Analytical control of the chemical composition of galvanic electrolytes of nickel plating by the ICP AES and ICP MS methods

Dvoretskov R.M., Karachevtsev F.N., Dyomin S.A.
Dvoretskov R.M., Karachevtsev F.N., Dyomin S.A. Analytical control of the chemical composition of galvanic electrolytes of nickel plating by the ICP AES and ICP MS methods // Proceedings of VIAM. 2023. No. 3. DOI: 10.18577/2307-6046-2023-0-3-117-131. URL: https://viam-works.ru/en/journal/2023/3/11
Keywords
analytical control, galvanic nickel plating, nickel sulfate, nickel chloride, electrolytes, inductively coupled plasma atomic emission spectrometry (ICP AES), inductively coupled plasma mass-spectrometry (ICP MS)
Abstract

This work is devoted to the issues of determining the chemical composition of galvanic nickel plating electrolytes using the methods of atomic emission spectrometry and inductively coupled plasma mass spectrometry. The mass fraction of components in model electrolyte solutions at different dilutions was determined. The metrological characteristics of the obtained results were evaluated. Concentration ranges were chosen to which it is optimal to dilute stock solutions in order to obtain reproducible and reliable results.

Reference list
  1. Khmeleva K.M., Kozlov I.A., Nikitin Ya.Yu., Nikiforov A.A. Modern trends of protective galvanic coatings working at high temperatures (review). Trudy VIAM, 2020, no. 12 (94), paper no. 07. Available at: http://www.viam-works.ru (accessed: July 04, 2022). DOI: 10.18577/2307-6046-2020-0-12-75-86.
  2. Vinogradov S.S., Nikiforov A.A., Demin S.A., Chesnokov D.V. Protection against corrosion of carbon steel. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 242–263. DOI: 10.18577/2071-9140-2017-0-S-242-263.
  3. Skryabin V.A., Fomichev V.O. Peculiarities of applying nickel coatings to parts made of steels and aluminum alloys. Nauchnye vesti, 2020, no. 1 (18), pp. 116–119.
  4. Vinogradov S.S., Nikiforov A.A., Balahonov S.V., Leshhev K.A. Ni–B chemical coating’s structure and properties investigation. Trudy VIAM, 2014, no. 12, paper no. 07. Available at: http://www.viam-works.ru (accessed: July 16, 2022). DOI: 10.18577/2307-6046-2014-0-12-7-7.
  5. Borisenko A.B., Khramtsov V.V., Nemtinov V.A., Krylov A.V., Matrokhin M.A. Development of the design of a chemical nickel plating plant operating as part of a galvanic line. Vestnik Tambovskogo gosudarstvennogo tekhnicheskogo universiteta, 2021, vol. 27, no. 2, pp. 275–284.
  6. Vinogradov S.S., Nikiforov A.A., Zakirova L.I. Cadmium replacement. Stage 2 – final. Galvanic thermal coating of zinc–tin system – real alternative to cadmium plating. Aviacionnye materialy i tehnologii, 2019, no. 3 (56), pp. 59–66. DOI: 10.18577/2071-9140-2019-0-3-59-66.
  7. Abramova M.G. Revisiting the confirmation of the identity of the corrosion destruction mechanism of aluminum alloys (review). Part 1. Atmospheric corrosion. Aviacionnye materialy i tehnologii, 2020, no. 4 (61), pp. 86–94. DOI: 10.18577/2071-9140-2020-0-4-86-94.
  8. Abramova M.G. Revisiting the confirmation of the identity of the corrosion destruction mechanism of aluminum alloys (review). Part 2. Corrosion in sea water. Aviation materials and technology, 2021, no. 1 (62), paper no. 09. Available at: http://www.journal.viam.ru (accessed: August 20, 2022). DOI: 10.18577/2713-0193-2021-0-1-95-103.
  9. Churilov D.G., Stekolnikov Yu.A., Arapov I.S. Restoration of parts using combined composite coatings with further hardening. Sovremennye materialy, tekhnika i tekhnologii, 2021, no. 1 (34), pp. 52–58.
  10. Nochovnaya N.A., Bazyleva O.A., Kablov D.E., Panin P.V. Intermetallic alloys based on titanium and nickel. Ed. E.N. Kablov. Moscow: VIAM, 2018, 308 p.
  11. Kablov E.N., Sidorov V.V., Min P.G., Vadeev V.E., Kramer V.V. Research and development of technological parameters of vacuum melting of corrosion-resistant heat-resistant nickel alloys. Metallurg, 2021, no. 2, pp. 62–67.
  12. Nikiforov A.A., Demin S.A., Khmeleva K.M. Electrochemical treatment of parts obtained by selective laser fusion. Trudy VIAM, 2021, no. 7 (101), paper no. 01. Available at: http://www.viam-works.ru (accessed: July 25, 2022). DOI: 10.18577/2307-6046-2021-0-7-3-12.
