Heat-resistant aluminum alloys 1151 and B-1213 welded fuselage panels fabrication and testing

Antipov V.V., Panteleev M.D., Sviridov A.V., Skupov A.A., Odintsov N.S.
Antipov V.V., Panteleev M.D., Sviridov A.V., Skupov A.A., Odintsov N.S. Heat-resistant aluminum alloys 1151 and B-1213 welded fuselage panels fabrication and testing // Proceedings of VIAM. 2023. No. 5. DOI: 10.18577/2307-6046-2023-0-5-33-42. URL: https://viam-works.ru/en/journal/2023/5/3
Keywords
laser welding, heat-resistant, aluminum alloy, microstructure, mechanical properties
Abstract

The welded joints heat-resistant aluminum alloys V-1213 and 1151 were researched. The welded joints were performed according to the tested modes on the Laser Weld 8R60 laser welding complex. The properties joints, provided within ones and twice welding were given. The strength level of welded fuselage elements with an intermittent asymmetrical seam; with an intermittent symmetrical seam, with a continuous seam is investigated. The tests results of welded stringer panels with the bearing capacity determination during shear are presented.

Reference list
  1. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N., Antipov V.V., Klochkova Yu.Yu. Aluminium-lithium alloys of a new generation and layered aluminum-glass plastics based on them. Tsvetnye metally, 2016, no. 8 (884), pp. 86–91. DOI: 10.17580/tsm.2016.08.13.
  3. Kablov E.N. Modern materials – the basis of innovative modernization of Russia. Metally Evrazii, 2012, no. 3, pp. 10–15.
  4. Kablov E.N. Materials for aerospace engineering. Vse materialy. Entsiklopedicheskiy spravochnik, 2007, no. 5, pp. 7–27.
  5. Bliznyuk V., Vasiliev L., Vul V. et al. The truth about supersonic and passenger aircraft. Moscow: Moskovsky Rabochiy, 2000, 335 p.
  6. Altman M.B., Andreev G.N., Arbuzov Yu.P. et al. Application of aluminum alloys. Moscow: Metallurgy, 1985, 344 p.
  7. Fomin V.M., Malikov A.G., Orishich A.M., Antipov V.V., Klochkov G.G., Skupov A.A. Heat treatment effect on structure of joint weld sheets from V-1469 alloy of Al–Cu–Li system manufactured by laser welding. Aviacionnye materialy i tehnologii, 2018, no. 1 (50), pp. 9–18. DOI: 10.18577/2071-9140-2018-0-1-9-18.
  8. Bulina N.V., Malikov A.G., Orishich А.М., Klochkov G.G. Research of the structural-phase composition of laser weld joint depending on the thermal processing of the aluminum alloy V-1469. Aviacionnye materialy i tehnologii, 2019, no. 2 (55), pp. 31–39. DOI: 10.18577/2071-9140-2019-0-2-31-39.
  9. Panteleev M.D., Bakradze M.M., Skupov A.A., Scherbakov A.V., Belozor V.E. Technological features of fusion welding of aluminum alloy V-1579. Aviacionnye materialy i tehnologii, 2018, no. 3 (52), pp. 11–17. DOI: 10.18577/2071-9140-2018-0-3-11-17.
  10. Rokhlin L.L., Bochvar N.R., Dobatkina T.V. Joint influence of some transition metals on the change in the phase composition and recrystallization of aluminum. Tekhnologiya legkikh splavov, 2009, no. 2, pp. 20–27.
  11. Grigorev M.V., Antipov V.V., Vakhromov R.O. et al. Structure and properties of ingots from Al–Cu–Mg system alloy with silver microadditives. Aviacionnye materialy i tehnologii, 2013, no. 3, pp. 3–6.
  12. Ivanova A.O., Vahromov R.O., Grigor'ev M.V., Senatorova O.G. Effect of small additive of silver on structure and properties of Al–Cu–Mg alloys. Trudy VIAM, 2014, no. 10, paper no. 01. Available at: http://www.viam-works.ru (accessed: December 01, 2022). DOI: 10.18577/2307-6046-2014-0-10-1-1.
  13. Aluminum alloy and product made from it: pat. 2278179 Rus. Federation; filed 21.12.04; publ. 20.06.06.
  14. Oglodkova Yu.S., Lukina E.A., Vakhromov R.O., Antipov K.V. Influence of artificial aging regimes on the structure and properties of the high-temperature alloy V-1213 of the Al–Cu–Mg–Ag system. Metallovedenie i termicheskaya obrabotka metallov, 2014, no. 8 (710), pp. 13–19.
  15. Chirkov E.F., Kononova L.A., Shmelyova V.S. Effect of equiatomic cu and mg content on ageing processes of 1151 (Al–Cu–Mg) high-temperature weldable structural alloy. Aviacionnye materialy i tehnologii, 2013, no. S2, pp. 20–24.
  16. Chirkov E.F. Rate of loss of strength when heatings – criterion of assessment of thermal stability of structural alloys of Al–Cu–Mg and Al–Cu systems. Trudy VIAM, 2013, no. 2, paper no. 02. Available at: http://www.viam-works.ru (accessed: December 01, 2022).
  17. Panteleev M.D., Sviridov A.V., Skupov A.A., Odintsov N.S. Aluminum-Lithium alloy V-1469 welded fuselage constructions survivability. Aviation materials and technologies, 2022, no. 1 (69), paper no. 03. Available at: http://www.journal.viam.ru (accessed: December 01, 2022). DOI: 10.18577/2713-0193-2022-0-4-25-35.
  18. Dittrich D., Standfuss J., Liebscher J. et al. Laser Beam Welding of Hard to Weld Al Alloys for a Regional Aircraft Fuselage Design – First Results. Physics Procedia, 2011, no. 12, pp. 113–122.