Photocurable acrylate compositions (review)

Sarychev I.A. S, Butuzov A.V., Serkova E.A., Dolgova E.V.
Sarychev I.A. S, Butuzov A.V., Serkova E.A., Dolgova E.V. Photocurable acrylate compositions (review) // Proceedings of VIAM. 2022. No. 9. DOI: 10.18577/2307-6046-2022-0-9-68-82. URL: https://viam-works.ru/en/journal/2022/9/6
Keywords
composition, acrylate, monomer, oligomer, active diluent, photopolymerization, shrinkage, 3D printing
Abstract

A review of photocurable acrylate compositions, which can be used for a wide range of tasks, including 3D printing, has been carried out. The main (meth)acrylate monomers, oligomers and diluents, comonomers and special additives are considered. The influence of the structure of monomers and active diluents on the properties of the polymer is described. The mechanisms of photoinitiation and the mechanisms of chain transfer agents are presented. The influence of the introduction of epoxy resins into the composition of photocurable acrylate compositions is indicated. The conclusion is made about the possibilities of wide modification of such compositions.

Reference list
  1. Vnuk V.V., Kamayev S.V., Markov M.A., Cherebylo S.A. Features of parts fabrication by using multicomponent resins by laser stereolithography. Aviacionnye materialy i tehnologii, 2018, no. 4 (53), pp. 31–36. DOI: 10.18577/2071-9140-2018-0-4-31-36.
  2. UV Curable Resins&Formulated Products Market Size | Share | Forecast. Available at: https://www.verifiedmarketresearch.com/product/uv-curable-resins-formulated-products-market (accessed: June 07, 2022).
  3. Kablov E.N. Additive technologies – the dominant of the national technological initiative. Intellekt i tekhnologii, 2015, no. 2 (11), pp. 52–55.
  4. Kablov E.N. Present and future of additive technologies. Metally Evrazii, 2017, no. 1, pp. 2–6.
  5. Bednarczyk P., Irska I., Gziut K., Ossowicz-Rupniewska P. Novel Multifunctional Epoxy (Meth)Acrylate Resins and Coatings Preparation via Cationic and Free-Radical Photopolymerization. Polymers, 2021, no. 13, pp. 1718. DOI: 10.3390/polym13111718.
  6. Manmeet K., Srivastava A.K. Photopolymerization: A review. Journal of Macromolecular Science. Part C, 2002, no. 42 (4), pp. 481–512. DOI: 10.1081/MC-120015988.
  7. Mukhametov R.R., Petrova A.P. Thermosetting binders for polymer composites (review). Aviacionnye materialy i tehnologii, 2019, no. 3 (56), pp. 48–58. DOI: 10.18577/2071-9140-2019-0-3-48-58.
  8. Chatani S., Kloxin C.J., Bowman C.N. The power of light in polymer science: Photochemical processes to manipulate polymer formation, structure, and properties. Polymer Chemistry, 2014, no. 5, pp. 2187–2201. DOI: 10.1039/C3PY01334K.
  9. Corrigan N., Yeow J., Judzewitsch P., Xu J., Boyer C. Seeing the light: Advancing materials chemistry through photopolymerization. Angewandte Chemie International Edition, 2019, no. 58, pp. 5170–5189. DOI: 10.1002/anie.201805473.
  10. Photopolymer composition for 3D printing: pat. 9902860 US; filed 30.08.16; publ. 01.03.18.
  11. Photocurable resin composition for Stereolithography 3D printing: pat. 101980037 KR; filed 14.03.17; publ. 29.08.19.
  12. Photocurable material composition and cured product thereof: pat. 20200157258 US; filed 09.08.13; publ. 10.02.14.
  13. Sandmeier M., Paunović N., Conti R. et al. Solvent-Free Three-Dimensional Printing of Biodegradable Elastomers Using Liquid Macrophotoinitiators. Macromolecules, 2021, no. 54 (17), pp. 7830–7839. DOI: 10.1021/acs.macromol.1c00856.
  14. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  15. Zarek M., Layani M., Cooperstein I. et al. 3D Printing of Shape Memory Polymers for Flexible Electronic Devices. Advance Materials, 2016, no. 28, pp. 4449−4454. DOI: 10.1002/adma.201503132.
  16. Palaganas J., de Leon A.C., Mangadlao J. et al. Facile Preparation of Photocurable Siloxane Composite for 3D Printing. Macromolecular Materials and Engineering, 2017, no. 302 (5), pp. 1–9. DOI: 10.1002/mame.201600477.
  17. Patel D.K., Sakhaei A.H., Layani M. et al. Highly Stretchable and UV Curable Elastomers for Digital Light Processing Based 3D Printing. Advance Materials, 2017, no. 29, pp. 1–7. DOI: 10.1002/adma.201606000.
  18. Stassi S., Fantino E., Calmo R. et al. Polymeric 3D Printed Functional Microcantilevers for Biosensing Applications. ACS Applied Materials & Interfaces, 2017, no. 9 (22), pp. 19193−19201. DOI: 10.1021/acsami.7b04030.
