The article presents the results of a study of the surface quality of cladding sheets made of alloys of the D16ch type. Methods of metallographic and fractographic analyzes have shown that the appearance of bubbles in the investigated sheets is caused by the presence of internal interfaces (in the form of pores in the base of sheets and cladding), as well as defective areas of poor-quality welding of the cladding and production and heat treatment of sheets, diffuses hydrogen dissolved in the metal or formed on the surface of the sheets during the reaction of aluminum with water vapor. A tendency towards a decrease in the relative elongation in sheets with surface bubbles compared to sheets without defects was revealed.

Reference list
  1. Kablov E.N. The main directions of development of materials for aerospace technology of the
  2. XXI century. Perspektivnye materialy, 2000, no. 3, pp. 27–36.
  3. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  4. Antipov V.V. Prospects for development of aluminium, magnesium and titanium alloys for aerospace engineering. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 186–194. DOI: 10.18577/2107-9140-2017-0-S-186-194.
  5. Kablov E.N. Formation of domestic space materials science. Vestnik RFFI, 2017, no. 3, pp. 97–105.
  6. Fridlyander I.N. Aluminum alloys in aircraft in the periods 1970–2000 and 2001–2015. Tekhnologiya legkikh splavov, 2002, no. 4, pp. 1212–1217.
  7. Duyunova V.A., Nechaikina T.A., Oglodkov M.S., Yakovlev A.L., Leonov A.A. Perspective developments in the field of light materials for modern aerospace technology. Tekhnologiya legkikh splavov, 2018, no. 4, pp. 28–43.
  8. Selivanov A.A., Tkachenko E.A., Popova O.I., Babanov V.V. High-strength wrought aluminum weldable V-1963 alloy for details of primary structure of modern aviation engineering. Trudy VIAM, 2017, no. 2 (50), paper no. 01. Available at: http://www.viam-works.ru (accessed: December 29, 2021). DOI: 10.18577/2307-6046-2017-0-2-1-1.
  9. Kishkina S.I. Fracture resistance of aluminum alloys. Moscow: Metallurgiya, 1981, 280 p.
  10. Atlas of structures of ingots and semi-finished products from aluminum alloys. Ed. V.I. Dobatkin, V.I. Elagin, L.M. Khitrov. Moscow: Metallurgiya, 1971, 152 p.
  11. Aluminum alloys. Structure and properties of semi-finished products from aluminum alloys.
  12. Ed. V.I. Elagin, V.A. Livanov. 2nd ed., rev. and add. Moscow: Metallurgiya, 1984, 408 p.
  13. Dobatkin V.I., Gabidullin R.M., Kolachev B.A., Makarov G.S. Gases and oxides in wrought aluminum alloys. Moscow: Metallurgiya, 1976, 264 p.
  14. Davydov D.M., Titov V.I., Letov A.F., Lutsenko A.N. Comparative evaluation of methods for determining the content of hydrogen in metal materials. Trudy VIAM, 2019, no. 11 (83), paper no. 09. Available at: http://www.viam-works.ru (accessed: December 29, 2021). DOI: 10.18577/2307-6046-2019-0-11-75-84.
  15. Tsukrov S.L. Development of technology for hardening semi-finished products from aluminum alloys. Perspektivnyye tekhnologii legkikh i spetsialnykh splavov. Moscow: Fizmatlit, 2006, pp. 323–338.
  16. Kolobnev N.I., Ber L.B., Tsukrov S.L. Thermal treatment of deformable aluminum alloys.
  17. Ed. E.N. Kablov. Moscow: APRAL, 2020, 552 p.
  18. Grigorenko V.B., Morozovа L.V. The usage of fractographic analysis to diagnostic the causes of destruction of products from medium-carbon steel. Trudy VIAM, 2018, no. 8 (68), paper no. 10. Available at: http://www.viam-works.ru (accessed: December 29, 2021). DOI: 10.18577/2307-6046-2018-0-8-98-111.
  19. Zhegina I.P., Prokhodtseva L.V., Shvanova N.F. Fractographic method for assessing the quality of the material. Aviacionnye materialy i tehnologii, 2001, no. 1, pp. 42–61.