Foam ceramic filters based on domestic refractory materials

Part 1
Deynega G.I., Kuzmina I.G., Bityutskaya O.N., Narskiy A.R.
Deynega G.I., Kuzmina I.G., Bityutskaya O.N., Narskiy A.R. Foam ceramic filters based on domestic refractory materials. Part 1 // Proceedings of VIAM. 2023. No. 11. DOI: 10.18577/2307-6046-2023-0-11-17-25. URL: https://viam-works.ru/en/journal/2023/11/2
Keywords
foam ceramic filters, foundry production, superalloys, ceramic suspension, refractories, mechanical properties, zirconium (IV) oxide
Abstract

In the first part of the study conducted at the National Research Center «Kurchatov Institute» – VIAM, the technology of manufacturing foam ceramic filters designed to purify the melt from non-metallic inclusions is considered. Technological parameters for the manufacture of foam ceramic filters using domestic refractory materials have been developed, several experimental samples of filters based on aluminum oxide (III) and zirconium oxide (IV) have been manufactured, their physical and mechanical properties have been determined. The full compliance of the properties of the manufactured filters with the requirements of the technical specification has been established.

Reference list
  1. Echin A.B., Deynega G.I., Narsky A.R. New developments of NRC «Kurchatov Institute» – VIAM in the field of materials for casting processes of superalloys. Trudy VIAM, 2023, no. 8 (126), paper no. 02. Available at: http://www.viam-works.ru (accessed: September 11, 2023). DOI: 10.18577/2307-6046-2023-0-8-13-24.
  2. Kablov E.N., Shompolov E.G., Sidorov V.V., Rigin V.E., Kayumov R.G. Organization of production of cast rod (charge) billets from nickel casting heat-resistant alloys. Elektrometallurgiya, 2007, no. 1, pp. 2–5.
  3. Bondarenko Yu.A. Trends in the development of high-temperature metal materials and technologies in the production of modern aircraft gas turbine engines. Aviacionnye materialy i tehnologii, 2019, no. 2 (55), pp. 3–11. DOI: 10.18577/2071-9140-2019-0-2-3-11.
  4. Echin A.B., Bondarenko Yu.A., Kolodyazhny M.Yu., Surova V.A. Review of perspective high-temperature superalloys based on refractory non-metallic materials for production of gas turbine engines. Aviation materials and technologies, 2023, no. 3 (72), paper no. 03. Available at: http://www.journal.viam.ru (accessed: September 11, 2023). DOI: 10.18577/2713-0193-2023-0-3-30-41.
  5. Kablov E.N., Ospennikova O.G., Sidorov V.V., Rigin V.E., Kablov D.E. Features of the technology of smelting and casting modern foundry high-heat-resistant nickel alloys. Vestnik MGTU im. N.E. Baumana. Ser.: Mechanical engineering, 2011, no. SP2, pp. 68–78.
  6. Sidorov V.V., Iskhodzhanova I.V., Rigin V.E., Folomeikin Yu.I. Evaluation of filtration efficiency during casting of complex-alloyed nickel melt. Elektrometallurgiya, 2011, no. 11, pp. 17–21.
  7. Kablov E.N., Sidorov V.V., Kablov D.E., Min P.G. The metallurgical fundamentals for high quality maintenance of single crystal heat-resistant nickel alloys. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 55–71. DOI: 10.18577/2071-9140-2017-0-S-55-71.
  8. Demchenko A.I., Shevyakov V.F., Korovin V.A., Belyaev S.V., Gushchin V.N. Improving the quality of nickel alloy by filtration through a ceramic foam filter. Liteyshchik Rossii, 2019, no. 6, pp. 29–33.
  9. Staroverov Yu.S., Chernov Yu.A. Application of ceramic foam filters in foundries and steelmaking abroad. Ogneupory, 1992, no. 1, pp. 38–40.
  10. Ofitserov A.A., Zavolosnov B.S. Foam ceramic filters for filtration of heat-resistant nickel alloys. Liteynoe proizvodstvo, 1993, no. 4, pp. 19–20.
  11. Babashov V.G., Varrik N.M., Karaseva T.A. Porous ceramic for filtration of metal melts and hot gases (rеview). Trudy VIAM, 2020, no. 8 (90), paper no. 6. Available at: http://www.viam-works.ru (accessed: August 24, 2023). DOI: 10.18577/2307-6046-2020-0-8-54-63.
  12. Ten E.B., Voevodina M.A. Filtration of high-strength cast iron melt. Liteynoe proizvodstvo, 1993, no. 7, pp. 5–8.
  13. Dibrov I.A., Kozlov A.V. Developments in the field of melting, pouring, modifying and refining foundry alloys. Liteynoe proizvodstvo, 2000, no. 6, pp. 24–26.
  14. Emelyanov V.O., Martynov K.V., Mutilov V.N., Sokolov A.V., Sukhanova V.P. Aqueous solution of silica sol as an alternative to ethyl silicate in LVM. Liteynoe proizvodstvo, 2012, no. 3, pp. 30–31.
  15. Min P.G., Vadeev V.E. The development and introduction into serial production of the new superalloy VZhL125 for the advanced aviation engines vanes. Aviation materials and technologies, 2023, no. 1 (70), paper no. 01. Available at: http://www.journal.viam.ru (accessed: August 24, 2023). DOI: 10.18577/2713-0193-2023-0-3-3-14.