  19. Gou M., Qu X., Zhu W. et al. Bio-Inspired Detoxification Using 3D-Printed Hydrogel Nanocomposites. Nature Communications, 2014, no. 5, pp. 3774. DOI: 10.1038/ncomms4774.
  20. Kablov E.N., Yakovlev N.O., Kharitonov G.M., Mekalina I.V. Features of the relaxation behavior of polymer glasses based on polymethyl methacrylate and their consideration in the strength calculation of aviation glazing. Vse materialy. Entsiklopedicheskiy spravochnik, 2016, no. 9, pp. 2–9.
  21. Chiappone A., Fantino E., Roppolo I. et al. 3D Printed PEG-Based Hybrid Nanocomposites Obtained by Sol–Gel Technique. ACS Applied Materials & Interfaces, 2016, no. 8, pp. 5627–5633. DOI: 10.1021/acsami.5b12578.
  22. Warner J., Soman P., Zhu W. et al. Design and 3D Printing of Hydrogel Scaffolds with Fractal Geometries. ACS Biomaterials Science & Engineering, 2016, no. 2, pp. 1763–1770. DOI: 10.1021/acsbiomaterials.6b00140.
  23. Liska R., Schuster M., Inführ R. et al. Photopolymers for Rapid Prototyping. Journal of Coatings Technology and Research, 2007, no. 4, pp. 505–510. DOI: 10.1007/s11998-007-9059-3.
  24. Yue J., Zhao P., Gerasimov J.Y. et al. 3D-Printable Antimicrobial Composite Resins. Advanced Functional Materials, 2015, no. 25, pp. 6756–6767. DOI: 10.1002/adfm.201502384.
  25. Al Mousawi A., Dumur F., Garra P. et al. Carbazole Scaffold Based Photoinitiator/Photoredox Catalysts: Toward New High-Performance Photoinitiating Systems and Application in LED Projector 3D Printing Resins. Macromolecules, 2017, no. 50, pp. 2747–2758. DOI: 10.1021/acs.macromol.7b00210.
  26. Al Mousawi A., Garra P., Schmitt M. et al. 3-Hydroxyflavone and N-Phenylglycine in High Performance Photoinitiating Systems for 3D Printing and Photocomposites Synthesis. Macromolecules, 2018, no. 51, pp. 4633–4641. DOI: 10.1021/acs.macromol.8b00979.
  27. Credi C., Fiorese A., Tironi M. et al. 3D Printing of Cantilever-Type Microstructures by Stereolithography of Ferromagnetic Photopolymers. ACS Applied Materials & Interfaces, 2016, no. 8, pp. 26332–26342. DOI: 10.1021/acsami.6b08880.
  28. (Meth)Acrylates Containing Urethane Groups: pat. 5658712 US; filed 09.08.93; publ. 19.08.97.
  29. Boddapati A., Rahane S.B., Slopek R.P. et al. Gel Time Prediction of Multifunctional Acrylates Using a Kinetics Model. Polymer, 2011, no. 52, pp. 866–873. DOI: 10.1016/j.polymer.2010.12.024.
  30. Ligon-Auer S.C., Schwentenwein M., Gorsche C. et al. Toughening of Photo-Curable Polymer Networks: A Review. Polymer Chemistry, 2016, no. 7, pp. 257–286. DOI: 10.1039/C5PY01631B.
  31. Kim L.U., Kim J.W., Kim C.K. Effects of Molecular Structure of the Resins on the Volumetric Shrinkage and the Mechanical Strength of Dental Restorative Composites. Biomacromolecules, 2006, no. 7, pp. 2680–2687. DOI: 10.1021/bm060453h.
  32. Moraes R.R., Garcia J.W., Barros M.D. et al. Control of Polymerization Shrinkage and Stress in Nanogel-Modified Monomer and Composite Materials. Dental Materials, 2011, no. 27, pp. 509–519. DOI: 10.1016/j.dental.2011.01.006.
  33. Liquid, Radiation-Curable Composition, Especially for Stereolithography: pat. 5972563 US; filed 29.07.96; publ. 26.10.99.
  34. Kablov E.N., Laptev A.B., Prokopenko A.N., Gulyaev A.I. Relaxation of polymeric composite materials under the prolonged action of static load and climate (review). Part 1. Binders. Aviation materials and technologies, 2021, no. 4 (65), paper no. 08. Available at: http://www.journal.viam.ru (accessed: July 6, 2022). DOI: 10.18577/2071-9140-2021-0-4-70-80.
  35. Stereolithography Resin Compositions and Three-Dimensional Objects Made Therefrom: pat. 8980971 US; filed 21.05.13; publ. 28.11.13.
  36. Photosensitive Compositions: pat. 5476748 US; filed 14.12.93; publ. 19.12.95.
  37. Method of Forming a Three-Dimensional Object by Stereolithography and Composition Therefore: pat. 4942001 US; filed 31.10.89; publ. 17.07.90.
