Application of fiberglass brand VPS-53K, processed atmospheric pressure plasma, in the manufacture of aircraft products

Barannikov A.A., Sudyin Yu.I., Veshkin E.A, Satdinov R.A.
Barannikov A.A., Sudyin Yu.I., Veshkin E.A, Satdinov R.A. Application of fiberglass brand VPS-53K, processed atmospheric pressure plasma, in the manufacture of aircraft products // Proceedings of VIAM. 2022. No. 9. DOI: 10.18577/2307-6046-2022-0-9-83-98. URL: https://viam-works.ru/en/journal/2022/9/7
Keywords
helicopter technology, helicopter main and tail rotor blade, surface preparation method, atmospheric pressure plasma, fiberglass, wetting angle, surface free energy, adhesion work, adhesive bond strength
Abstract

The article is devoted to the testing of fiberglass grade VPS-53K treated with atmospheric pressure plasma in the production environment of the manufacturer of the main and tail rotor blades of a helicopter. It has been established that atmospheric pressure plasma increases the wettability of the fiberglass surface and the strength of the adhesive joint of «the spar‒sheathing» (fiberglass grade VPS-53K). The guaranteed time interval between the processing of fiberglass with atmospheric pressure plasma and the gluing process is no more than 6 mon.

Reference list
  1. Kablov E.N. Formation of domestic space materials science. Vestnik RFBR, 2017, no. 3, pp. 97–105.
  2. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  3. Kablov E.N. Materials of a new generation and digital technologies for their processing. Vestnik Rossiyskoy akademii nauk, 2020, vol. 90, no. 4, pp. 331–334.
  4. Kablov E.N. VIAM: new generation materials for PD-14. Krylya Rodiny, 2019, no. 7–8, pp. 54–58.
  5. Mukhametov R.R., Petrova A.P. Thermosetting binders for polymer composites (review). Aviacionnye materialy i tehnologii, 2019, no. 3 (56), pp. 48–58. DOI: 10.18577/2071-9140-2019-0-3-48-58.
  6. Basharov E.A., Vagin A.Yu. Analysis of the use of composite materials in the design of helicopter airframes. Trudy MAI, 2017, no. 92, pp. 1–33.
  7. Doroshenko N.I., Chursova L.V. Evolution of materials for blades of helicopters. Aviacionnye materialy i tehnologii, 2012, no. 2, pp. 16–18.
  8. Doroshenko N.I. Application of PCM in the design of helicopter propeller blades. Polymer composite materials for the aerospace industry: materials of All-Rus. sci.-tech. conf. (Moscow, December 6, 2019). Moscow: VIAM, 2019, 208 p.
  9. Davydova I.F., Kablov E.N., Kavun N.S. Heat-resistant non-combustible polyimide fiberglass for products of aviation and rocket technology. Vse materialy. Entsiklopedicheskiy spravochnik, 2009, no. 7, pp. 2–11.
  10. Popov Y.O., Kolokolceva T.V., Gusev Y.A., Gromova A.A. Development of the constructive and technological solution for a sheet fibreglass for tail section skins of helicopter rotor blades. Trudy VIAM, 2016, no. 1 (37), paper no. 05. Available at: http://www.viam-works.ru (accessed: December 12, 2021). DOI: 10.18577/2307-6046-2016-0-1-42-49.
  11. Popov Yu.O., Kolokoltseva T.V., Khrulkov A.V. The new generation of materials and technologies for helicopter blade spars. Aviacionnye materialy i tehnologii, 2014, no. S2, pp. 5–9. DOI: 10.18577/2071-9140-2014-0-S2-5-9.
  12. Barannikov A.A., Рostnov V.I., Veshkin E.A., Starostina I.V. Link between the energy characteristics of the surface of fiberglass of the VPS-53К brand and the strength of the adhesive joint based on it. Trudy VIAM, 2020, no. 10 (92), paper no. 05. Available at: http://www.viam-works.ru (accessed: December 12, 2021). DOI: 10.18577/2307-6046-2020-0-10-40-50.
