Influence of climatic conditions on CFRP VKU-39 after three year outdoor exposition in eight climatic zones
Veligodsky I.M., Koval T.V., Gulyaev I.N. Influence of climatic conditions on CFRP VKU-39 after three year outdoor exposition in eight climatic zones // Proceedings of VIAM. 2023. No. 8. DOI: 10.18577/2307-6046-2023-0-8-113-128. URL: https://viam-works.ru/en/journal/2023/8/10
Keywords
natural climatic tests, CFRP, optical microscopy, flexural strength, compressive strength, dynamic mechanical analysis, moisture saturation of polymer composites
Abstract
The climatic resistance of CFRP to influence of eight types of climate of different climatic zones during the three year exposition were investigated. Exposed polymer composite was studied by optical microscopy, dynamical mechanical analysis, moisture saturation, flexural strengthandcompressive strength of polymer composite were determined. Deterioration of upper layer of polymer matrices after exposition was shown. Relationship between climatic factors influence on polymer composites, changing of polymer matrices condition and decreasing of material strength was found.
Reference list
- Nurmukhametova A.N., Zenitova L.A. Carbon fiber. Market conditions, demand structure, promising markets for products based on it, areas of application. Butlerovskiye soobshcheniya, 2022, vol. 72, no. 10, pp. 102–130. DOI: 10.37952/ROI-jbc-01/2272-10-102.
- Kablov E.N. Materials of the new generation – the basis of innovation, technological leadership and national security of Russia. Intellekt i tekhnologii, 2016, no. 2, pp. 16–22.
- Molchanov B.I., Gudimov M.M. Properties of carbon plastics and their applications. Aviatsionnaya promyshlennost, 1997, no. 3-4, pp. 58–60.
- Lebedeva O.V., Sipkina E.I. Polymer composites and their properties. Izvestiya vuzov. Prikladnaya khimiya i biotekhnologiya, 2022. Vol. 12. No. 2 (41), pp. 192–207. DOI: 10.21285/2227-2925-2022-12-2-192-207.
- Kolesnik K.A. Modeling of moisture saturation in polymer composites in real climatic environmental conditions. Aviacionnye materialy i tehnologii, 2017, no. 4 (49), pp. 77–86. DOI: 10.18577/2071-9140-2017-0-4-77-86.
- Kablov E.N., Laptev A.B., Prokopenko A.N., Gulyaev A.I. Relaxation of polymeric composite materials under the prolonged action of static load and climate (review). Part 1. Binders. Aviation materials and technologies, 2021, no. 4 (65), paper no. 08. Available at: http://www.journal.viam.ru (accessed: December 23, 2022). DOI: 10.18577/2071-9140-2021-0-4-70-80.
- Donetsky K.I., Karavaev R.Yu., Bystrikova D.V., Mishchun M.I. Properties of carbon fiber reinforced plastic based on a biaxial volume-reinforcing braided preform for the manufacture of elements of tubular structures. Konstruktsii iz kompozitsionnykh materialov, 2022, no. 2 (166), pp. 8–14. DOI: 10/52190/2073-2562_2022_2_8.
- Mishurov K.S., Mishkin S.I. Environmental effect on properties of CFRP (Carbon Fiber Reinforced Plastic) VKU-39. Trudy VIAM, 2016, no. 12 (48), paper no. 08. Available at: http://www.viam-works.ru (accessed: December 23, 2022). DOI: 10.18577/2307-6046-2016-0-12-8-8.
- Imametdinov E.Sh., Kondrashov S.V., Gulyaev I.N., Terekhov I.V. Comparative evaluation of the effect of modification with thermoplastic powders on the value of residual compressive strength of carbon fiber. Vse materialy. Entsiklopedicheskiy spravochnik, 2022, no. 7, pp. 22–31.
- Gulyaev A.I., Yakovlev N.O., Krylov V.D., Lashov O.A. Application of fractographic analysis in the study of interlayer fracture of PCM. Aviaсionnye materialy i tehnologii, 2017, no. 3 (48), pp. 65–73. DOI: 10.18577/2071-9140-2017-0-3-65-73.
