Characteristics of AMg6 alloy under static and cyclic loading
Monin S.A., Medvedev P.N., Ponomarev K.E., Strelnikov I.V. Characteristics of AMg6 alloy under static and cyclic loading // Proceedings of VIAM. 2024. No. 12. DOI: 10.18577/2307-6046-2024-0-12-96-108. URL: https://viam-works.ru/en/journal/2024/12/9
Keywords
creep, fatigue, cyclic creep, AMg6, Larson–Miller, welding modeling, friction welding, vibration during welding
Abstract
The results of tests to determine the creep characteristics of aluminum alloy AMg6 under static and cyclic loading at elevated temperatures are presented in the article. Characteristics of static and cyclic creep are necessary to predict residual stresses in a welded structure subjected to vibration during welding. Creep curves under static and cyclic loading are analyzed and compared. The effect of the variable component of the load on creep resistance is estimated using the Larson–Miller equation.
Reference list
- Panteleev M.D., Sviridov A.V., Skupov A.A., Odintsov N.S. Aluminum-Lithium alloy V-1469 welded fuselage constructions survivability. Aviation materials and technologies, 2022, no. 4 (69), paper no. 03. Available at: http://www.journal.viam.ru (accessed: April 10, 2024). DOI: 10.18577/2713-0193-2022-0-4-25-35.
- Kablov E.N., Lukin V.I., Zhegina I.P., Ioda E.N., Loskutov V.M. Features and Prospects of Welding Aluminum-Lithium Alloys. Aviacionnye materialy i technologii, 2002, no. 4, pp. 3–12.
- Mai Xuan D., Gnevko A.I., Puchkov Yu.A. Study of cryogenic treatment influence on residual stresses and properties of D16 aluminium alloy. Aviacionnye materialy i tehnologii, 2020, no. 2 (59), pp. 25–31. DOI: 10.18577/2071-9140-2020-0-2-25-31.
- Jose M.J., Kumar S.S., Sharma A. Vibration assisted welding processes and their influence on quality of welds. Science and Technology of Welding & Joining, 2016, is. 4, pp. 45–49. DOI: 10.1179/1362171815Y.0000000088.
- Ingram E., Golan O., Haj-Ali R., Noam Eliaz. The effect of localized vibration during welding of the microstructure and mechanical behavior of steel welds. Materials, 2019, no. 12 (2553). DOI: 10.3390/ma12162553.
- Ponomarev K.E., Strelnikov I.V. Prospects for the Application of Various Methods of Vibration Treatment of Critical Welded Structures of Spacecraft. Kosmicheskie apparaty i tekhnologii, 2023, no. 2, pp. 126–131. DOI: 10.26732/j.st.2023.2.05.
- Taira S., Otani R. Theory of High-Temperature Strength of Materials. Ed. V.B. Kireev. Moscow: Metallurgiya, 1986, 280 p.
- Radchenko V.P., Saushkin M.N. Creep and Relaxation of Residual Stresses in Hardened Structures. Moscow: Mashinostroenie, 2005, 226 p.
- Strizhalo V.A. Cyclic strength and creep of metals under low-cycle loading under low and high temperature conditions. Kyiv: Naukova Dumka, 1978, 238 p.
- Birger I.A. Residual stresses. Moscow: Mashgiz, 1963, 232 p.
- Dubovova E.V. Development of methods for calculating the relaxation of residual stresses in hardened structural elements under steady-state and cyclic creep conditions: abstract thesis, Cand. Sc. (Tech.). Samara, 2012, 20 p.
- Khokhlov A.V. Analysis of general properties of creep curves under cyclic step loading generated by the linear theory of heredity. Vestnik Samarskogo gosudarstvennogo tekhnicheskogo universiteta. Ser.: Fiziko-matematicheskiye nauki, 2017, vol. 21, no. 2, pp. 326–361.
- Khokhlov A.V. Properties of the creep curve family under step loading of the linear constitutive relation of viscoelasticity. Problemy prochnosti i plastichnosti, 2015, vol. 77, no. 4, pp. 344–359.
- Artemyev D.M., Bukanov V.A., Sadkin K.E., Ilyin A.V. Finite element modeling of residual stress relaxation during post-weld tempering of a large-sized structure made of high-strength steel. Trudy Krylovskogo gosudarstvennogo nauchnogo tsentra, 2018, no. 1, pp. 130–136.
- Bulkov A.B., Peshkov V.V., Petrenko V.R., Balbekov D.N. Modeling the process of high-temperature deformation of metal during diffusion welding under creep conditions. Vestnik VGTU, 2011, no. 8, pp. 4–8.
- Kiselev A.S. Development of methods for analysis and design of welding technology based on computer modeling of the thermally deformed and structural state of welded structures: thesis, Dr. Sc. (Tech.). Moscow, 1999, 317 p.
- Experimental methods for studying deformations and stresses: reference manual. Ed. B.S. Kasatkin. Kyiv: Naukova Dumka, 1981, 584 p.
- Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Kablov E.N., Antipov V.V., Chesnokov D.V., Kutyrev A.E. Application of Al–Mg–Si–Cu system aluminum alloy combined anodic dissolution for prognosis of tensile strength loss during natural exposure testing. Aviacionnye materialy i tehnologii, 2020, no. 2 (59), pp. 63–73. DOI: 10.18577/2071-9140-2020-0-2-63-73.
- Calculations and strength tests. Creep test method under regular multi-cycle loading: P 50-54-35-88. Moscow: VNIIMASH, 1988, 24 p.
- Erasov V.S., Oreshko E.I. Fatigue tests of metal materials (review). Part 1. Main definitions, loading parameters, representation of results of tests. Aviacionnye materialy i tehnologii, 2020, no. 4 (61), pp. 59–70. DOI: 10.18577/2071-9140-2020-0-4-59-70.
- Dowling N.E. Mechanical Behavior of Materials: Engineering methods for Deformation, Fracture, and Fatigue. 2nd ed. Upper Saddle River, 1999, 830 p.
- Maruyama K., Abe F., Sato H. et al. On the physical basis of a Larson‒Miller constant of 20. International Journal of Pressure Vessels and Piping. 2018, no. 159, pp. 93–100.
- Larson F.R., Miller J. A time-temperature relationship for rupture and creep stresses. Transcriptions of ASME, 1952, vol. 7, pp. 765–775.