To the issue of helicopter rotor blades repair from polymer composite materials in field conditions
UDC
629.7.026.56
DOI
10.18577/2307-6046-2024-0-4-83-97
Article PDF (Russian)
(787.98 KB)
How to cite
Barannikov A.A., Veshkin E.A, Sudyin Yu.I., Chertishchev V.Yu. To the issue of helicopter rotor blades repair from polymer composite materials in field conditions // Proceedings of VIAM. 2024. No. 4. DOI: 10.18577/2307-6046-2024-0-4-83-97. URL: https://viam-works.ru/en/journal/2024/4/6
Keywords
helicopter equipment, main rotor blade, polymer composite materials, surface preparation, atmospheric pressure plasma, nondestructive testing methods, repair
Abstract
The article presents the results of the analysis of the design-force diagrams of the main rotor blades of the domestic helicopter equipment and the main stages of the technological process of their repair. According to the results of the analysis the input parameters for the development of the technology of repair of helicopter rotor blades from polymer composite materials in field conditions are revealed and presented. In the process of narration the directions of repair technologies development and main innovations of SIC «Kurchatov Institute» – VIAM are shown.
Reference list
- Kablov E.N. New Generation Materials and Technologies for Their Digital Processing. Herald of the Russian Academy of Sciences, 2020, vol. 90, no. 2, pp. 225–228.
- Kablov E.N. Formation of domestic space materials science. Vestnik RFFI, 2017, no. 3, pp. 97–105.
- Kablov E.N. VIAM: new generation materials for PD-14. Krylya Rodiny, 2019, no. 7–8, pp. 54–58.
- Erasov V.S., Sibayev I.G. Scheme for the development and evaluation of properties of structural aviation composite materials. Aviation materials and technologies, 2023, no. 1 (70), paper no. 05. Available at: http://www.journal.viam.ru (accessed: December 04, 2023). DOI: 10.18577/2071-9140-2023-0-1-61-81.
- Startsev V.O., Antipov V.V., Slavin A.V., Gorbovets M.A. Modern domestic polymer composite materials for aviation industry (review). Aviation materials and technologies, 2023, no. 2 (71), paper no. 10. Available at: http://www.journal.viam.ru (accessed: December 04, 2023). DOI: 10.18577/2713-0193-2023-0-2-122-144.
- Helicopter NH-90 in service with the German Armed Forces. Available at: https://topwar.ru (accessed: November 14, 2023).
- Doroshenko N.I. Application of PCM in the design of helicopter rotor blades. All-Rus. sci.-tech. conf. «Polymer composite materials for the aerospace industry». Moscow: VIAM, 2019, pp. 23–41.
- Grebenikov A.G., Dyachenko Yu.V., Kollerov V.V. et al. Structural and technological features of helicopter load-bearing surfaces made of polymer composite materials. Otkrytye informatsionnye i kompyuternye integrirovannye tekhnologii, 2019, no. 84, pp. 4–49.
- Basharov E.A., Vagin A.Yu. Analysis of the use of composite materials in the design of helicopter airframes. Trudy MAI, 2017, no. 92, pp. 1–33.
- Bogdanov Yu.S., Mikheev R.A., Skulkov D.D. Helicopter design: a textbook for aviation technical schools. Moscow: Mashinostroyenie, 1990, 272 p.
- Zavalov O.A., Basharov E.A. Guidelines for laboratory work «Design of main and tail rotor blades». Available at: http://elibrary.mai.ru/MegaPro/Download/ToView/15843?idb=New
- MAI2014 (accessed: November 14, 2023).
- Slyusar B.N., Fleck M.B., Goldberg E.S. et al. Helicopter technology. Technology for the production of helicopter blades and aircraft structures from polymer composite materials. Rostov-on-Don: YuNTs RAS, 2013, 230 p.
- Zavalov O.A. Design of rotors and tail rotors of helicopters: textbook. A guide to coursework and diploma design. Moscow: MAI, 2019, 72 p.
- Mikheyev S.V., Bourtsev B.N., Danilkina V.L. et al. Kamov Composite Blades. 31st European Rotorcraft Forum. Florence, 2015, pр. 1650–1672.
- Topolev V.V. Design and operation of the Mi-171 helicopter: textbook, allowance. Tyumen:
- NP «Personnel Training Center», 2008, 158 p.
- Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Postnov V.I., Veshkin E.A., Makrushin K.V., Sudin Yu.I. Technological features of manufacturing polymer composite materials of main rotor blades for a light helicopter. Aviation materials and technologies, 2023, no. 1 (70), paper no. 06. Available at: http://www.journal.viam.ru (accessed: December 04, 2023). DOI: 10.18577/2713-0193-2023-0-1-30-50.