- Semyonova L.V., Nefyodov N.I. Recovery technology for PWC systems with polyurethane enamel for the operating aviation articles after wornout PLC removal. Aviacionnye materialy i tehnologii, 2014, no. S3, pp. 47–50. DOI: 10.18577/2071-9140-2014-0-s3-47-50.
- Yakovlev N.O., Gulyaev A.I., Lashov O.A. Crack firmness of layered polymeric composite materials (review). Trudy VIAM, 2016, no. 4, paper no. 12. Available at: http://www.viam-works.ru (accessed: December 23, 2022) DOI: 10.185772307-6046-2016-0-4-12-12.
- Sorokin A.E., Ivanov M.S., Sagomonova V.A. Thermoplastic polymer composite materials based on polyetheretherketones of various manufacturers. Aviation materials and technologies, 2022, no. 1 (66), paper no. 04. Available at: http://www.journal.viam.ru (accessed: December 23, 2022). DOI: 10.18577/2071-9140-2022-0-1-41-50.
- Gunyaeva A.G., Sidorina A.I., Kurnosov A.O., Klimenko O.N. Polymeric composite materials of new generation on the basis of binder VSE-1212 and the filling agents alternative to ones of Porcher Ind. and Toho Tenax. Aviacionnye materialy i tehnologii, 2018, no. 3 (52), pp. 18–26. DOI: 10.18577/2071-9140-2018-0-3-18-26.
- Chertishchev V.Yu., Ospennikova O.G., Boichuk A.S., Dikov I.A., Generalov A.S. Determina-tion of the size and depth of defects in multilayer PCM honeycomb structures based on the mechanical impedance value. Aviaсionnye materialy i tehnologii, 2020, no. 3 (60), pp. 72–94. DOI: 10.18577/2071-9140-2020-0-3-72-94.
- Donetsky K.I., Timoshkov P.N., Safronov A.M. Non-autoclave molding of prepregs. Konstruktsii iz kompozitsionnykh materialov, 2022, no. 1 (165), pp. 29–34. DOI: 10.52190/2073-2562_2022_1_29.
- Marakhovsky P.S., Vorobyov N.N., Gulyaev A.I., Tkachuk A.I. Influence of polyarylsulfone additives on the climatic resistance of epoxy-based carbon fiber. Vysokomolekulyarnye soyedineniya. Seriya A, 2022, vol. 64, no. 2, pp. 113–119.
- Strungar E.M., Staroverov O.A., Lunegorova E.M. Comprehensive assessment of the processes of fatigue accumulation of damage and destruction of samples with operational stress concentrators. Diagnostics, Resource and Mechanics of materials and structures, 2022, no 4, pp. 37–49. DOI: 10.17804./2410.-08.2022.4.037.-049.
- Veligodskiy I.M., Koval T.V., Kurnosov A.O., Marakhovskiy P.S. Study of resistance of glass fiber reinforced plastic to natural weathering in different climatic conditions. Trudy VIAM, 2022, no. 11 (117), paper no. 12. Available at: http://www.viam-works.ru (accessed: December 23, 2022). DOI: 10.18577/2307-6046-2022-0-11-134-148.
- Salnikov V.G., Startsev O.V., Lebedev M.P., Kopyrin M.M., Vapirov Yu.M. Influence of daily and seasonal changes in relative humidity and temperature on the moisture saturation of carbon fiber in open climatic conditions. Vse materialy. Entsiklopedicheskiy spravochnik, 2022, no. 5, pp. 2–10.
- Donetskiy K.I., Karavayev R.Yu., Tsybin A.I., Veshkin E.A., Mikhaldykin E.S. Constructional fiberglass plastic for manufacturing of enclosing sheeting elements. Aviacionnyye materialy i tehnologii, 2017, no. 3 (48), pp. 56–64. DOI: 10.18577/2071-9140-2017-0-3-56-64.