Effect of temperature on drying time and viability of epoxyvinyl ether resin putty
Marchenko S.A., Skivko P.V. Effect of temperature on drying time and viability of epoxyvinyl ether resin putty // Proceedings of VIAM. 2024. No. 10. DOI: 10.18577/2307-6046-2024-0-10-84-93. URL: https://viam-works.ru/en/journal/2024/10/8
Keywords
unsaturated polyester resins, epoxy vinyl ether resin, putty, drying time to degree 3, viability.
Abstract
The influence of ambient temperature and humidity on the curing rate of putty based on unsaturated polyester resin (epoxy vinyl ether) was studied: the viability of the putty after mixing with a hardener and accelerator, the drying time to degree 3 of the putty coating was investigated. The physical and mechanical properties of the putty coating during curing under various temperature and humidity conditions have been determined. The optimal temperature and humidity (when working in open areas) were determined during the curing of coatings based on epoxy vinyl ether putty.
Reference list
- Kablov E.N. Aviation Materials Science: Results and Prospects. Vestnik Rossiyskoy akademii nauk, 2002, vol. 72, no. 1, pp. 3–12.
- Kablov E.N. Structural and Functional Materials – the Basis of Economic and Scientific-Technical Development of Russia. Voprosy materialovedeniya, 2006, no. 1, pp. 64–67.
- Kablov E.N. Aviation Materials Science in the 21st Century. Prospects and Tasks. Aviation Materials. Selected Works of VIAM 1932–2002. Moscow: MISiS–VIAM, 2002, pp. 23–47.
- Tkachuk A.I., Zagora A.G., Donetsky K.I., Evdokimov A.A. Polymeric matrixes for composite materials used in the construction of quickly built bridge structures. Trudy VIAM, 2020, no. 12 (94), paper no. 07. Available at: http://www.viam-works.ru (accessed: August 21, 2024). DOI: 10.18577/2307-6046-2020-0-12-67-74.
- Doriomedov M.S. Russian and world market of polymer composites (review). Trudy VIAM, 2020, no. 6–7 (89), paper no. 04. Available at: http://www.viam-works.ru (accessed: August 20, 2024). DOI: 10.18577/2307-6046-2020-0-67-29-37.
- Sidorina A.I. Multiaxial carbon fabrics in the products of aviation technology (review). Aviation materials and technologies, 2021, no. 3 (64), paper no. 10. Available at: http://www.journal.viam.ru (accessed: August 21, 2024). DOI: 10.18577/2713-0193-2021-0-3-105-116.
- Harish V., Nagaiah N., Niranjana Prabhu T. et al. Preparation and characterization of lead monoxide filled unsaturated polyester based polymer composites for gamma radiation shielding applications. Journal of Applied Polymer Science, 2009, vol. 112, is. 3, pp. 1503–1508.
- Martínez-Barrera G., Villarruel U., Vigueras-Santiago E. et al. Compressive strength of gamma-irradiated polymer concrete. Polymer Composites, 2008, vol. 29, is. 11, pp. 1210–1217.
- Kucherenko E.V., Shcherbakov A.S., Arzamastsev S.V. Composite materials based on polyester resin. Sovremennye innovatsii, 2016, no. 3 (5), pp. 5–7.
- Tkachuk A.I., Terekhov I.V., Gurevich Ya.M., Grigoreva K.N. Research of the influence of the modifying additives nature on the rheological and thermomechanical properties of a photopolymer composition based on epoxy vinyl ester resin. Aviacionnye materialy i tehnologii, 2019, no. 3 (56), pp. 31–40. DOI: 10.18577/2071-9140-2019-0-3-31-40.
- Cook M.I., Dubowik D.A., Walker F.H. Improved high solids epoxy paints with new curing agents. Fabre und Lack, 2000, vol. 106 (4), pp. 28–43.
- Brock T., Groteklaus M., Mischke P. Unsaturated polyesters. European Guide to Paints and Coatings. Moscow: Paint-Media, 2007, pp. 73–78.
- Sertsova A.A., Koroleva M.Yu., Yurtov E.V. et al. Fire-resistant polymer nanocomposites based on metal oxides and hydroxides. Khimicheskaya tekhnologiya, 2009, vol. 10, no. 12, pp. 706–712.
- Pravednikova O.B., Dutikova O.S., Karelina I.M. et al. Effect of nano-sized metal compounds on the flameproof properties of plasticized polyvinyl chloride. Fiber Chemistry, 2009, vol. 41 (2), pp. 80–84.
- Nacharkina A.V., Zelenina I.V., Valueva M.I., Barbotko S.L. Fire safety of high-temperature carbon fiber reinforced plastics for aviation purposes (review). Trudy VIAM, 2022, no. 7 (113), paper no. 12. Available at: http://www.viam-works.ru (accessed: August 26, 2024). DOI: 10.18577/2307-6046-2022-0-7-134-150.
- Sorina T.G., Polyakov D.K., Korobko A.P., Penskaya T.V. Vinyl ester resins for pultrusion technology. Elektrotekhnika, 2002, no. 4, pp. 49–51.
- Li P., Yu Y., Yang X. Effects of initiators on the cure kinetics and mechanical properties of vinyl ester resins. Journal of Applied Polymer Science, 2008, vol. 109, is. 4, pp. 2539–2545.
- Garay A., Paese L., Souza J., Amico S. Studies on thermal and viscoelastic properties of vinyl ester resin and its composites with glass fiber. Matéria, 2015, vol. 20, pp. 64–71.
- Fraga A., Alvarez V., Vazquez A., de La Osa O. Relationship between dynamic mechanical properties and water absorption of unsaturated polyester and vinyl ester glass fiber composites. Journal of Composite Materials, 2003, vol. 37, pp. 1553–1574.
- Zhang J., Richardson M. Micro-heterogeneity of urethane vinylester resin networks. Polymer, 2000, vol. 41, is. 18, pp. 6843–6849.
- Borodina I.A., Kozik V.V., Borilo L.P. Effect of natural silicates on the curing of unsaturated polyester resins. Izvestiya Tomskogo politekhnicheskogo universiteta, 2005, vol. 308, no. 3, pp. 118–122.
- Dilmiev V.V., Onina S.A. Features of modification of unsaturated polyester resins on the example of orthophthalic. Vestnik nauki, 2024, vol. 4, no. 5 (74), pp. 1805–1808.