- Mi-8 helicopter. Technical Operation Instructions. Available at: https://tehclub.site/
- storage/products/07-20/vertolet-mi-8-instruktsiya-po-tekhnicheskoy-ekspluatatsii.pdf (accessed: December 04, 2023).
- Aviation unit and aviation intermediate maintenance manual. CH-47D helicopter. Available at: http://www.chinook-helicopter.com/Publications/CH-47D_Technical_Publications/23_Series/TM_
- 55-1520-240-23-1.pdf (accessed: December 04, 2023).
- Helicopter maintenance by Joe Schafer. Available at: https://linguisticstudentindonesia.
- files.wordpress.com/2020/08/helicopter-maintenance.pdf (accessed: December 04, 2023).
- Bell 212. Maintenance manual. Available at: https://www.bellcustomer.com/Bulletins/
- Download?FileName=212-Inspection_and_Airworthiness_Limitations.pdf&CategoryID=139 (accessed: December 04, 2023).
- Bell 429. Maintenance planning information. Available at: https://www.bellcustomer.com/Bulletins/
- Download?FileName=429-Airworthiness_Limitations_and_Scheduled_Maintenance.pdf&Category
- ID=-1&categoryname=Airworthiness%20Limitations%20and%20Scheduled%20Maintenance (accessed: December 04, 2023).
- Joachim T. Repair and Substantiation of the NH90 Sandwich Composite Bottom Shell. Available at: https://www.sto.nato.int/publications/pages/results.aspx?k=Repair%20and%20Substantiation%20of%20the%20NH90%20Sandwich%20Composite%20Bottom%20Shell&s=Search%20All%20STO%20Reports (accessed: December 04, 2023). DOI: 10.14339/STO-MP-AVT-266-05-PDF.
- Mazza J.J., Storage K.M. Bonded Repair in the United States Air Force and Work to Expand Future Capability. Available at: https://www.sto.nato.int/publicаtions/pages/results.aspx?k=Bonded
- %20Repair%20in%20the%20United%20States%20Air%20Force%20and%20Work%20to%20Expand%20Future%20Capability&s=Search%20All%20STO%20Reports (accessed: December 04, 2023). DOI: 10.14339/STO-MP-AVT-266-04-PDF.
- Xie Z., Li X., Wang S. Parametrical study on stepped-lap repair of composite laminates. Available at: http://www.i-asem.org/publication_conf/structures16/11.ICAAS16/M4J.2.AS703_
- 1256F1.pdf (accessed: December 04, 2023).
- Xie Z., Wang S., Li X. Composite Tapered Scarf Joint Repair: Analytical Model and Experimental Validation. Amsterdam: Atlantis Press, 2016, pp. 720–726.
- Orsatelli J.-P., Paroissien E., Lachaud F., Schwartz S. Bonded flush repairs for aerospace composite structures: A review on modelling strategies and application torepairs optimization, reliability and durability. Composite Structures, 2023, vol. 304, рart 2, аrt. 116338. DOI: ff10.1016/j.compstruct.2022.116338.
- Campilho R., Pinto A., Moura M. et al. Taper angle optimization of scarf repairs in carbon-epoxy laminates. Available at: https://www.semanticscholar.org/paper/Taper-angle-optimization-of-scarf-repairs-in-Campilho-Pinto/c2222dcdaa9b3ac70d9bd79dd24e6b820e424ce3 (accessed: December 04, 2023).
- Collombet F., Davila Y., Avila S. et al. Proof of a composite repair concept for aeronautical structures: a simplified method. Mechanics & Industry, 2019, no. 20 (8), pp. 812. DOI: 10.1051/meca/2020056.
- Marrón A. Scarf joint modeling and analysis of composite materials. Available at: https://core.ac.uk/download/pdf/36698412.pdf (accessed: December 04, 2023).
- Mollenhauer D., Storage K., Czabaj M. et al. United States Air Force Investigation and Evaluation of Composite Scarf Repairs. Available at: https://www.sto.nato.int/publications/pages/
- reults.aspx?k=United%20States%20Air%20Force%20Investigation%20and%20Evaluation%20of%20Composite%20Scarf%20Repairs&s=Search%20All%20STO%20Reports (accessed: December 04, 2023). DOI: 10.14339/STO-MP-AVT-266-14-PDF.
- Ghafafian C., Popiela B., Trappe V. Failure Mechanisms of GFRP Scarf Joints under Tensile Load. Materials, 2021, vol. 14 (7), pp. 1806. DOI: 10.3390/ma14071806.
