Peculiarities of assessing the resistance of polymeric materials to biodegradation in laboratory conditions

Part 2. Samples and methods for their analysis
Ermishev V.Yu., Laptev A.B., Startsev V.O.
Ermishev V.Yu., Laptev A.B., Startsev V.O. Peculiarities of assessing the resistance of polymeric materials to biodegradation in laboratory conditions. Part 2. Samples and methods for their analysis // Proceedings of VIAM. 2023. No. 8. DOI: 10.18577/2307-6046-2023-0-8-138-148. URL: https://viam-works.ru/en/journal/2023/8/12
Keywords
biodegradation, bacterial strains, enzymatic reactions, synthetic polymer materials, biodegradable polymers (BDP), sample form factor
Abstract

Рresents a brief comparative analysis of domestic and foreign standards for testing non-metallic materials when interacting with microorganisms. Laboratory methods for analyzing the degree of biodegradation of materials used, among other things, in the test standards for synthetic polymers, are given. The significance of the physical dimensions of polymer samples for the search and testing of microorganism strains for the ability to use the chemical component of the material as a nutrient substrate is shown.

Reference list
  1. Kablov E.N. New generation materials and digital technologies for their processing. Vestnik Rossiyskoy akademii nauk, 2020, vol. 90, no. 4, pp. 331–334.
  2. Kablov E.N., Startsev V.O. Systematical analysis of the climatics influence on mechanical properties of the polymer composite materials based on domestic and foreign sources (review). Aviacionnye materialy i tehnologii, 2018, no. 2 (51), pp. 47–58. DOI: 10.18577/2071-9140-2018-0-2-47-58.
  3. Kablov E.N., Laptev A.B., Prokopenko A.N., Gulyaev A.I. Relaxation of polymeric composite materials under the prolonged action of static load and climate (review). Part 1. Binders. Aviation materials and technologies, 2021, no. 4 (65), paper no. 08. Available at: http://www.journal.viam.ru (accessed: March 29, 2023). DOI: 10.18577/2071-9140-2021-0-4-70-80.
  4. Webb H., Arnott J., Crawford R., Ivanova E. Plastic degradation and its environment alimplications with special reference to poly(ethylene terephthalate) // Polymers, 2013, vol. 5, pp. 1–18. DOI: 10.3390/polym5010001.
  5. Ermishev V.Yu. Metabolic possibilities of bacteria with respect to synthetic hydro-carbons used in the production of non-metallic materials (review). Trudy VIAM, 2023, no. 2 (120), paper no. 11. Available at: http://www.viam-works.ru (accessed: March 24, 2023). DOI: 10.18577/2307-6046-2023-0-2-132-146.
  6. Ohtake Y., Kobayashi T., Asabe H. et al. Oxidative degradation and molecular weight change of LDPE buried under bioactive soil for 32–37 years // Journal Applied Polymer Science, 1998, vol. 70, p. 1643–1648. DOI: 10.1002/291097-4622819981128.
  7. Yang H., Chen Z.Q., Wang Y. et al. Composition and structure of microbialite ecosystems following the end-Permian mass extinction in South China // Palaeogeography, Palaeoclimatology, Palaeoecology, 2011, vol. 308, pp. 111–128. DOI: 10.1016/j.palaeo.2010.05.029.
  8. Laptev A.B., Nikolaev E.V., Kurshev E.V., Goryashnik Yu.S. Features of biodegradation of thermoplastics based on polyesters in different climatic zones. Trudy VIAM, 2019, no. 7 (79), paper no. 10. Available at: http://www.viam-works.ru (accessed: March 15, 2023). DOI: 10.18577/2307-6046-2019-0-7-84-91.
  9. Yakovenko T.V., Bukharev G.M., Bobyreva T.V., Pykhtin A.A., Oparina L.A., Parshina L.N. Biocidal additives selection for foamed polyurethanes modification. Trudy VIAM, 2019, no. 7 (79), paper no. 04. Available at: http://www.viam-works.ru (accessed: March 18, 2023). DOI: 10.18577/2307-6046-2019-0-7-34-41.