  13. Barannikov A.A., Postnova M.V., Krasheninni-kova E.V., Vasyukov A.N. Application of new technologies in the production of helicopter main rotor blades. Trudy VIAM, 2021, no. 11 (105), paper no. 09. Available at: http://www.viam-works.ru (accessed: December 9, 2021). DOI: 10.18577/2307-6046-2021-0-11-91-102.
  14. Barannikov A.A., Sudyin Yu.I., Veshkin E.A., Satdinov R.A. Determination of the permissible storage time of polymeric composite materials after surface treatment with atmospheric pressure plasma before bonding. Trudy VIAM, 2022, no. 5 (111), paper no. 07. Available at: http://www.viam-works.ru (accessed: June 1, 2022). DOI: 10.18577/2307-6046-2022-0-5-26-40.
  15. Barannikov A.A., Postnov V.I., Veshkin E.A., Strelnikov S.V. The role of fiberglass surface preparation for gluing. Klei. Germetiki. Tekhnologii, 2019, no. 6, pp. 19–27. DOI: 10.31044/1813-7008-2019-0-6-19-27.
  16. Barannikov A.A., Postnov V.I., Veshkin E.A., Satdinov R.A. The use of atmospheric pressure plasma as a method of preparing the surface of polymer composite materials for gluing. Polymer composite materials and production technologies of a new generation: materials of V All-Rus. sci.-tech. conf. (Moscow, November 19, 2021). Moscow: NRC "Kurchatov Institute" – VIAM, 2021, 259 p.
  17. Operating manual OCA 15EC: Version 1.0; English; Valid as of firmware version 10.27, and SCA software version 4.4.1 Build 1046. Data Physics Instruments GmbH. Available at: https://vdocuments.site/manual-sca20-u.html (accessed: April 15, 2022).
  18. Thomsen F. Practical Contact Angle Measurement (5). Custom – made models: from contact angle to surface free energy. KRUSS Technical Note TN315e, pp. 1–6. Available at: https://warwick.ac.uk/fac/cross_fac/sciencecity/programmes/internal/themes/am2/booking/dropshapeanalyser/practical_contact_angle_measurement_5.pdf (accessed: April 15, 2022).
  19. Langer M., Otto D. Methods for studying the surface characteristics of polymers after plasma treatment. Comparative analysis. Analiz i kontrol: tekhnologii, pribory, resheniya, 2018, no. 2 (39), pp. 2–7.
  20. Bogdanova Yu.G. Adhesion and its role in ensuring the strength of polymer composites: textbook for students according to special "Composite nanomaterials". Moscow: Lomonosov Moscow State University, 2010, 68 p.
  21. Vilnave Zh.Zh. Adhesive connections. Moscow: Technosfera, 2007, 384 p.
  22. Cagle Ch. Adhesive connections. Ed. D.A. Kardashov. Moscow: Mir, 1971, 295 p.
  23. MIL-HDBK-17-3F: Composite materials handbook. Volume 3 of 5. Polymer matrix composites materials usage, design, and analysis. CMH-17 Secretariat, Materials Sciences Corporation. Horsham, 2002, 734 с.
  24. Peters S.T. Handbook of Composites. Second Edition. New York: Chapman & Hall, 1998, 1120 с.
  25. Tracey A.C. Effect of Atmospheric Pressure Plasma Treatment on Surface Characteristics and Adhesive Bond Quality of Peel Ply Prepared Composites. Available at: https://digital.lib.washington.edu/researchworks/handle/1773/27522 (accessed: November 12, 2020).
  26. Takeda T., Yasuoka T., Hoshi H. et al. Effectiveness of flame-based surface treatment for adhesive bonding of carbon fiber reinforced epoxy matrix composites. Composites. Part A: Applied Science and Manufacturing, 2019, vol. 119, pp. 30–37.
