Structural features and mechanical properties of joints, produced by electron beam welding of strip extrusions from aluminum-lithium alloy V-1469
UDC
669.715:669.018.62
DOI
10.18577/2307-6046-2024-0-4-33-49
Article PDF (Russian)
(1.95 MB)
How to cite
Benarieb I., Romanenko V.A., Panteleev M.D., Oglodkov M.S., Ovchinnikov V.V., Filonova E.V. Structural features and mechanical properties of joints, produced by electron beam welding of strip extrusions from aluminum-lithium alloy V-1469 // Proceedings of VIAM. 2024. No. 4. DOI: 10.18577/2307-6046-2024-0-4-33-49. URL: https://viam-works.ru/en/journal/2024/4/3
Keywords
aluminum-lithium alloys, Al–Cu–Li system, alloy V-1469, electron-beam welding, liquation cracks, differential scanning calorimetry
Abstract
This paper presents results of study of the microstructure and mechanical properties of welded joints produced by electron beam welding of strip extrusions from high-strength alloy V-1469 of Al–Cu–Li system. The features of the structural and phase state of the material
in various zones of electron beam welding joint are studied by means of scanning and transmission
electron microscopy, thermal analysis and thermodynamic modeling. The influence of welding speed
on the mechanical properties and nature of fracture of welds was studied
Reference list
- Kablov E.N., Antipov V.V., Oglodkova Yu.S., Oglodkov M.S. Experience and prospects for the use of aluminum-lithium alloys in aviation and space technology products. Metallurg, 2021, no. 1, pp. 62–70.
- Kablov E.N., Antipov V.V., Klochkova Yu.Yu. New generation aluminum-lithium alloys and layered aluminum-fiberglass plastics based on them. Tsvetnye metally, 2016, no. 8 (884), pp. 86–91.
- Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Kolobnev N.I., Khokhlatova L.B., Lukina E.A. Trends in the development of aluminum-lithium alloys and technologies for their processing. Ed. E.N. Kablov. Moscow: VIAM, 2019, 367 p.
- Grushko O.E., Ovsyannikov B.V., Ovchinnikov V.V. Aluminum-lithium alloys: metallurgy, welding, metal science. Moscow: Nauka, 2014, 296 p.
- Betsofen S.Ya., Antipov V.V., Knyazev M.I. Alloys of the Al–Cu–Li and Al–Mg–Li systems: phase composition, texture and anisotropy of mechanical properties (review). Deformatsiya i razrusheniye materialov, 2015, no. 11, pp. 10–26.
- Elagin V.I., Zakharov V.V. Modern Al–Li alloys and prospects for their development. Tekhnologiya legkikh splavov, 2013, no. 4, pp. 17–23.
- Ovsyannikov B.V., Komarov S.B. Development of production of deformed semi-finished
- products from aluminum-lithium alloys at JSC KUMZ. Tekhnologiya legkikh splavov, 2014, no. 1, рр. 97–103.
- Prasad N.E., Gokhale A., Wanhill R.J.H. Aluminium-lithium alloys: processing, properties, and applications. Amsterdam: Elsevier, 2014, 652 p.
- Dorin T., Vahid A., Lamb J. Aluminium lithium alloys. Fundamentals of aluminium metallurgy. Cambridge: Woodhead Publishing, 2018, pp. 387–438. DOI: 10.1016/B978-0-08-102063-0.00011-4.
- Starke E.A.(Jr.) Historical development and present status of aluminium-lithium alloys. Aluminium-lithium alloys. Processing, properties and applications. Oxford: Elsevier Inc., 2014, pp. 3–26.
- Rioja R.J., Liu J. The Evolution of Al–Li Base Products for Aerospace and Space Applications. Metallurgical and Materials Transactions A, 2012, vol. 43, no. 9, pp. 25–37.
- Antipov V.V., Tkachenko E.A., Zajtsev D.V., Selivanov A.A., Ovsyannikov B.V. Тhe influence of homogenizing annealing regimes on the structural phase state and mechanical properties of aluminum-lithium alloy 1441 ingots. Trudy VIAM, 2019, no. 3 (75), paper no. 05. Available at: http://www.viam-works.ru (accessed: December 18, 2023). DOI: 0.18577/2307-6046-2019-0-3-44-52.
- Oglodkov M.S., Romanenko V.A., Benarieb I., Rudchenko A.S., Grigoryev M.V. Study of industrial semi-finished products from advanced aluminum-lithium alloys for aircraft products. Aviation materials and technologies, 2023, no. 3 (72), paper no. 05. Available at: http://www.journal.viam.ru (accessed: December 18, 2023). DOI: 10.18577/2713-0193-2023-0-3-62-77.