  38. Zhang Y., Li Y., Thakur V.K. et al. Bio-based reactive diluents as sustainable replacements for styrene in MAESO resin. RSC Advances, 2018, no. 8, pp. 13780. DOI: 10.1039/c8ra00339d.
  39. Decker C., Viet T.T., Decker D., Weber-Koehl E. UV-radiation curing of acrylate/epoxide systems. Polymer, 2001, no. 42, pp. 5531–5541. DOI: 10.1016/S0032-3861(01)00065-9.
  40. Cai Y., Jessop J.L.P. Decreased Oxygen Inhibition in Photopolymerized Acrylate/Epoxide Hybrid Polymer Coatings as Demonstrated by Raman Spectroscopy. Polymer, 2006, no. 47, pp. 6560–6566. DOI: 10.1016/j.polymer.2006.07.031.
  41. Lalevée J., Tehfe M.A., Dumur F. et al. Light-Harvesting Organic Photoinitiators of Polymerization. Macromolecular Rapid Communications, 2013, no. 34, pp. 239–245. DOI: 10.1002/marc.201200578.
  42. Wiersma D. The Smallest Random Laser. Nature, 2000, no. 406, pp. 133–135. DOI: 10.1038/35018184.
  43. Green W.A. Industrial Photoinitiators: A Technical Guide. CRC Press: Boca Raton, 2010, 302 р.
  44. Rapid Prototyping Resin Compositions: pat. 8293810 US; filed 29.08.05; publ. 23.10.12.
  45. Photopolymerizable Compositions Containing an Alkylbisacylphosphine Oxide: pat. 5472992 US; filed 28.04.94; publ. 05.12.95.
  46. Fodran E., Koch M., Menon U. Mechanical and Dimensional Characteristics of Fused Deposition Modeling Build Styles. SFF Symposium Proceedings, 1996, pp. 419–442.
  47. Wayner D.D.M., Clark K.B., Rauk A., Yu D., Armstrong D.A. C‒H Bond Dissociation Energies of Alkyl Amines: Radical Structures and Stabilization Energies. Journal of the American Chemical Society, 1997, no. 119, pp. 8925–8932. DOI: 10.1021/ja971365v.
  48. Crivello J.V. The Discovery and Development of Onium Salt Cationic Photoinitiators. Journal of Polymer Science. Part A: Polymer Chemistry, 1999, no. 37, pp. 4241–4254. DOI: 10.1002/(SICI)1099-0518(19991201)37:234241::AID-POLA1>3.0.CO;2-R.
  49. Fouassier J.-P., Lalevée J. Photoinitiators for Polymer Synthesis: Scope, Reactivity, and Efficiency. Weinheim: Wiley-VCH Verlag & Co. KGaA, 2012, 490 p.
  50. Crivello J.V., Lam J.H.W. Photoinitiated Cationic Polymerization with Triarylsulfonium Salts. Journal of Polymer Science: Polymer Chemistry Edition, 1996, no. 34, pp. 32331–3253. DOI: 10.1002/pola.1996.873.
  51. Zastrogina O.B., Serkova E.А., Sarychev I.A., Vavilova M.I. Influence of Russian and Chinese vinyflex on the properties of the VFT binder and fiberglass based on it. Aviacionnye materialyi tehnologii, 2020, no. 3 (60), pp. 3–9. DOI: 10.18577/2071-9140-2020-0-3-3-9.
  52. Curable Composition: pat. 8362148 US; filed 12.03.08; publ. 29.01.13.
  53. Peer G., Eibel A., Gorsche C. et al. Ester-Activated Vinyl Ethers as Chain Transfer Agents in Radical Photopolymerization of Methacrylates. Macromolecules, 2019, no. 52 (7), pp. 2691–2700.
  54. Gorsche C., Koch T., Moszner N., Liska R. Exploring the Benefits of β-Allyl Sulfones for More Homogeneous Dimethacrylate Photopolymer Networks. Polymer Chemistry, 2015, no. 6, pp. 2038−2047. DOI: 10.1039/C4PY01582G.
  55. Gauss P., Ligon-Auer S.C., Griesser M. et al. The Influence of Vinyl Activating Groups on β-Allyl Sulfone-Based Chain Transfer Agents for Tough Methacrylate Networks. Journal of Polymer Science. Part A: Polymer Chemistry, 2016, no. 54, pp. 1417–1427. DOI: 10.1002/pola.27993.
  56. Gorsche C., Seidler K., Knaack P. et al. Rapid Formation of Regulated Methacrylate Networks Yielding Tough Materials for Lithography-Based 3D Printing. Polymer Chemistry, 2016, no. 7, pp. 2009–2014. DOI: 10.1039/C5PY02009C.
  57. Yagci Y., Jockusch S., Turro N.J. Photoinitiated Polymerization: Advances, Challenges, and Opportunities. Macromolecules, 2010, no. 43, pp. 6245–6260. DOI: 10.1021/ma1007545.
  58. Photosensitive Compositions Useful in Three-Dimensional Part-Building and Having Improved Photospeed: pat. 5418112 US; filed 10.11.93; publ. 23.05.95.