- Sun C., Zhao W., Zhou J. et al. Mechanical behaviour of composite laminates repaired with a stitched scarf patch. Composite Structures, 2021, vol. 255, pp. 112928. DOI: 10.1016/j.compstruct.2020.112928.
- Gungner M., Ramström M. Robust repair methods of primary structures in composite. Available at: https://www.diva-portal.org/smash/get/diva2:632489/FULLTEXT01.pdf (accessed: December 04, 2023).
- Xie Z., Li X., Yan Q. Scarf Repair of Composite Laminates. MATEC Web of Conferences. Available at: https://www.researchgate.net/publication/304575167_Scarf_Repair_of_Composite_
- Laminates (accessed: December 04, 2023). DOI: 10.1051/matecconf/20166105019.
- Tomblin J., Salah L., Yang C. Effects of repair procedures applied to composite airframe structures. Available at: https://depts.washington.edu/amtas/events/jams_06/Salah_Repair.pdf (accessed: December 04, 2023).
- Budhe S., Banea M.D., De Barros S. Bonded repair of composite structures in aerospace application: a review on environmental issues. Applied Adhesion Science, 2018, vol. 6, art. 3. DOI: 10.1186/s40563-018-0104-5.
- Halliwell S. Repair of fibre reinforced polymer structures. Available at: https://compositesuk.co.uk/wp-content/uploads/2021/12/repairoffrpstructures.pdf (accessed: December 04, 2023).
- Ashfort C., Ilcewicz L. Certification of Bonded Aircraft Structure and Repairs. Available at: https://www.sto.nato.int/publications/pages/results.aspx?k=Cynthia%20Ashfort&s=Search%20All%20STO%20Reports (accessed: December 04, 2023).
- Helicopter components, sections and systems. Available at: https://www.faa.gov/sites/faa.gov/files/
- regulations_policies/handbooks_manuals/aviation/helicopter_flying_handbook/hfh_ch04.pdf (accessed: December 04, 2023).
- Seneviratne W., Tomblin J., Saathoff C. Evaluation of aged bonded rotor blades. Available at: https://www.wichita.edu/industry_and_defense/NIAR/Documents/jams-presentations-2021/Evaluation
- -of-Aged-Bonded-Rotor-Blades-Seneviratne.pdf (accessed: December 04, 2023).
- Ilcewicz L., Cheng L. FAA composite guidance and relevant resource. Available at: https://www.aviation.govt.nz/assets/aircraft/composite-seminar/faa-composite-guidance.pdf (accessed: December 04, 2023).
- Salah L. CACRC depot bonded repair round robin investigation. Available at: https://www.wichita.edu/industry_and_defense/NIAR/Documents/CACRCDepotBondedLSalah.pdf
- (accessed: December 04, 2023).
- Composite Repair of Military Aircraft Structures. Neuilly sur Seine: AGARD, 1995, 24 р.
- Sałaciński M., Kowalski R., Szmidt M., Augustyn S. A New Approach to Modelling and Testing the Fatigue Strength of Helicopter Rotor Blades during Repair Process. Fatigue of Aircraft Structures, 2019, vol. 11, pp. 56–67. DOI: 10.2478/fas-2019-0006.
- Lewis A. Making composite repairs to the 787. Available at: https://skybrary.aero/sites/
- default/files/bookshelf/3851.pdf (accessed: December 04, 2023).
- Fualdes C. Experience and lessons learned of a composite aircraft. Available at: https://icas.org/media/pdf/ICAS%20Congress%20General%20Lectures/2016/2016%20Composite%20Aircraft%20Fualdes.pdf (accessed: December 04, 2023).
- Barannikov A.A., Рostnov V.I., Veshkin E.A., Starostina I.V. Link between the energy characteristics of the surface of fiberglass of the VPS-53К brand and the strength of the adhesive joint based on it. Trudy VIAM, 2020, no. 10 (92), paper no. 05. Available at: http://www.viam-works.ru (accessed: November 14, 2023). DOI: 10.18577/2307-6046-2020-0-10-40-50.
- Pieczonka L., Staszewski W.J. et al. Nondestructive testing of composite patch repairs. 11th
- European Conference on Non-Destructive Testing. Prague, 2014. DOI: 10.13140/2.1.1691.8723.
- Antipov V.V., Boichuk A.S., Chertishchev V.Yu., Yakovleva S.I., Barannikov A.A. Identification of operational damage from blades of rotors and tail rotors made of PCM in operating conditions. Trudy VIAM, 2023, no. 7 (125), paper no. 08. Available at: http://www.viam-works.ru (accessed: November 14, 2023). DOI: 10.18577/2307-6046-2023-0-7-93-103.