Investigation of the influence of technological parameters of heat treatment on microstructure of brazing joints of VT20 alloy with VPr16 solder

Afanasiev-Khodykin A.N., Galushka I.A., Sviridov A.V., Naprienko S.A.
Afanasiev-Khodykin A.N., Galushka I.A., Sviridov A.V., Naprienko S.A. Investigation of the influence of technological parameters of heat treatment on microstructure of brazing joints of VT20 alloy with VPr16 solder // Proceedings of VIAM. 2024. No. 5. DOI: 10.18577/2307-6046-2024-0-5-3-12. URL: https://viam-works.ru/en/journal/2024/5/1
Keywords
brazing, high-temperature brazing, titanium based brazing alloy, titanium alloys, high-alloy solders, microstructure of a brazing seam
Abstract

The results of investigation of the influence of the assembly gap width on the microstructure of brazing joints of pseudo-α-alloy VT20 with VPr16 solder are presented. The soldered samples after brazing and subsequent homogenization heat treatment (HHT) are analyzed. The main types of microstructures formed in the solder joint are identified and regression equations of the influence of the gap width and duration of the HHT on the main transition points of the solder joint microstructure are constructed. The dynamics of change of alloying elements (aluminum, zirconium, copper and nickel) in the solder joint and diffusion zone has been studied. The optimum microstructure is selected, which does not have a boundary in the center of the seam and boundaries of the junction of crystals.

Reference list
  1. Illarionov A.G. Technological and operational properties of titanium alloys: textbook. Ekaterinburg: Ural Univ. Publ. House, 2014, 137 p.
  2. Kablov E.N., Putyrsky S.V., Yakovlev A.L., Krokhina V.A., Naprienko S.A. Study of resistance to fatigue fracture of forgings made of high-strength titanium alloy VT22M, manufactured with final deformation in the (α+β)- and β-regions. Titan, 2021, no. 1 (70), pp. 26–33.
  3. Nochovnaya N.A., Bazyleva O.A., Kablov D.E., Panin P.V. Intermetallic alloys based on titanium and nickel. Ed. E.N. Kablov. Moscow: VIAM, 2018, 308 p.
  4. Makushina M.A., Kochetkov A.S., Nochovnaya N.A. Cast titanium alloys for aviation equipment (review). Trudy VIAM, 2021, no. 7 (101), paper no. 05. Available at: http://www.viam-works.ru (accessed: February 26, 2024). DOI: 10.18577/2307-6046-2021-0-7-39-47.
  5. Duyunova V.A., Oglodkov M.S., Putyrskiy S.V., Kochetkov A.S., Zueva O.V. Modern technologies for melting titanium alloy ingots (review). Aviation materials and technologies, 2022, no. 1 (66), paper no. 03. Available at: http://www.journal.viam.ru (accessed: February 26, 2024). DOI: 10.18577/2071-9140-2022-0-1-30-40.
  6. Yongjuan J., Xishan Y., Xingqiang G. et al. The influence of Zr content on the performance of TiZrCuNi brazing filler. Materials science and engineering A, 2016, vol. 678, рp. 190–196. DOI: 10.1016/J.MSEA.2016.09.115.
  7. Sviridov A.V., Afansiev-Khodykin A.N., Galushka I.A. Influence of manufacturing technologies of brazing alloy powder VPr28 on powder features (review). Aviation materials and technologies, 2022, no. 1 (69), paper no. 02. Available at: http://www.journal.viam.ru (accessed: February 26, 2024). DOI: 10.18577/2713-0193-2022-0-4-16-24.
  8. Skupov A.A., Sviridov A.V., Khodakova E.A., Afanasev-Khodykin A.N. Creation of joints from intermetallic titanium alloys (review). Trudy VIAM, 2021, no. 7 (101), paper no. 04. Available at: http://www.viam-works.ru (accessed: February 26, 2024). DOI: 10.18577/2307-6046-2021-0-7-31-38.
  9. Petrunin I.E., Bereznikov Yu.I., Bunkina R.R. et al. Handbook on soldering. 3rd ed. rev. and add. Moscow: Mashinostroenie-1, 2003, 480 p.
  10. Petrunin I.E., Markova I.Yu., Ekatova A.S. Metallurgy soldering. Moscow: Metallurgiya, 1976, 264 p.
  11. Lashko N.F., Lashko S.V. Soldering of metals. Moscow: Mashinostroenie, 1977, 328 p.
  12. Khorunov V.F., Maksimova S.V. Brazing of heat-resistant alloys at the present stage. Svarochnoe proizvodstvo, 2010, no. 10, pp. 24–27.
  13. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  14. Klopotov V.D., Potekaev A.I., Klopotov A.A. et al. Triple diagrams based on titanium aluminide. Analysis and construction. Izvestia TPU, 2013, no. 2, pp. 96–100.
  15. Kornilov I.I., Budberg P.B. Chemical interaction of titanium with other elements. Uspekhi khimii, 1955, vol. 25, is.1, pp. 1474–1501.
  16. Kogachi M., Minamigawa S., Kakahigashi K. Long Range Orderin L12 ternary intermetallic compound Al3Ti-X (X=Fe, Ni, Cu, Ag). Scripta metallurgica et materiala, 1992, vol. 27, pp. 407–412.
  17. State diagrams of metallic systems. Ed. N.V. Ageev. Moscow: VINITI, 1966, is. 12, 352 p.
  18. Grytsiv A., Chen X-Q., Witusiewicz V.T. et al. Atom order and thermodynamic properties of the ternary Laves phase Ti (TiyNixAl1–x–y)2. Zeitschrift fur Kristallographie, 2006, vol. 221, pp. 334–348.
  19. Schuster J.C. Critical data evaluation of the aluminium–nickel–titanium system. Intermetallics, 2006, vol. 14, pp. 1304–1311.
  20. Schuster J.C., Pan Z., Liu S., Weitzer F., Du Y. On the constitution of the ternary system Al–Ni–Ti. Intermetallics, 2007, vol. 15, pp. 1257–126.
  21. Milman Yu.V., Miracle D.B., Chugunova S.I. et al. Mechanical behavior of Al3Ti intermetallic and L12 phases on its basis. Intermetallics, 2001, vol. 9, pp. 839–845.
  22. Nakayama Y., Mabuchi H. Formation of Ternary L12 compounds in Al3Ti-base alloys. Intermetallics, 1993, vol. 1, pp. 41–48.
  23. Antashev V.G., Nochovnaya N.A., Pavlova T.V., Ivanov V.I. Heat-resistant titanium alloys. Vse materialy. Entsiklopedicheskiy spravochnik, 2007, no. 3, pp. 7–8.
  24. Cao J., Qi J., Song X., Feng J. Welding and Joining of Titanium Aluminides. Materials, 2014, no. 7, pp. 4930–4962.
  25. Shapiro A., Rabinkin A. State of the art of titanium-based brazing filler metals. Welding journal, 2003, vol. 82, no. 10, pp. 36–43.
  26. TiNiNbZr high-temperature brazing filler metal for TiAl alloy, preparation method and brazing method thereof: pat. CN 110605498A; appl. 14.05.19; publ. 24.12.19.