Technology of braze design type «blisk» from dissimilar alloys

Rylnikov V.S., Afanasiev-Khodykin A.N., Galushka I.A.
Rylnikov V.S., Afanasiev-Khodykin A.N., Galushka I.A. Technology of braze design type «blisk» from dissimilar alloys // Proceedings of VIAM. 2013. No. 10. URL: https://viam-works.ru/en/journal/2013/10/2
Abstract

In the article the problem of producing high-strength permanent connection of dissimilar alloys intermetallic alloy monocrystal VKNA-4Y and deformed nickel superalloy EP975 in relation to the construction type «blisk». The processes occurring in the process of diffusion brazing and soldering behavior of the alloying elements and solder in the solder materials and brazed heat-affected zones.