Development of a set of reference samples of casting heat-resistant alloy VZHL718

Min P.G., Yakimovitch P.V., Alekseev A.V.
Min P.G., Yakimovitch P.V., Alekseev A.V. Development of a set of reference samples of casting heat-resistant alloy VZHL718 // Proceedings of VIAM. 2023. No. 8. DOI: 10.18577/2307-6046-2023-0-8-129-137. URL: https://viam-works.ru/en/journal/2023/8/11
Keywords
standard samples, refining, cast heat-resistant alloys, x-ray fluorescence spectrometry, atomic emission spectrometry, glow discharge mass spectrometry, optical emission spectroscopy
Abstract

Рresents the results of the development of a set of standard samples of cast superalloy VZhL718. The process of choosing the optimal composition of the alloy is described, as well as the use of various technologies for obtaining a material suitable for calibrating various spectral equipment: mass spectrometers with a glow discharge, optical emission and х-ray fluorescence spectrometers, etc. The determination of 22 elements (Fe, Al, Cr, Co , Mo, Ti, Nb, Ta, P, Mn, Cu, Zn, As, Se, Cd, Sb, Te, Pb, Bi, V, Ag, Sn) in the obtained standard samples.

Reference list
  1. Kablov E.N., Ospennikova O.G., Svetlov I.L. Highly efficient cooling of GTE hot section blades. Aviacionnye materialy i tehnologii, 2017, no. 2 (47), pp. 3–14. DOI: 10.18577/2071-9140-2017-0-2-3-14.
  2. Bondarenko Yu.A. Trends in the development of high-temperature metal materials and technologies in the production of modern aircraft gas turbine engines. Aviacionnye materialy i tehnologii, 2019, no. 2 (55), pp. 3–11. DOI: 10.18577/2071-9140-2019-0-2-3-11.
  3. Popovich A.A., Panchenko O.V., Naumov A.A., Sviridov A.V., Skupov A.A., Sbitneva S.V. Friction stir welding of aluminum-lithium alloy V-1469-T. Aviacionnye materialy i tehnologii, 2019, no. 4 (57), pp. 11–17. DOI: 10.18577/2071-9140-2019-0-4-11-17.
  4. Min P.G., Vadeev V.E., Kramer V.V. The development of the new VZhM200 superalloy and the technology of its production for casting of the advanced engines’ blades by the directional crystallization. Aviation materials and technologies, 2021, no. 3 (64), paper no. 02. Available at: http://www.journal.viam.ru (accessed: February 11, 2023). DOI: 10.18577/2071-9140-2021-0-3-11-18.
  5. Kablov E.N., Chabina E.B., Morozov G.A., Muravskaya N.P. Assessment of compliance of new materials using highlevel CO and MI. Kompetentnost, 2017, no. 2, pp. 40–46.
  6. Letov A.F., Karachevtsev F.N. Experience in the development of standard samples of aviation alloys. Mir izmereniy, 2012, no. 8, pp. 31–35.
  7. State Standard 8.753–2011. State system for ensuring the uniformity of measurements. Standard materials (substances). Moscow: Standinform, 2011, 19 p.
  8. Shavnev A.A., Babashov V.G., Varrik N.M. Continuous fibers based on alumina (review). Aviacionnye materialy i tehnologii, 2020, no. 4 (61), pp. 27–34. DOI: 10.18577/2071-9140-2020-0-4-27-34.
  9. Kablov E.N., Morozov G.A., Krutikov V.N., Muravskaya N.P. Certification of standard samples of structure of complex-alloyed alloys using standard. Aviacionnye materialy i tehnologii, 2012, no. 2, pp. 9–11.
  10. Handbook of x-ray spectrometry. 2nd ed., rev. and exp. Ed. R.E. Van Grieken, A.A. Marcowicz. New York: Marcel Dekker, Inc., 2001, рр. 14–56.
  11. Karachevtsev F.N., Letov A.F., Protsenko O.M., Yakimova M.S. Development of standard samples of the composition of aviation alloys. Standartnyye obraztsy, 2013, no. 4, pp. 30–34.
  12. Karachevtsev F.N., Rassokhina L.I., Gerasimov V.V., Visik E.M. Obtaining standard samples for express analysis of heat-resistant nickel alloys. Metallurgiya mashinostroyeniya, 2013, no. 6, pp. 18–19.
  13. Parish R.M., Karachevtsev F.N., Zakvzdkina T.N., mechanic E.A. Determination of the chemical composition of highly lifted nickel alloys of aviation purposes by NPES-ISP in combination with microwave sampling. Zavodskaya laboratoriya. Diagnostika materialov, 2013, vol. 79, no. 9, pp. 6–9.
  14. Saka T. Glow discharge mass spectrometry. Compendium of Surface and Interface Analysis, 2018, vol. 36, pp. 211–217.
  15. Hu J., Wang H. Determination of Trace Elements in Super Alloy by ICP-MS. Mikrochimica Acta, 2001, vol. 137, pp. 149–155.