Study of the influence of different graphene contents on the properties of a ceramic composite material
UDC
661.183.4-911.48
DOI
10.18577/2307-6046-2022-0-8-88-97
Article PDF (Russian)
(954.24 KB)
How to cite
Lebedeva Yu.E., Shchegoleva N.E., Gulyaev A.I., Turchenko M.V. Study of the influence of different graphene contents on the properties of a ceramic composite material // Proceedings of VIAM. 2022. No. 8. DOI: 10.18577/2307-6046-2022-0-8-88-97. URL: https://viam-works.ru/en/journal/2022/8/7
Keywords
hot pressing, ceramic composite, graphene, zirconium boride, silicon carbide, consolidation
Abstract
The effect of graphene content on the physical and mechanical properties and oxidative resistance of samples of ceramic composite material (CCM) obtained by hot pressing has been studied. The introduction of graphene in an amount of 1–2 vol. % led to an increase in the microhardness of CMC from 24,8 to 26,5 GPa, a decrease in open porosity from 0,8 to 0,2 %, and an increase in oxidation resistance at a temperature of 1500 °C by 63 %. . The structure of graphene with a hexagonal crystal lattice was studied by scanning and transmission electron microscopy: graphene has a scaly fragmentation structure with agglomerate sizes from 1 to 8 μm.
Reference list
- Yumin A., Xianghong X., Kaixuan G. Effect of SiC whiskers and graphene nanosheets on the mechanical Properties of ZrB2–SiCw-Graphene ceramic composites. Ceramic international, 2016, vol. 42, is. 12, pp. 14066–14070.
- Nguyen V.-H., Delbari S.A., Shahedi Asl M. et al. Mohammadreza Shokouhimehr Combined role of SiC whiskers and graphene nano-platelets on the microstructure of spark plasma sintered ZrB2 ceramics. Ceramics International, 2021, vol. 47, pp. 12459–12466.
- Cheng Y., Hu P., Zhou Sh. et al. Using macroporous graphene networks to toughen ZrC–SiC ceramic. Journal of the European Ceramic Society, 2018, vol. 38, is. 11, pp. 3752–3758.
- Balak Z., Azizieh M., Kafashan H. Optimization of effective parameters on thermal shock resistance of ZrB2–SiC-based composites prepared by SPS: using Taguchi design. Materials Chemistry and Physics, 2017, vol. 196, pp. 333–3340.
- Vafa N.P., Nayebi B., Shahedi Asl M. Reactive hot pressing of ZrB2-based composites with changes in ZrO2/SiC ratio and sintering conditions. Part II: mechanical behavior. Ceramics International, 2016, vol. 42, no. 2, pp. 2724–2733.
- Kablov E.N., Grashchenkov D.V., Isaeva N.V., Solntsev S.S., Sevastyanov V.G. High-temperature structural composite materials based on glass and ceramics for promising aircraft products. Steklo i keramika, 2012, no. 4, pp. 7–11.
- Shahedi Asl M., Farahbakhsh I., Nayebi B. Characteristics of multi–walled carbon nanotube toughened ZrB2–SiC ceramic composite prepared by hot pressing. Ceramics International, 2016, vol. 42, is. 1, pp. 1950–1958.
- Sevastyanov V.G., Simonenko E.P., Simonenko N.P., Grashchenkov D.V., Solntsev S.St., Ermakova G.V., Prokopchenko G.M., Kablov E.N., Kuznetsov N.T. Obtaining filamentous silicon carbide crystals using the method of the method in the volume of sic-curamika. Kompozity i nanostruktury, 2014, vol. 6, no. 4, pp. 198–211.
- Kuznetsov B.Yu., Sorokin O.Yu., Vaganova M.L., Osin I.V. Synthesis of model high-temperature ceramic matrices by the method of spark plasma sintering and the study of their properties for
- the production of composite materials. Aviacionnye materialy i tehnologii, 2018, no. 4 (53), pp. 37–44. DOI: 10.18577/2071-9140-2018-0-4-37-44.
- Belyachenkov I.O., Schegoleva N.E., Chainikova A.S., Vaganova M.L., Shavnev A.A. The influ-ence of sintering and modifying additives on the sintering process and the properties of silicon nitride ceramics. Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 70–78. DOI: 10.18577/2071-9140-2020-0-1-70-78.
- Babashov V.G., Varrik N.M., Maksimov V.G., Samorodova O.N. Oxide fiber coated with silicon carbide for producing composite materials. Aviation materials and technologies, 2021, no. 3 (64), paper no. 09. Available at: http://www.journal.viam.ru (accessed: April 07, 2022). DOI: 10.18577/2713-0193-2021-0-3-94-104.
- Zhitnyuk S.V. Oxygen-free ceramic materials for the space technics (review). Trudy VIAM, 2018, no. 8 (68), paper no. 8. Available at: http://www.viam-works.ru (accessed: April 07, 2022). DOI: 10.18577/2307-6046-2018-0-8-81-88.
- Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Wang X., Zhao J., Cui E. et al. Nano/microstructures and mechanical properties of Al2O3–WC–TiC ceramic composites incorporating graphene with different sizes. Materials Science & Engineering A, 2021, vol. 812, art. 141132.
- Ahmad I., Islam M., Habis N.A., Parves S. Hot-pressed graphene nanoplatelets or/and zirconia reinforced hybrid alumina nanocomposites with improved toughness and mechanical characteristics. Journal Materials Science and Technology, 2020, vol. 40, pp. 135–145.
- Feng Y.H., Fang J.H., Wu J. et al. Mechanical and tribological properties of plasma sprayed graphene nanosheets/Al2O3 + 13 % TiO2 composite coating. Tribology International, 2020, no. 146, аrt. 106233.
- Li Z.L., Zhao J., Sun J.L. Reinforcement of Al2O3/TiC ceramic tool material by multi-layer grapheme. Ceramic International, 2017, vol. 43, pp. 11421–11427.
- Wang X.C., Zhao J., Cui E.Z. Microstructure, mechanical properties and toughening mechanisms of graphene reinforced Al2O3–WC–TiC composite ceramic tool material. Ceramic International, 2019, vol. 45, pp. 10321–10329.
- Liu Y.Z., Jiang X.S., Shi J.L. Research on the interface properties and strengthening-toughening mechanism of nanocarbon-toughened ceramic matrix composites. Nanotechnology Revews, 2020, vol. 9, pp. 190–208.
- Sun J.L., Zhao J., Huang Z.F. Preparation and properties of multilayer graphene reinforced binderless TiC nanocomposite cemented carbide through twostep sintering. Materials & Design, 2020, no. 188, art. 108495.
- Rezaie A., Fahrenholtz W.G., Hilmas G.E. The effect of a graphite addition on oxidation of ZrB2–SiC in air at 1500 °C. Journal of European Ceramic Society, 2013, vol. 33, pp. 413–421.