  27. Zaldivar R.J., Nokes J., Steckel G.L. et al. The Effect of Atmospheric Plasma Treatment on the Chemistry, Morphology and Resultant Bonding Behavior of a Pan-Based Carbon Fiber-Reinforced Epoxy Composite. Journal of Composite Materials, 2009, vol. 44, is. 2, pp. 137–156. DOI: 10.1177/0021998309345343.
  28. Dighton C., Rezai A., Ogin S.L., Watts J.F. Atmospheric plasma treatment of CFRP composites to enhance structural bonding investigated using surface analytical techniques. International Journal of Adhesion and Adhesives, 2019, vol. 91, p. 142–149. DOI: 10.1016/j.ijadhadh.2019.03.010.
  29. Zaldivar R.J., Steckel G.L, Morgan B.A. et al. Bonding Optimization on Composite Surfaces using Atmospheric Plasma Treatment. Journal of Adhesion Science and Technology, 2012, vol. 26, is. 1–3, pp. 381–401.
  30. Hansen W. Plasma for Aviation and Aerospace Industries. Available at: https://www.plasmatreat.com/downloads/english/15-04_IST_aerospace.pdf (accessed: July 12, 2021).
  31. Williams T., Yu H., Hicks R. Atmospheric pressure plasma activation of polymers and composites for adhesive bonding: A Critical Review. Reviews of Adhesion and Adhesives, 2013, vol. 1, no. 1, pp. 46–87. DOI: 10.7569/RAA.2013.097302.
  32. Serrano J.S. Surface modifications of composite materials by atmospheric pressure plasma treatment: PhD-Thesis. Madrid: Universidad Rey Juan Carlos, 2011, 302 p. Available at: https://eciencia.urjc.es/bitstream/10115/11379/1/Thesis_June%202011%20JSS-SLU-AUF_v5.pdf (accessed: December 12, 2021).
  33. Gleich H. Zusammenhang zwischen Oberflächenenergie und Adhäsionsvermögen von Polymer werkstoffen am Beispiel von PP und PBT und deren Beeinflussung durch die Niederdruck-Plasmatechnologie: dis. Universtät Duisburg-Essen, 2004, 103 p. Available at: https://duepublico2.unidue.de/servlets/MCRFileNodeServlet/duepublico_derivate_00005593/gleichdiss.pdf (accessed: December 12, 2021).
  34. Rodríguez B.N. Pre-Treatment for adhesive bonding of aerospace composite components: PhM-Thesis. London: Brunel University, 2016, 133 p. Available at: https://bura.brunel.ac.uk/bitstream/2438/14669/1/FulltextThesis.pdf (accessed: December 12, 2021).
  35. Al-Maliki H.L.R. Adhesive and tribological behaviour of cold atmospheric plasma-treated polymer surfaces: PhD Dissertation. Gödöllő: Szent István University, 2018, 115 p. Available at: https://szie.hu/sites/default/files/hayder_lateef_dissertation.pdf (accessed: December 12, 2021).
  36. Lisco F., Shaw A., Wright A. et al. Atmospheric-pressure plasma surface activation for solution processed photovoltaic devices. Solar Energy, 2017, vol. 146, pp. 287–297.
  37. Kostova K.G., Nishimea T.M.C., Castroa A.H.R. et al. Surface modification of polymeric materials by cold atmospheric plasma jet. Applied Surface Science, 2014, vol. 314, pp. 367–375.
  38. Akiyama H., Hasegawa K., Sekigawa T., Yamazaki N. Atmospheric pressure plasma treatment for composites bonding. Mitsubishi Heavy Industries Technical Review, 2018, vol. 55, no. 2, pp. 1–5.
  39. Lucchetta G. Experimental analysis of atmospheric plasma treatment and resin optimization for adhesive bonding of carbon fiber/epoxy composites. Available at:http://tesi.cab.unipd.it/48832/1/Tesi_ANTONELLO_Julien.pdf (accessed: December 12, 2021).