  10. ASTM D4939-89. Standard Test Method for Subjecting Marine Antifouling Coating to Biofouling and Fluid Shear Forces in Natural Seawater, 2020. Available at: https://www.astm.org/d4939-89r20 (accessed: April 10, 2023). DOI: 10.1520/D4939-89R20.
  11. State Standard 9.803–88. A unified system of protection against corrosion and aging. Fungicides. Method for determining effectiveness. Moscow: Publishing House of Standards, 1998, 28 p.
  12. ASTM E2111-12. Standard Quantitative Carrier Test Method to Evaluate the Bactericidal, Fungicidal, Mycobactericidal, and Sporicidal Potencies of Liquid Chemicals, 2018. Available at: https://www.astm.org/E2111-12r18 (accessed: April 10, 2023). DOI: 10.1520/E2111-12R18.
  13. ASTM E2783-11. Standard Test Method for Assessment of Antimicrobial Activity for Water Miscible Compounds Using a Time-Kill Procedure. Test method, 2016. Available at: https://www.astm.org/E2783-11r16 (accessed: April 10, 2023). DOI: 10.1520/E2783-11R16.
  14. ASTM E645-13. Standard Practice for Evaluation of Microbicides Used in Cooling Water Systems, 2018. Available at: https://www.astm.org/E645-13 (accessed: April 10, 2023). DOI: 10.1520/E0645-13.
  15. State Standard 9.050–75. A unified system of protection against corrosion and aging. Lacoclance coatings. Methods of laboratory tests on resistance to molds. Moscow: Publishing house of standards, 1976, 5 p.
  16. State Standard 9.058–75. A unified system of protection against corrosion and aging. The materials are polymer, wood, fabric, paper, cardboard. Testing methods for resistance to termite damage. Moscow: Publishing house of standards, 1976, 9 p.
  17. ASTM D5588-97. Standard Test Method for Determination of the Microbial Condition of Paint, Paint Raw Materials, and Plant Areas, 2021. Available at: https://www.astm.org/D5588-97r21 (accessed: April 10, 2023). DOI: 10.1520/D5588-97R21.
  18. ASTM D5590-00. Standard Test Method for Determining the Resistance of Paint Films and Related Coatings to Fungal Defacement by Accelerated Four-Week Agar Plate. Available at: https://www.astm.org/ D5590-00 (accessed: April 10, 2023). DOI: 10.1520/D5590-00.
  19. State Standard 9.060–75. A unified system of protection against corrosion and aging. Fabrics. The method of laboratory tests for resistance to microbiological destruction. Moscow: Publishing House of Standards, 1977, 10 p.
  20. ISO 17556-2012. Plastics – Determination of the ultimate aerobic biodegradability of plastic materials in soil by measuring the oxygen demand in a respirometer or the amount of carbon dioxide evolve, 2019. Available at: https://www.iso.org/standard/56089 (accessed: April 10, 2023).
  21. State Standard 9.085–78. A unified system of protection against corrosion and aging. Lubents lubricants. Testing methods for bio resistance. Moscow: Publishing House of Standards, 1978, 5 p.
  22. State Standard 9.023–74. A unified system of protection against corrosion and aging. Oil fuels. The method of laboratory tests of bio resistance of fuels protected by antimicrobial additives. Moscow: Publishing house of standards, 1975, 5 p.
  23. ASTM E1259-16. Standard Practice for Evaluation of Antimicrobials in Liquid Fuels Boiling Below 390 °C, 2018. Available at: https://www.astm.org/E1259-16 (accessed: April 10, 2023). DOI: 10.1520/E1259-16.
  24. State Standard 9.049–91. A unified system of protection against corrosion and aging. The materials are polymer and their components. Methods of laboratory tests on resistance to mold mushrooms. Moscow: Publishing house of standards, 1991, 13 p.
