Estimation of electrical properties distribution under elastic deformation of the control object by eddy current method
Shitikov V.S., Pichugin S.S. Estimation of electrical properties distribution under elastic deformation of the control object by eddy current method // Proceedings of VIAM. 2024. No. 11. DOI: 10.18577/2307-6046-2024-0-11-89-99. URL: https://viam-works.ru/en/journal/2024/11/7
Keywords
eddy current inspection, stress-strain state, specific electrical conductivity, frequency variation, tensile stresses, compressive stresses
Abstract
The article deals with the possibility of estimating the distribution of electrical properties along the depth of the object using eddy current method of nondestructive testing. Experimental testing of stress-strain state estimation of titanium alloy plate at bending by means of transducer signal acquisition in a wide range of frequencies is carried out. The experimental data was analyzed using analytical calculation of the transducer signal. As a result of the studies, the relationship between mechanical stresses and electrical conductivity was established, and the possibility of effective control of the stress level by eddy current method was shown.
Reference list
- Kablov E.N., Bakradze M.M., Gromov V.I., Voznesenskaya N.M., Yakusheva N.A. New high strength structural and corrosion-resistant steels for aerospace equipment developed by FSUE «VIAM» (review). Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 3–11. DOI: 10.18577/2071-9140-2020-0-1-3-11.
- Oreshko E.I., Erasov V.S., Yakovlev N.O., Utkin D.A. Methods for determining the mechanical characteristics of materials using indentation (review). Aviation materials and technology, 2021, no. 1 (62), paper no. 10. Available at: http://www.journal.viam.ru (accessed: May 17, 2024). DOI: 10.18577/2713-0193-2021-0-1-104-118.
- Kablov E.N., Evgenov A.G., Bakradze M.M., Nerush S.V., Krupnina O.A. New generation materials and digital additive technologies for the production of resource parts of FSUE VIAM. Part 1. Materials and synthesis technologies. Elektrometallurgiya, 2022, no. 1, pp. 2–12.
- Nochovnaya N.A., Shiryaev A.A., Sharapkin D.S. Complex of mechanical and operational properties of rolled blanks from metastable-β-titanium alloy VT47. Aviation materials and technologies, 2022, no. 3 (68), paper no. 05. Available at: http://www.journal.viam.ru (accessed: May 17, 2024). DOI: 10.18577/2713-0193-2022-0-3-50-59.
- Kablov E.N., Startsev V.O. Effect of internal stresses on the aging of polymer composite materials (review). Mekhanika kompozitnykh materialov, 2021, vol. 57, no. 5, pp. 805–822.
- Podzhivotov N.Yu. The minimum samples amounts for an assessment of the initial moments of distribution of tensile ultimate strength for the samples of structural metallic materials. Aviation materials and technologies, 2021, no. 2 (63), paper no. 11. Available at: http://www.journal.viam.ru (accessed: May 17, 2024). DOI: 10.18577/2713-0193-2021-0-2-103-114.
- Pichugin S.S., Shitikov V.S., Golovkov A.N. Non-destructive methods for residual stress assessment. Trudy VIAM, 2024, no. 1 (131), paper no. 10. Available at: http://www.viam-works.ru (accessed: May 17, 2024). DOI: 10.18577/2307-6046-2024-0-1-101-112.
- Shitikov V.S., Pichugin S.S., Kudinov I.I. Analysis of the Possibility of Estimating Residual Stresses by the Eddy Current Method of Non-Destructive Testing. Elektrometallurgiya, 2024, no. 2. pp. 22–28. DOI: 10.31044/1684-5781-2024-0-2-22-28.
- Kekalo I.B. Physical Properties of Metals. Section «Electrical Properties»: Laboratory Workshop. Moscow, 1998, 139 p.
- Dorofeev A.L., Lyubashev G.A., Ostanin Yu.Ya. Measuring Coating Thickness Using Eddy Currents. Moscow: Mashinostroenie, 1975, 64 p.
- Bakunov A.S., Gerasimov V.G., Ostanin Yu.Ya. Eddy current testing with clamp-on transducers. Moscow: Mosk. Energ. In-t, 1985, 86 p.
- Gerasimov V.G., Klyuev V.V., Shaternikov V.E. Methods and devices of electromagnetic testing. Ed. V.E. Shaternikov. Moscow: Spektr, 2010, 256 p.
- Avtaev V.V., Kotova A.E., Gladkikh A.V., Boychuk A.S. Equipment for bending tests constructive and similar samples welded hybrid panels of the wing. Trudy VIAM, 2018, no. 9 (69), paper no. 09. Available at: http://www.viam-works.ru (accessed: May 17, 2024). DOI: 10.18577/2307-6046-2018-0-9-83-91.
- State Standard 9.019–74. Unified system of protection against corrosion and aging. Aluminum and magnesium alloys. Methods of accelerated tests for stress corrosion cracking. Moscow: Publ. House of Standards, 1974, 18 p.
- Pisarenko G.S., Yakovlev A.P., Matveev V.V. Handbook of strength of materials. Kyiv: Naukova Dumka, 1988, 736 p.