Application area and physical and mechanical properties of phenol-rubber foam plastic grade FK-20
Kapustianskaia M.A., Mishurov K.S., Studenov I.G. Application area and physical and mechanical properties of phenol-rubber foam plastic grade FK-20 // Proceedings of VIAM. 2023. No. 3. DOI: 10.18577/2307-6046-2023-0-3-3-12. URL: https://viam-works.ru/en/journal/2023/3/1
Keywords
foam plastic, composite material, polymer, microstructure, rubber, phenolic aldehyde oligomers
Abstract
The main physical and mechanical properties of FK-20 phenolic foam based on the products of combination of nitrile rubbers with phenolic aldehyde oligomers have been studying. This foam use as a heat-resistant structural filler for three-layer structures and the manufacture of various structural elements. The results of the study of the microstructure of the foam plastic grade FK-20 and the effect of elevated temperature on the values of its compressive strength are shown. It is established that the foam is efficient at a temperature of 120 °C.
Reference list
- Zastrogina O.B., Sinyakov S.D., Serkova E.А. Materials based on phenolformaldehyde oligomers of resol and novolac tipes (review). Part 2. Trudy VIAM, 2021, no. 11 (105), paper no. 06. Available at: http://www.viam-works.ru (accessed: September 13, 2022). DOI: 10.18577/2307-6046-2021-0-11-55-65.
- Samatadze A.I., Parahin I.V., Porosova N.F., Tumanov A.S. Production of phenolic-elastomer foams by sulfur-free vulcanization. Aviacionnye materialy i tehnologii, 2013, no. 3, pp. 49–52.
- Raskutin A.E. Development strategy of polymer composite materials. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 344–348. DOI: 10.18577/2071-9140-2017-0-S-344-348.
- Mukhametov R.R., Petrova A.P. Thermosetting binders for polymer composites (review). Aviacionnye materialy i tehnologii, 2019, no. 3 (56), pp. 48–58. DOI: 10.18577/2071-9140-2019-0-3-48-58.
- Kolosova A.S., Pikalov E.S. Modern gas-filled polymeric materials and products. Mezhdunarodny zhurnal prikladnykh i fundamentalnykh issledovaniy, 2020, no. 10, pp. 54–67.
- Lavrov N.A. Traditions and innovations in chemistry and technology of polymers. Plasticheskie massy, 2021, no. 7–8, pp. 3–7. DOI: 10.35164/0554-2901-2021-7-8-3-7.
- Berlin A.A., Shutov F.A. Foam polymers based on reactive oligomers. Moscow: Khimiya, 1978, 296 p.
- Parakhin I.V., Tumanov A.S. Phenolic-rubber foamed plastic of higher increased plasticity. Aviacionnye materialy i tehnologii, 2014, no. 4, pp. 65–67. DOI: 10.18577/2071-9140-2014-0-4-65-67.
- Samatadze A.I., Parakhin I.V., Porosova N.F. The choice of plasticizer for phenol-rubber foam. Kompozity i nanostruktury, 2014, vol. 6, no. 2, pp. 117–124.
- Kablov E.N. The main results and directions of development of materials for advanced aviation technology. 75 years. Aviation materials. Moscow: VIAM, 2007, pp. 20–26.
- Kablov E.N. Materials for aerospace engineering. Vse materialy. Entsiklopedicheskiy spravochnik, 2007, no. 5, pp. 7–27.
- Yakusheva N.A. High-strength constructional steels for landing gears of perspective products of aircraft equipment. Aviacionnye materialy i tehnologii, 2020, no. 2 (59), pp. 3–9. DOI: 10.18577/2071-9140-2020-0-2-3-9.
- Semenova S.N., Chaykun A.M., Suleymanov R.R. Ethylene-propylene-diene rubber and its use in rubber materials for special purposes (review). Aviacionnye materialy i tehnologii, 2019, no. 3 (56), pp. 23–30. DOI: 10.18577/2071-9140-2019-0-3-23-30.
- Kablov E.N. Without new materials, there is no future. Metallurg, 2013, no. 12, pp. 4–8.
- Khimenko G.S., Popov V.A., Fleishman S.L. The use of foam material FK-20-ST in the production of reflectors for antennas of radio-electronic aircraft equipment. Foam plastics: collection of articles. Ed. A.A. Moiseeva, V.V. Pavlova, M.Ya. Borodin. Moscow: Oborongiz, 1960, pp. 109–116.