- Sharonov N.I., Sharapov M.G. Control of the process of formation of a welded joint during electron beam welding of aluminum alloys of increased thickness. Voprosy materialovedenia, 2018, no. 2 (94), pp. 167–174.
- Bondarev A.A., Nesterenkov V.M. Electron beam welding of thin-sheet volumetric structures made of aluminum alloys. Avtomaticheskaya svarka, 2011, no. 6, pp. 43–47.
- Skalsky E.G., Botvina L.R., Lyasota I.N. Features of structural and mechanical heterogeneity in welded joints of alloy 1201-T, made by electron beam welding. Avtomaticheskaya svarka, 2012, no. 7, pp. 19–23.
- Ternovoy E.G., Bondarev A.A. Electron beam welding of thick-walled shells made of aluminum alloys AMg6 and M40. Avtomaticheskaya svarka, 2012, no. 4, pp. 8–14.
- Troshin A.A., Shepelevich M.V. Improving the quality of welded joints made of aluminum alloys during electron beam welding. Aktualnye problemy aviatsii i kosmonavtiki, 2013, vol. 1, no. 9, pp. 119–120.
- Erypalov L.A., Kovalev D.S. Optimization of electron beam welding technology for products made of aluminum alloys. Aktualnye problemy aviatsii i kosmonavtiki, 2012, vol. 1, no. 8, pp. 91–93.
- Bashenko V.V., Sharonov N.I. Features of electron beam welding of pressed-stamped aluminum alloys. Nauchno-tekhnicheskiye vedomosti Sankt-Peterburgskogo gosudarstvennogo politekhnicheskogo universiteta, 2010, no. 3 (106), pp. 139–143.
- Cam G., Ventzke V., Dos Santos J.F. et al. Characterization of electron beam welded aluminium alloys. Science and Technology of Welding and Joining, 1999, vol. 4, no. 5, pp. 317–323.
- Chen G., Yin Q., Zhang G., Zhang B. Underlying causes of poor mechanical properties of aluminum-lithium alloy electron beam welded joints. Journal of Manufacturing Processes, 2020, vol. 50, pp. 216–223.
- Hosseini S.A., Abdollah-Zadeh A., Naffakh-Moosavy H., Mehri A. Elimination of hot cracking in the electron beam welding of AA2024-T351 by controlling the welding speed and heat input. Journal of Manufacturing Processes, 2019, vol. 46, pp. 147–158.
- Chen G., Yin Q., Zhang G., Zhang B. Fusion-diffusion electron beam welding of aluminum lithium alloy with Cu nano-coating. Materials and Design, 2020, vol. 188, p. 108439.
- Bárta J., Šimeková B., Marônek M., Dománková M. Electron Beam Welding of 2099-T83 aluminium-lithium alloy thick plates. MATEC Web of Conferences, 2019, vol. 269, art. 02010.
- Sorokin L.I. Formation of hot cracks in the heat-affected zone during welding of heat-resistant nickel alloys (review). Svarochnoe proizvodstvo, 2005, no. 8, pp. 38–43.
- Samarina M.V., Alov A.A., Elagin V.I., Kozlovskaya V.P. Influence of the structure of welded semi-finished products from aluminum alloys on the sensitivity to heat-affected cracks. Tekhnologiya legkikh splavov, 1976, no. 11, pp. 7–11.
- Malikov A.G., Orisic A.M. Preparation of high-strength laser welded joints of aluminum alloys for aviation purposes. Fotonika, 2019, vol. 13, no. 4, pp. 356–366.
- Belyanin V.P., Denisov B.S., Meilakh A.I. et al. Features of the formation of the fusion zone of welds of alloy 1420. Aviatsionnaya promyshlennost, 1989, no. 9, p. 70.
- Ivanov S.Yu., Karkhin V.A., Mikhailov V.G. et al. Modeling of the formation of liquation cracks during laser welding of Al–Mg–Si alloys. Izvestiya TulGU. Tekhnicheskiye nauki, 2015, is. 6, part 2, pp. 66–74.
- Fridlyander I.N., Grushko O.E., Shamray V.F., Klochkov G.G. High-strength structural
- Al–Cu–Li–Mg alloy of low density, alloyed with silver. Metallovedenie i termicheskaya obrabotka metallov, 2007, no. 6 (624), pp. 3–7.
- Istomin-Kastrosky V.V., Shamray V.F., Grushko O.E., Klochkova Yu.Yu., Ryazantseva M.A.
- The influence of additions of silver, magnesium, zirconium on the aging of the B-1469 alloy of the
- Al–Cu–Li system. Metally, 2010, no. 5, pp. 73–78.