  25. ASTM C1338-08. Standard Test Method for Determining Fungi Resistance of Insulation Materials and Facings, 2014. Available at: https://www.astm.org/C1338-08 (accessed: April 10, 2023). DOI: 10.1520/C1338-08.
  26. ASTM G21-15. Standard Practice for Determining Resistance of Synthetic Polymeric Materials to Fungi, 2021. Available at: https://www.astm.org/G21-15e01 (accessed: April 10, 2023). DOI: 10.1520/G0021-15R21E01.
  27. ASTM D4783-01. Standard Test Methods for Resistance of Adhesive Preparations in Container to Attack by Bacteria, Yeast, and Fungi, 2021. DOI: 10.1520/D4783-01R21.
  28. Lucas N., Bienaime C., Belloy C. et al. Polymer biodegradation: mechanisms and estimation techniques // Chemosphere, 2008, no. 4, p. 429. DOI: 10.1016/j.chemosphere.2008.06.064.
  29. Suvorova A.I., Tyukova I.S. Biodegradable systems: thermodynamics, rheological properties and biocation // Vysokomolekulyarnye soyedineniya, 2008, vol. 50, no. 7, pp. 1162–1171.
  30. ASTM D5338-15. Standard Test Method for Determining Aerobic Biodegradation of Plastic Materials Under Controlled Composting Conditions, 2021. Available at: https://www.astm.org/D5338-15r21 (accessed: April 10, 2023). DOI: 10.1520/D5338-15R21.
  31. ASTM D5509-96. Standard Practice for Exposing Plastics to a Simulated Compost Environment. Available at: https://www.astm.org/ D5509-96 (accessed: April 10, 2023).
  32. Averina A.E., Nikolaev E.V. The use of the method of radioactive indicators to study the mechanisms of structural changes in polymeric materials // Climate 2018: issues of forecasting corrosion, aging and biopersion of materials: Materials III All-Rus. Sci.-tech. Conf. (Gelendzhik, July 19–20, 2018). Moscow: VIAM, 2018, pp. 7–21.
  33. Voges R., Heys J.R., Moenius T. Preparation of compounds labeled with tritium and carbon-14. Wiley, 2009, pp. 682.
  34. Ledderose C., Bao Y., Zhang J., Junger W.G. Novel method for real-time monitoring of ATP release reveals multiple phases of autocrine purinergic signalling during immune cell activation // Acta Physiologica, 2015, vol. 213, pp. 334–345. DOI: 10.1111/apha.12435.
  35. Cho M.H., Niles A., Huang R. et al. A bioluminescent cytotoxicity assay for assessment of membrane integrity using a proteolytic biomarker // Toxicology in Vitro, 2008, vol. 22, pp. 1099–1106. DOI: 10.1016/j.tiv.2008.02.013.
  36. Moravec R.A., O’Brien M.A., Daily W.J. et al. Cell-based bioluminescent assays for all three proteasome activities in a homogeneous format // Analytical Biochemistry, 2009, vol. 387, pp. 294–302. DOI: 10.1016/j.ab.2009.01.016.
  37. Zhang T., Herbert F. Application of real-time polymerase chain reaction for quantification of microorganisms in environmental samples // Applied microbiology and biotechnology, 2006, vol. 70, pp. 281–289. DOI: 10.1007/s00253-006-0333-6.
  38. Zislis T., Mark D.E., Cerbas E.L., Hollinger J.O. Scanning electron microscopic study of cell attachment to biodegradable polymer implants // Journal Oral Implantology, 1989, vol. 15, pp. 160–167.
  39. Funabashi M., Ninomiya F., Kunioka M. Biodegradation of Polycaprolactone Powders Proposed as Reference Test Materials for International Standard of Biodegradation Evaluation Method // Journal of polymers and the environment, 2007, vol. 15, pp. 7–17. DOI: 10.1007/s10924-006-0041-4.