S. Development and researching of thermostable sol-gel coatings in Y2O3–AL2O3–SIO2 system for SiC-based materials // Proceedings of VIAM. 2013. No. 12. URL: https://viam-works.ru/en/journal/2013/12/3
Abstract

In the course of the work with purpose of the obtaining by sol-gel method protective high-temperature coatings of Y2O3–Al2O3–SiO2 system technique of the preparation film-formation solution was perfected, influence of the components ratio in initial solution on physic-chemical characteristics of solutions, gels and sintered materials was studied, phase formations were studied. Application capability of this coatings to protective SiC materials at high temperature was investigated.

Reference list
  1. Kablov E.N. Strategicheskie napravleniya razvitiya materialov i tehnologiy ih pererabotki na period do 2030 goda [Strategic directions of the development of materials and technologies of their processing for the period until 2030] //Aviatsionnye materialy i tehnologii. 2012. №S. S. 7–17.
  2. Kablov E.N., Graschenkov D.V., Isaeva N.V., Solntsev S.S. Perspektivnye vysokotemperaturnye keramicheskie kompozitsionnye materialy [Advanced high-temperature ceramic composite materials] //Rossiyskiy himicheskiy zhurnal. 2010. T. LIV. №1. S. 20–24.
  3. Simonenko E.P., Simonenko N.P., Sevast'yanov V.G., Graschenkov D.V., Kuznetsov N.T., Kablov E.N. Funktsional'no gradientnyj kompozitsionnyj material SiC/(ZrO2–HfO2–Y2O3), poluchennyj s primeneniem zol'-gel' metoda [Functionally gradient com-posite material SiC/(ZrO2–HfO2–Y2O3) produced by sol-gel method] //Kompozity i nanostruktury. 2011. №4. S. 52–64.
  4. Graschenkov D.V., Chursova L.V. Strategiya razvitiya kompozitsionnyh i funktsional'nyh materialov [Development strategy of composite and functional materials] //Aviatsionnye materialy i tehnologii. 2012. №S. S. 231–242.
  5. Solntsev S.S., Rozenenkova V.A., Mironova N.A. Vysokotemperaturnye steklokeram-icheskie pokrytiya i kompozitsionnye materialy [High-Temperature Glass-Ceramic Coat-ings and Composite Materials] //Aviatsionnye materialy i tehnologii. 2012. №S. 359–368.
  6. Graschenkov D.V., Solntsev S.St., Schegoleva N.E., Naumova A.S., Gaponov B.N. Steklokeramicheskiy kompozitsionnyj material [Glass-Ceramic Composite Material] //Aviatsionnye materialy i tehnologii. 2012. №S. S. 368–372.
  7. Krenkel W., Berndt F. C/C–SiC composites for space applications and advanced friction systems //Materials Science and Engineering A. 2005. V. 412. №1–2. Р. 177–181.
  8. Westwood M.E., Hayes F.H., Day R.J., Taylor R. Oxidation Protection of Ceramic Composites with Carbon Fibre Reinforsment //J. Mater. Sci. 1996. V. 31. P. 1389–1397.
  9. Jacobson N.S. Corrosion of silicon-based ceramics in combustion environments //J. Eur. Ceram. Soc. 1993. V. 76. Р. 3–28.
  10. Huang J.-F., Li H.-J., Zeng X.-R. Influence of preparation technology on the microstructure and anti-oxidation property of SiC–Al2O3-mullite multi-coatings for carbon/carbon composites //Applied Surfase Science. 2006. V. 252. Р. 4244–4249.
  11. Cabet C. Review: Oxidation of SiC/SiC Composites in Low Oxidizing and High Tem-perature Environment /Materials Issues for Generation IV Systems. 2008. R. 351–366.
  12. Mironov V.V., Kochetkov Yu.M., Vvedenskiy V.S. i dr. Eksperimental'nye issledovaniya rabotosposobnosti tonkostennyh neohlazhdaemyh sopel ZhRD iz uglerodnyh kompozitsionnyh materialov [Experimental studies of operability of thin-walled un-cooled composite nozzles of LRE made of carbon composite materials] //Aviakosmicheskaya tehnika i tehnologiya. 2001. №3. S. 55–61.
  13. Toropov I.A. i dr. Diagrammy sostoyaniya silikatnyh system [Phase diagrams of silicate systems: Handbook]: Spravochnik. M.-L.: Nauka. 1965. 258 s.
  14. Harrysson R., Vomacka P Glass formation in the system Y2O3–Al2O3–SiO2 under conditions of laser melting //J. of the European Ceramic Society. 1994. №14. P. 377–380.
  15. Toropov I.A., Bondar' I.A., Lazarev A.N., Smolin Yu.I. Silikaty redkozemel'nyh elementov i ih analogi [Silicates of rare-earth elements and their analogues]. L.: Nauka. 1971. 230 s.
  16. www.mincryst.ru
  17. Shima J.B., Yoshikawa A., Nikl M., Soloviev N., Pejchal J., Yoon D.H., Fukuda T. Growth and characterization of Yb3+-doped YAlO3 fiber single crystals grown by the modified micro-pulling-down method //Journal of Crystal Growth. 2003. №256. Р. 298–304.
  18. Liang Wu, Guanghua Liu, Jiangtao Li, Bin He, Zengchao Yang, Yixiang Chen Dependence of glass-forming ability on starting compositions in Y2O3–Al2O3–SiO2 system //Ceramics – Silikáty. 2011. V. 55. №3. P. 228–231.
