Study of isothermal phase transformations kinetics in heat-resistant alloys based on gamma titanium aluminide TiAl

Akbulatov R.R., Efremova A.P., Bogachev I.A., Panin P.V.
Akbulatov R.R., Efremova A.P., Bogachev I.A., Panin P.V. Study of isothermal phase transformations kinetics in heat-resistant alloys based on gamma titanium aluminide TiAl // Proceedings of VIAM. 2024. No. 11. DOI: 10.18577/2307-6046-2024-0-11-22-32. URL: https://viam-works.ru/en/journal/2024/11/3
Keywords
titanium aluminide TiAl, beta-solidifying gamma alloys, peritectically solidified gamma alloys, Temperature–Time–Transformation (TTT) diagrams, thermal stability, X-ray diffraction (XRD) analysis, selective electron beam melting (SEBM)
Abstract

An experimental investigation of structure evolution kinetics in heat-resistant intermetallic TiAl-based alloys of various classes has been accomplished under the conditions of high-temperature exposures in the temperature range 900–1300 °C and durations of 15–240 min. The Temperature–Time–Transformation diagrams (TTT-diagrams) have been constructed to summarize data on isothermal phase transformations in the studied alloys with initial structures after selective electron beam melting.

Reference list
  1. Kim Y.-W., Kim S.-L. Advances in gammalloy materials–processes–application technology: successes, dilemmas, and future. Journal of Metals, 2018, vol. 70, pp. 553–560. DOI: 10.1007/s11837-018-2747-x.
  2. Appel F., Paul J.D.H., Oehring M. Gamma Titanium Aluminide Alloys: Science and Technology. Weinheim: Wiley-VCH Verlag & Co, KGaA, 2011, 745 p.
  3. Kablov E.N., Nochovnaya N.A., Panin P.V., Alekseev E.B., Novak A.V. Study of the structure and properties of heat-resistant alloys based on titanium aluminides with gadolinium microadditives. Inorganic Materials: Applied Research, 2017, vol. 8, no. 4, pp. 634–641. DOI: 10.1134/S2075113317040116.
  4. Mayer S., Erdely P., Fischer F.D. et al. Intermetallic β‐solidifying γ‐TiAl based alloys − from fundamental research to application. Advanced Engineering Materials, 2017, vol. 19, art. 1600735.
  5. Clemens H., Mayer S. Design, processing, microstructure, properties, and applications of advanced intermetallic TiAl alloys. Advanced Engineering Materials, 2013, vol. 15, pp. 191–215.
  6. Wimler D., Lindemann J., Reith M. et al. Designing advanced intermetallic titanium aluminide alloys for additive manufacturing. Intermetallics, 2021, vol. 131, art. 107109.
  7. Chen W., Yang Y., Liu L.L. et al. Microstructure control and tensile properties of EBM γ-TiAl. Aeronautical Manufacturing Technology, 2017, vol. 1-2, pp. 37–41.
  8. Körner C. Additive manufacturing of metallic components by selective electron beam melting – a review. International Materials Reviews, 2016, vol. 61, no. 5, pp. 361–377.
  9. Murr L.E., Gaytan S.M., Ramirez D.A. et al. Metal fabrication by additive manufacturing using laser and electron beam melting technologies. Journal of Materials Science and Technology, 2012, vol. 28, pp. 1–14.
  10. Wartbichler R., Clemens H., Mayer S. Electron beam melting of a β‐solidifying intermetallic titanium aluminide alloy. Advanced Engineering Materials, 2019, vol. 21, аrt. 1900800.
  11. Reith M., Franke M., Schloffer M., Körner C. Processing 4th generation titanium aluminides via electron beam based additive manufacturing – characterization of microstructure and mechanical properties. Materialia, 2020, vol. 14, art. 100902.
  12. Schwerdtfeger J., Körner C. Selective electron beam melting of Ti-48Al-2Nb-2Cr: microstructure and aluminium loss. Intermetallics, 2014, vol. 49, pp. 29–35.
  13. Panin P.V., Zavodov A.V., Lukina E.A. Effect of thermal exposure on microstructure evolution and mechanical properties of cast beta-solidifying TiAl-based alloy doped with Gd. Intermetallics, 2022, vol. 145, art. 107534. DOI: 10.1016/j.intermet.2022.107534.
  14. Xia K., Wu X., Song D. Effects of Gd addition, lamellar spacing and loading direction on creep behavior of a fully lamellar Ti–44Al–1Mn–2,5Nb alloy. Acta Materialia, 2004, vol. 52, pp. 841–849. DOI: 10.1016/j.actamat.2003.10.018.
  15. Chen Y.Y., Li B.H., Kong F.T. Microstructural refinement and mechanical properties of Y-bearing TiAl alloys. Journal of Alloys and Compounds, 2008, vol. 457, pp. 265–269. DOI: 10.1016/j.jallcom.2007.03.050.
