Issues of assessing the tightness of fabric-film materials and flexible pipelines of air conditioning systems made of them
Makrushin K.V., Barannikov A.A., Ishchenko I.A., Sudyin Yu.I. Issues of assessing the tightness of fabric-film materials and flexible pipelines of air conditioning systems made of them // Proceedings of VIAM. 2024. No. 12. DOI: 10.18577/2307-6046-2024-0-12-75-84. URL: https://viam-works.ru/en/journal/2024/12/7
Keywords
fabric-film materials, flexible pipelines, air conditioning systems, control tightness, requirements, polymers
Abstract
The article presents the main principles, methods and techniques for assessing the tightness of fabric-film materials (FMM) and flexible pipelines of air conditioning systems (ACS) of aircraft made of them. The tightness of these products is one of the main requirements and is necessary for the reliable functioning of the ACS. The article presents a method for calculating the tightness indicators during tests using the manometric method, diagrams of a device for monitoring the tightness of the TPM, a stand for testing the tightness of flexible pipelines, and a brief technological process for performing tightness monitoring operations.
Reference list
- State Standard 22607–77. Air conditioning systems for aircraft and helicopters. Terms and definitions. Moscow: Publ. House of Standards, 1977, 7 p.
- Tkacheva V.R., Galka G.A. Review of existing aircraft air conditioning systems. Molodoy uchenyy, 2016, no. 23 (127), pp. 91–95.
- Kablov E.N. What to make the future from. New generation materials, technologies for their creation and processing – the basis of innovations. Krylya Rodiny, 2016, no. 5, pp. 8–18.
- Startsev V.O., Antipov V.V., Slavin A.V., Gorbovets M.A. Modern domestic polymer composite materials for aviation industry (review). Aviation materials and technologies, 2023, no. 2 (71), paper no. 10. Available at: http://www.journal.viam.ru (accessed: October 14, 2024). DOI: 10.18577/2713-0193-2023-0-2-122-144.
- Erasov V.S., Sibayev I.G. Scheme for the development and evaluation of properties of structural aviation composite materials. Aviation materials and technologies, 2023, no. 1 (70), paper no. 05. Available at: http://www.journal.viam.ru (accessed: October 14, 2024). DOI: 10.18577/2713-0193-2023-0-1-61-81.
- Kablov E.N. Materials are the basis of any business. Delovaya slava Rossii, 2013, no. 2, pp. 4–9.
- Veshkin E.A., Satdinov R.A., Postnov V.I., Strelnikov S.V. Modern polymer materials for manufacture of elements of the air conditioning system in flying apparatus. Trudy VIAM, 2017, no. 12 (60), paper no. 06. URL: http://www.viam-works.ru (accessed: August 23, 2024). DOI: 10.18577/2307-6046-2017-0-12-6-6.
- Film-based material and product based on it: pat. 2733779 Rus. Federation; appl. 11.11.19; publ. 06.10.20.
- Sutubalov A.I., Podzhivotov N.Yu., Shershak P.V., Yakovlev N.O. Evaluation of homogeneity of physical and mechanical properties of semi-finished products for aviation purpose. Aviation materials and technologies, 2024, no. 1 (74), paper no. 10. Available at: http://www.journal.viam.ru (accessed: October 14, 2024). DOI: 10.18577/2713-0193-2024-0-1-121-135.
- Ivanov М.S., Pavlukovich N.G., Donskih I.N., Morozova V.S. Influence of operational factors on the properties of fabricfilm material for lowpressure air ducts of the air conditioning system of aircraft. Trudy VIAM, 2023, no. 4 (122), paper no. 11. Available at: http://www.viam-works.ru (accessed: September 20, 2024). DOI: 10.18577/2307-6046-2023-0-4-118-127.
- State Standard 24054–80. Mechanical engineering and instrument making products. Leak test methods. General requirements. Moscow: Publ. House of Standards, 1980, 14 p.
- Industry standard 1 00128‒74. Industry standard. Leakage of products. Norms. Moscow: MAP, 1987, 7 p.
- Industry standard 1 41318‒2002. Aviation standard. Hydrogas systems. Leakage testing by manometric method. Moscow: MAP, 2002, 7 p.
- Flexible pipeline made of polymer composite material: pat. 2733797 Rus. Federation; appl. 11.11.19, publ. 06.10.20.
- Kablov E.N. Main directions of development of materials for aerospace engineering. Perspektivnye materialy, 2000, no. 3, pp. 27–36.