  19. Del' Pino K.H.S. Termicheskoe razlozhenie i nekotorye fiziko-himicheskie svoystva kristallogidratov nitrata ittriya [Thermal decomposition and some physical-chemical properties of yttrium nitrate crystalline hydrates]: Avtoref. dis. k.h.n. M.: RHTU im. Mendeleeva. 1981. 16 s.
  20. Yahong Zhang, Navrotsky A. Thermochemistry of Glasses in the Y2O3–Al2O3–SiO2 System //J. Am. Ceram. Soc. 2003. V. 86. №10. P. 1727–1732.
  21. Shen Xiaoyi, Zhai Yuchun Preparation and optical properties of Y2O3/SiO2 powder //Rare metals. 2011. V. 30. №1. Р. 33–38.
  22. MacLaren I., Richter G. The structure and possible origins of stacking faults in gamma-yttrium disilicate //Philosophical Magazine. 2009. V. 89. №2. P. 169–181.
  23. Ya-Qin Wang, Jian-Feng Huang, Li-Yun Cao,1 and Xie-Rong Zeng Direct Preparation of Y2SiO5 Nanocrystallites by a Microwave Hydrothermal Process //ISRN Nanotech-nology. 2011. V. 1. P. 1–5.
  24. Ziqi Sun, Meishuan Li, Yanchun Zhou Thermal properties of single-phase Y2SiO5 //Journal of the European Ceramic Society. 2009. №29. P. 551–557.
  25. Zarzyki J. Past and Present of Sol-Gel Science and Technology //J. of Sol-Gel Science and Technology. 1997. №8. Р. 17–22.
  26. Mackenzie J.D. Sol-Gel Research-Achievements Since 1981 and Prospects for the Fu-ture //J. of Sol-Gel Science and Technology. 2003. №26. Р. 23–27.
  27. Andrianov N.T. Zol'-gel' metod v tehnologii oksidnyh materialov [The sol-gel method in the oxide materials technology] //Steklo i keramika. 2003. №10. S. 17–22.
  28. Atkinson A., Segal D.L. Some Recent Developments in Aqueous Sol-Gel Processing //J. of Sol-Gel Science and Technology. 1998. №13. Р. 133–139.
  29. Simonenko E.P., Ignatov N.A., Simonenko N.P., Ezhov Yu.S., Sevast'yanov V.G., Kuznetsov N.T. Sintez vysokodispersnyh sverhtugoplavkih karbidov tantala-tsirkoniya Ta4ZrC5 i tantala-gafniya Ta4HfC5 cherez zol'-gel' tehniku [Synthesis of fine-grained ultra-refractory carbides of tantalum-zirconium Ta4ZrC5 and tantalum-hafnium Ta4HfC5 by the sol-gel techniques] //Zhurnal neorganicheskoy himii. 2011. №56 (11). S. 1763–1769.
  30. Sevast'yanov V.G., Simonenko E.P., Simonenko N.P., Kuznetsov N.T. Sintez vysokodispersnogo tugoplavkogo oksida tsirkoniya–gafniya–ittriya s ispol'zovaniem zol'-gel' tehniki [Synthesis of fine-grained refractory oxide of zirconium-hafnium-yttrium by the sol-gel techniques] //Zhurnal neorganicheskoy himii. 2012. №57 (3). S. 355–361.
  31. Lebedeva Yu.E., Popovich N.V., Orlova L.A. Zaschitnye vysokotemperaturnye pokrytiya dlya kompozitsionnyh materialov na osnove SiC [High-temperature protective coatings for SiC-based composite materials] //Trudy VIAM. 2013. №2 (elektronnyj zhurnal).
  32. Uvarova N.E., Orlova L.A., Lebedeva Yu.E., Graschenkov D.V. Primenenie metoda elektronnogo paramagnitnogo rezonansa dlya izucheniya strukturnyh izmeneniy v protsesse geleobrazovaniya pri poluchenii keramiki i steklokeramiki zol'-gel' metodom [Usage of electron paramagnetic resonance for studying the structural changes during the gel formation process when producing ceramics and glass ceramic by the sol-gel method] //Aviatsionnye materialy i tehnologii. 2011. №3. S. 26–30.
  33. Aparacio M., Duran A. Yttrium silicate Coatings for Oxidation Protection of Carbon-silicon Carbide Composites [Yttrium silicate Coatings for Oxidation Protection of Carbon-silicon Carbide Composites] //J. Amer. Ceram. Soc. 2000. V. 83. №6. P. 1351–1355.
  34. Kolitsch U., Seifert H.J., Ludwig T., Aldinger F Phase equilibria and crystal chemistry in the Y2O3–Al2O3–SiO2 system [Phase equilibria and crystal chemistry in the Y2O3–Аl2О3–SiO2 system] //J. of Materials Research. 1999. V. 14. №2. Р. 447–455.
  35. Sarkisov P.D., Orlova L.A., Popovich N.V., Anan'eva Yu.E. Protsessy strukturoobrazovaniya pri poluchenii ittriysilikatnyh materialov zol'-gel' metodom [Structure formation processes in the course of production of yttrium silicate materials by the sol-gel method] //Steklo i keramika. 2007. №1. S. 3–6.
  36. Ziqi Sun, Meishuan Li, Yanchun Zhou Kinetics and Mechanism of Hot Corrosion of γ-Y2Si2O7 in Thin-Film Na2SO4 Molten Salt [Kinetics and mechanism of hot corrosion of γ-Y2Si2O7 in thin-film Na2SO4 molten salt] //J. Am. Ceram. Soc. 2008. V. 91. №7. P. 2236–2242.