Study of the habitus of mullite crystals in composite ceramics «mullite–zirconium dioxide»
UDC
666.762.14
DOI
10.18577/2307-6046-2023-0-1-119-127
Article PDF (Russian)
(710.41 KB)
How to cite
Maximov V.G., Babashov V.G., Varrik N.M., Lyulyukina G.Yu. Study of the habitus of mullite crystals in composite ceramics «mullite–zirconium dioxide» // Proceedings of VIAM. 2023. No. 1. DOI: 10.18577/2307-6046-2023-0-1-119-127. URL: https://viam-works.ru/en/journal/2023/1/10
Keywords
ceramic composite material, sol-gel method, mullite, zirconium dioxide, crystal structure, habitus
Abstract
Presents the results of studying the microstructure features of the ceramic composite material «mullite–zirconium dioxide». It is confirmed that the crystals of mullite, as in traditional mullite ceramics, have the habit of a long four-sided prism. Zirconium dioxide crystals provide hardening of the material by the mechanism of turning the crack to the interface, which, in combination with the specific habitus of the crystals of the main phase, leads to the formation of a characteristic highly developed fracture surface and improves the resistance of the material to cracking.
Reference list
- Kablov E.N., Evgenov A.G., Petrushin N.V., Bazyleva O.A., Mazalov I.S., Dynin N.V. New generation materials and digital additive technologies for the production of resource parts FSUE "VIAM". Part 3. Adaptation and creation of materials. Elektrometallurgiya, 2022, no. 4, pp. 15–25.
- Kablov E.N. Marketing of materials science, aircraft building and industry: present and future. Direktor po marketingu i sbytu, 2017, no. 5–6, pp. 40–44.
- Popov R.Yu., Dyatlova E.M., Sergievich O.A., Pogrebenkov V.M. Influence of modifying refractory and high-strength additives on the physical and technical characteristics of mullite-cordierite ceramics. Trudy Kolskogo nauchnogo tsentra RAN, 2018, no. 2-2, pp. 889–894. DOI: 10.25702/KSC.2307-5252.2018.9.1.889-894.
- Sadik C., El Amranib I.-E., Albizane A. Recent advances in silica-alumina refractory: A review. Journal of Asian Ceramic Societies, 2014, vol. 2, pp. 83–96.
- Lebedeva Yu.E., Shchegoleva N.E., Voronov V.A., Solntcev S.S. Al2O3 and ZrO2 ceramic materials obtained by sol-gel method. Trudy VIAM, 2021, no. 4 (98), paper no. 05. Available at: http://www.viam-works.ru (accessed: July 1, 2022). DOI: 10.18577/2307-6046-2021-0-4-61-73.
- Lebedeva Yu.E., Shchegoleva N.E., Voronov V.A., Kovaleva V.S., Chainikova A.S. Effect of modifying zirconium oxide additive on the properties of ceramic materials of the Y2O3–Al2O3–SiO2 system obtained by the sol-gel method. Trudy VIAM, 2021, no. 10 (104), paper no. 07. Available at: http://www.viam-works.ru (accessed: July 07, 2022). DOI: 10.18577/2307-6046-2021-0-10-67-78.
- Shchegoleva N.E., Chainikova A.S., Orlova L.A. Sintering process analysis in the manufacture of strontiumalumi-nosilicate glass ceramics by power-pressed method. Aviacionnye materialy i tehnologii, 2018, no. 4 (53), pp. 55–62. DOI: 10.18577/2071-9140-2018-0-4-55-62.
- Lavrov A.V., Yakovlev N.O., Erasov V.S. Destruction of ceramic materials under the influence of high-speed indenter. Aviacionnye materialy i tehnologii, 2018, no. 2 (51), pp. 88–94. DOI: 10.18577/2071-9140-2018-0-2-88-94.
- Dyatlova E.M., Minenkova G.Ya., Kolontaeva T.V. Intensification of sintering of mullite-cordierite ceramics using mineralizers. Glass and Ceramics, 2000, no. 12, p. 21.
- Osawa C.C., Bertran C.A. Mullite Formation from Mixtures of Alumina and Silica Sols: Mechanism and pH Effect. Journal of the Brazilian Chemical Society, 2005, vol. 16, no. 2, pp. 251–258.
- Sedmale G., Grace L., Zalite I. et al. Microstructure and properties of mullite–ZrO2(Y2O3)–Si3N4 ceramics sintered by various methods. Novye ogneupory, 2018, no. 7, pp. 49–54.
- Orgaz F. Densification and crystalization kinetics of mullite diphasic gels from non-isothermal dilatometry experiments. Boletin de la Sociedad Espanola de Ceramica y Vidrio, 2008, vol. 47, no. 6, pp. 358–365.
- Chen Yi, Lu Z., Wan W. et al. Effect of Urchin-Like Mullite Whiskers on the High-Temperature Performance of Porous SiO2-Based Ceramic Molds. Materials, 2019, no. 12, art. 1181. DOI: 10.3390/ma12071181.
- Barrientos-Hernґandez F.R., Pґerez-Labra M., Lobo-Guerrero A. et al. Effect of Particle Size and Sintering Temperature on the Formation of Mullite from Kyanite and Aluminum Mixtures. Advances in Materials Science and Engineering, 2021, vol. 2021, art. 6678297. DOI: 10.1155/2021/6678297.
- Pletnev P.M., Tyulkin D.S. Physical and chemical principles of obtaining refractories for the production of technical ceramics. Bulletin of the Siberian State University of Communications, 2016, no. 1, pp. 21–26.
- Lian J., Zhu B., Li X., Chen P. In-situ Synthesis of Column-like Mullite and SiC Whiskers and its Effect on Al2O3–SiC–C Refractory Properties. Journal of the Chinesse Ceramic Society, 2016, vol. 44, no. 9. Available at: http://www.gxyb.cbpt.cnki.net (accessed: July 01, 2022). DOI: 10.14062/j.issn.0454-5648.2016.09.21.
- Method for obtaining a powder of a ceramic composite material: pat. 2292320 Rus. Federation; filed 15.08.05; publ. 27.01.07.
- Varrik N.M., Maksimov V.G. Synthesis of the initial powder for obtaining mullite ceramics modified with zirconium dioxide. Ogneupory i tekhnicheskaya keramika, 2021, no. 5–6, р. 3.
- Method for producing a ceramic product: pat. 2486159 Rus. Federation; filed 22.06.11; publ. 27.06.13.
- Babashov V.G., Maksimov V.G., Varrik N.M. On the question of mullite crystallization in a ceramic composite material. Steklo i keramika, 2021, no. 12, pp. 9–14.
- Gulyaev A.P., Gulyaev A.A. Metallurgy: textbook for universities. Ed. 7th, rev. and add. Moscow: Alliance, 2011, 644 p.