  13. Goncharov B.E., Sipatov A.M., Cherkashneva N.N., Pleskan A.Yu., Samokhvalov N.Yu., Vaganova M.L., Sorokin O.Yu., Solntsev St.S., Evdokimov S.A. Studies of thermal shock resistance of an anti-oxidation coating for a multi-layered ceramic composite. Aviation materials and technologies, 2021, no. 4 (65), paper no. 06. Available at: http://www.journal.viam.ru (accessed: August 12, 2022). DOI: 10.18577/2713-0193-2021-0-51-58.
  14. Zakirova L.I., Laptev A.B. Properties of protective electroplating coatings for replacement of cadmium on steel fixing parts (review). Part 1. Morphology and corrosion resistance. Aviaсionnye materialy i tehnologii, 2020, no. 3 (60), pp. 37–46. DOI: 10.18577/2071-9140-2020-0-3-37-46.
  15. Laptev A.B., Zakirova L.I., Degovets M.L. Properties of protective galvanic coatings for replacement of cadmium on steel fixing parts (review). Part 2. Hydrogen embrittlement and frictional characteristics. Aviacionnye materialy i tehnologii, 2020, no. 4 (61), pp. 35–40. DOI: 10.18577/2071-9140-2020-0-4-35-40.
  16. Tikhonov R.D. Electrochemical deposition of NIFE alloy from concentrated chloride electrolyte. Nano- i mikrosistemnaya tekhnika, 2020, vol. 22, no. 8, pp. 422–433.
  17. Sevostyanov N.V. Automation of the selection of copper-nickel plating and technological parameters of deposition. Korroziya: materialy, zashchita, 2015, no. 4, pp. 9–16.
  18. Skopintsev V.D., Vinokurov E.G. Energy efficiency of the process of chemical nickel plating of surfaces. Khimicheskaya tekhnologiya, 2020, vol. 21, no. 10, pp. 434–440.
  19. Salakhova R.K., Tikhoobrazov A.B., Farafonov D.P., Smirnova T.B. Features of electrolytic deposition of abrasive-wear-resistant nickel-based coatings. Trudy VIAM, 2022, no. 2 (108), paper no. 08. Available at: http://www.viam-works.ru (accessed: July 26, 2022). DOI: 10.18577/2307-6046-2022-0-2-99-110.
  20. Smirnov G.A. Nickel layer control on metallized ceramics. Steklo i keramika, 2021, no. 5, pp. 9–13.
  21. Balyueva Yu.A., Sosnovskaya N.G., Rozentsveig I.B. Shine-forming action of trichloroethylamides with thioamide functions in the technology of electrochemical nickel plating. Sovremennye tekhnologii i nauchno-tekhnicheskiy progress, 2022, no. 9, pp. 11–12.
  22. Butrik R.V., Grabelnykh V.A., Sosnovskaya N.G., Korchevin N.A. Isothiuronium derivatives of pyridine as brightening additives in electrochemical nickel plating. Sovremennye tekhnologii i nauchno-tekhnicheskiy progress, 2021, no. 8, pp. 19–20.
  23. Sosnovskaya N.G., Istomina N.V., Korchevin N.A., Rozentsveig I.B. Influence of the structure of organic additives on the formation of shiny coatings during electrochemical nickel plating. Uspekhi v khimii i khimicheskoy tekhnologii, 2021, vol. 35, no. 5 (240), pp. 54–56.
  24. Soloveva I.A., Solovev D.S., Litovka Yu.V. Search for the current strength and degree of loading of the drum to reduce the unevenness of the galvanic coating of small parts. Prikaspiyskiy zhurnal: upravleniye i vysokiye tekhnologii, 2022, no. 2 (58), pp. 119–126.
  25. Hamburg Yu.D. Galvanic coatings. Application guide. Moscow: Technosfera, 2006, 216 p.
  26. Vyacheslavov P.M., Shmeleva N.M. Control of electrolytes and coatings. Leningrad: Mashinostroenie, 1985. 96 p.
  27. Karpov Yu.A. Analytical control of metallurgical production. Moscow: Metallurgiya, 1995, pp. 97–107.
  28. Nadezhdina M.E. Progressive technological processes of organization of production of enterprises of the chemical industry. Polzunovskiy almanakh, 2020, no. 1, pp. 55–58.
  29. Nadezhdina M.E., Shinkevich A.I., Shinkevich M.V. Monitoring system for digital production of an enterprise of the petrochemical industry. Competence, 2021, no. 7, pp. 36–39.
  30. Yakimovich P.V., Alekseev A.V. Wastewater analysis by ICP-MS. Metallurg, 2018, no. 1, pp. 13–18.
  31. Garmash A.V., Sorokina N.M. Metrological bases of analytical chemistry. Moscow: Lomonosov Moscow State University, 2012, 47 p.
  32. Nadezhdina M.E., Bobkov V.I. Implementation of the principles of system analysis of chemical technology in the transition to industry 4.0. Days of Student Science: collection of sci. Works of III Intern. stud. conf. Kazan, 2020, pp. 366–369.
  33. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  34. Karachevtsev F.N., Alekseev A.V., Letov A.F., Dvoretskov R.M. Plasma methods of nickel alloys elemental chemical composition analysis. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 483–497. DOI: 10.18577/2071-9140-2017-0-S-483-497.