  16. Li W., Inkson B., Horita Z., Xia K. Microstructure observations in rare earth element Gd-modified Ti-44 at% Al. Intermetallics, 2000, vol. 8, pp. 519–523. DOI: 10.1016/S0966-9795(99)00156-9.
  17. Lütjering G., Williams J.C. Titanium. Berlin-Heidelberg: Springer-Verlag, 2003, 406 p.
  18. Panin P.V., Lukina E.A., Shiryaev A.A. Temperature–Time–Transformation diagrams construction for beta-solidifying TiAl-based alloy in as-cast condition. IOP Conf. Series: Materials Science and Engineering (FarEastCon-2020), 2021, vol. 1079, art. 062010. DOI: 10.1088/1757-899X/1079/6/062010.
  19. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  20. Bondarenko Yu.A. Trends in the development of high-temperature metal materials and technologies in the production of modern aircraft gas turbine engines. Aviacionnye materialy i tehnologii, 2019, no. 2 (55), pp. 3–11. DOI: 10.18577/2071-9140-2019-0-2-3-11.
  21. Alekseev Е.B., Nochovnaya N.A., Novak A.V., Panin P.V. Wrought intermetallic titanium ortho alloy doped with yttrium Part 1. Research on ingot microstructure and rheological curves plotting. Trudy VIAM, 2018, no. 6 (66), paper no. 02. Available at: http://www.viam-works.ru (accessed: August 09, 2024). DOI: 10.18577/2307-6046-2018-0-6-12-21.
  22. Vasilev A.I., Putyrskiy S.V., Korotchenko A.Yu., Anisimova A.Yu. MIM technology as a method of manufacturing precision parts from metal-powder compositions, including titanium alloys (review). Trudy VIAM, 2021, no. 3 (97), paper no. 02. Available at: http://www.viam-works.ru (accessed: August 09, 2024). DOI: 10.18577/2307-6046-2021-0-3-16-27.
  23. Alloy based on titanium intermetallic compound and a product made from it: pat. 2606368 Rus. Federation; appl. 15.10.15; publ. 10.01.17.
  24. Titanium aluminum alloys modified by chromium and niobium and method of preparation: pat. US 4879092; appl. 03.06.88; publ. 07.11.89.
  25. Duyunova V.A., Oglodkov M.S., Putyrskiy S.V., Kochetkov A.S., Zueva O.V. Modern technologies for melting titanium alloy ingots (review). Aviation materials and technologies, 2022, no. 1 (66), paper no. 03. Available at: http://www.journal.viam.ru (accessed: August 09, 2024). DOI: 10.18577/2713-0193-2022-0-1-30-40.
  26. Panin P.V., Lukina E.A., Bogachev I.A., Medvedev P.N., Naprienko S.A. Additive synthesis of TiAl alloy of the Ti–Al–V–Nb–Cr–Gd system by selective electron beam melting. Metallurg, 2023, no. 3, pp. 55–65. DOI: 10.52351/00260827_2023_03_55.
  27. Panin P.V., Lukina E.A., Bogachev I.A., Naprienko S.A. Influence of technological parameters of selective electron beam melting on the chemical composition, microstructure and porosity of TiAl alloy of the Ti–Al–V–Nb–Cr–Gd system. Metallurg, 2023, no. 5, pp.54–66.
  28. Spitans S., Franz H., Baake E. Numerical modelling and optimization of the electrode induction melting for inert gas atomization (EIGA). Proceedings of 11th PAMIR International Conference – Fundamental and Applied MHD. Reims, 2019, pp. 327–331.
  29. Knyazev A.E., Vostrikov A.V. Sieving of powders additive and powder manufacturings (review). Trudy VIAM, 2020, no. 11 (93), paper no. 02. Available at: http://www.viam-works.ru (accessed: 09.08.2024). DOI: 10.18577/2307-6046-2020-0-11-11-20.
  30. Alishin M.I., Knyazev A.E. Production of metal-powder high-purity titanium alloy compositions by induction gas atomization for application in additive manufacturing. Trudy VIAM, 2017, no. 11 (59), paper no. 05. Available at: http://www.viam-works.ru (accessed: August 09, 2024). DOI: 10.18577/2307-6046-2017-0-11-5-5.
  31. Peskova A.V., Sukhov D.I., Mazalov P.B. Examination of the formation of the titanium alloy VT6 structure obtained by additive manufacturing. Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 38–44. DOI: 10.18577/2071-9140-2020-0-1-38-44.
  32. McCusker L.B., Von Dreele R.B., Cox D.E. et al. Rietveld refinement guidelines. Journal of Applied Crystallography, 1999, vol. 32, pp. 36–50. DOI: 10.1107/S0021889898009856.
  33. Ilyin A.A., Kolachev B.A., Polkin I.S. Titanium alloys. Composition, structure, properties: reference. Moscow: VILS-MATI, 2009, 520 p.
  34. Murray J.L. The Cr–Ti (chromium-titanium) system. Bulletin of Alloys Phase Diagrams, 1981, vol. 2, no. 2, pp. 174–181.
  35. Venkatraman M., Neumann J.P. Cr–Nb (chromium-niobium) system. Bulletin of Alloys Phase Diagrams, 1986, vol. 7, no. 5, pp. 462–466.