- Lukin V.I., Kulik V.I., Betsofen S.Ya., Lukina E.A., Sharov A.V., Panteleyev M.D., Samorukov M.L. Friction stir welding of high-strength aluminum-lithium V-1469 alloy semiproducts. Trudy VIAM, 2017, no. 12 (60), paper no. 02. Available at: http://viam-works.ru (accessed: December 21, 2023). DOI: 10.18577/2307-6046-2017-0-12-2-2.
- Panteleev M.D., Sviridov A.V., Skupov A.A., Odintsov N.S. Perspective welding technologies of aluminum-lithium alloy V-1469 applied to fuselage panels. Trudy VIAM, 2020, no. 12 (94), paper no. 04. Available at: http://www.viam-works.ru (accessed: December 25, 2023). DOI: 10.18577/2307-6046-2020-0-12-35-46.
- Bulina N.V., Malikov A.G., Orishich А.М., Klochkov G.G. Research of the structural-phase composition of laser weld joint depending on the thermal processing of the aluminum alloy V-1469. Aviacionnye materialy i tehnologii, 2019, no. 2 (55), pp. 31–39. DOI: 10.18577/2071-9140-2019-0-2-31-39.
- Ovchinnikov V.V., Grushko O.E., Alekseev V.V. et al. Structure and properties of welded joints of aluminum alloy V-1469 obtained by electron beam welding. Zagotovitelnye proizvodstva v mashinostroyenii, 2012, no. 5, pp. 7–11.
- Makhin I.D., Nikolaev V.V., Petrovichev P.S. Study of the weldability of alloys V-1469 and 01570S using electron beam welding in relation to the design of a promising manned spacecraft. Kosmicheskaya tekhnika i tekhnologii, 2014, no. 4, pp. 68–75.
- Egorov R.V., Ovchinnikov V.V. Electron beam welding of aluminum alloys based on the Al–Cu–Li system. Zagotovitelnye proizvodstva v mashinostroyenii, 2017, vol. 15, no. 7, pp. 294–298.
- Jia M., Zheng Z., Gong Z. Microstructure evolution of the 1469 Al–Cu–Li–Sc alloy during homogenization. Journal of alloys and compounds, 2014, vol. 614, pp. 131–139.
- Frindlyander I.N., Sandler V.S., Lukin V.I. Thermal tests of Al–Mg–Li alloys. Metallovedeniye i termicheskaya obrabotka metallov, 1991, no. 2, pp. 38–40.
- Examilioti T., Li W., Kashaev L. et al. On anisotropic tensile mechanical behavior of Al–Cu–Li AA2198 alloy under different ageing conditions. Journal of materials research and technology, 2023, vol. 24, pp. 895–908.
- Kablov E.N., Lukina E.A., Sbitneva S.V., Khokhlatova L.B., Zaitsev D.V. Formation of metastable phases during the decomposition of a solid solution during artificial aging Al-alloys. Tekhnologiya legkikh splavov, 2016, no. 3, pp. 7–17.
- Fomina M.A., Kutyrev A.E., Klochkova Yu.Yu., Sbitneva S.V. Research of corrosion characteristics of high-strength alloy of Al–Cu–Li system depending on various modes of heat treatment. Aviacionnye materialy i tehnologii, 2016, no. S2, pp. 39–48. DOI: 10.18577/2071-9140-2016-0-S2-39-48.
- Lequeu Ph., Smith K.P., Danielou A. Aluminum-copper-lithium alloy 2050 developed for medium to thick plate. Journal of Materials Engineering and Performance, 2010, vol. 19 (6), pp. 841–847.
- Yang Q., Lei L., Fan X. et al. Microstructure evolution and processing map of Al–Cu–Li–Mg–Ag alloy. Materials Chemistry and Physics, 2020, vol. 254, р. 123256.
- Jiang N., Xiang G., Zi-Qiao Z. Microstructure evolution of aluminum-lithium alloy 2195 undergoing commercial production. Transactions of Nonferrous Metals Society of China, 2010, vol. 20, pp. 740–745.
- Ovchinnikov V.V., Egorov R.V. Porosity of welds during electron beam welding of aluminum alloys alloyed with lithium. Vestnik IGEU, 2006, is. 4, pp. 1–5.
- Loshchinin Yu.V., Pakhomkin S.I., Fokin A.S. Influence of speed of heating at research of phase transformations in aluminum alloys DSC method. Aviacionnye materialy i tehnologii, 2011, no. 2, pp. 3–6.
- Kolobnev N.I., Ryabova E.N., Khokhlatova L.B., Oglodkov M.S. Features of the structure of ingots from alloys of the Al–Cu–Li system depending on the chemical composition. Vestnik MGTU im. N.E. Baumana. Ser.: Mashinostroyenie, 2016, no. 3, pp. 69–80. DOI: 10.18698/0236-3941-2016-3-69-80.