Study of the resistance of carbon fibers to oxidation
Sidorina A.I., Safronov A.M. Study of the resistance of carbon fibers to oxidation // Proceedings of VIAM. 2022. No. 7. DOI: 10.18577/2307-6046-2022-0-7-63-73. URL: https://viam-works.ru/en/journal/2022/7/6
Keywords
carbon fibers, reinforcing fillers, thermal oxidative resistance of carbon fibers, thermal oxidation
Abstract
Presents the results of a study of the resistance to oxidation of various types and manufacturers carbon fibers by exposure to a given temperature for a certain time. High-strength carbon fibers with standard and intermediate Young’s modulus were investigated. The obtained results of short-term and long-term tests correlate with the results of thermogravimetric analysis. It is shown that among the studied fibers, high-strength carbon fibers with intermediate Young’s modulus have the greatest thermal oxidative resistance.
Reference list
- Kablov E.N. Formation of domestic space materials science. Vestnik RFFI, 2017, no. 3, pp. 97–105.
- Sidorina A.I. Multiaxial carbon fabrics in the products of aviation technology (review). Aviation materials and technologies, 2021, no. 3 (64), paper no. 10. Available at: http://www.journal.viam.ru (accessed: April 1, 2022). DOI: 10.18577/2713-0193-2021-0-3-105-116.
- Gunyaeva A.G., Sidorina A.I., Kurnosov A.O., Klimenko O.N. Polymeric composite materials of new generation on the basis of binder VSE-1212 and the filling agents alternative to ones of Porcher Ind. and Toho Tenax. Aviacionnye materialy i tehnologii, 2018, no. 3 (52), pp. 18–26. DOI: 10.18577/2071-9140-2018-0-3-18-26.
- Park S.-J. Carbon Fibers. Singapore: Springer Verlag, 2019, 358 p.
- Varshavsky V.Ya. Carbon fibres. Moscow: Varshavsky V.Ya., 2007, 496 p.
- Mikhailin Yu.A. Structural polymeric composite materials. Moscow: Nauchnye osnovy i tekhnologii, 2008, 822 p.
- Carbon fibers and carbon composites. Ed. E. Fitzer. Moscow: Mir, 1988, 338 p.
- Govorov A.V., Galiguzov A.A., Tikhonov N.A. et al. Investigation of the kinetics of oxidation of carbon fibers of various types. Novye ogneupory, 2015, no. 11, pp. 34–39.
- Comprehensive Composite Materials. Ed. A. Kelly, C. Zweben. Oxford: Pergamon Press, 2000, 6000 p.
- Tagawa M., Ohmae N., Umeno M. et al. Surface Characterization of Carbon Fibers Exposed to 5 eV Energetic Atomic Oxygen Beam Studied by Wetting Force Measurements. Japanese Journal of Applied Physics, 1991, vol. 30, pp. 2134–2138.
- Laptev A.B., Nikolayev E.V., Kolpachkov E.D. Thermodynamic characteristics of aging of polymeric composite materials under conditions of real exploitation. Aviaсionnye materialy i tehnologii, 2018, no. 3, pp. 80–88. DOI: 10.18577/2071-9140-2018-0-3-80-88.
- Kablov E.N. The role of fundamental research in the creation of new generation materials. Reports of the XXI Mendeleev Congress on General and Applied Chemistry: in 6 vols. St. Petersburg, 2019, vol. 4, p. 24.
- Vetrova E.Yu., Shchekin V.K., Kurs M.G. Comparative evaluation of methods for the determination of corrosion aggressivity of the atmosphere. Aviacionnye materialy i tehnologii, 2019, no. 1 (54), pp. 74–81. DOI: 10.18577/2071-9140-2019-0-1-74-81.
- Tong Y., Wang X., Su H., Xu L. Oxidation kinetics of polyacrylonitrile-based carbon fibers in air and the effect on their tensile properties. Corrosion Science, 2011, vol. 53, pp. 2484–2488.
- Kablov E.N. Materials of a new generation and digital technologies for their processing. Vestnik Rossiyskoy akademii nauk, 2020, vol. 90, no. 4, pp. 331–334.
- Wang Z.M., Yamashita N., Wang Z.X. et al. Air oxidation effects on microporosity, surface property, and CH4 adsorptivity of pitch-based activated carbon fibers. Journal of Colloid Interface Science, 2004, vol. 276, is. 1, pp. 143–150.
- Rong H., Ryu Z., Zheng J., Zhang Y. Effect of air oxidation of Rayon-based activated carbon fibers on the adsorption behavior for formaldehyde. Carbon, 2002, vol. 40, pp. 2291–2300.
- Poila E.J., Serra J.L. Oxidation of Carbon Fiber-Reinforced Silicon Carbide Matrix Composites at Reduced Oxygen Partial Pressures. Journal of the American Ceramic Society, 2011, vol. 94, is. 7, pp. 2185–2192.
- Hosokai S., Kishimoto K., Norinaga K. et al. Characteristics of Gas-Phase Partial Oxidation of Nascent Tar from the Rapid Pyrolysis of Cedar Sawdust at 700–800 °C. Energy & Fuels, 2010, vol. 24, pp. 2900–2009.
- Gourdin C. Ageing of carbon fibres of various origins. 4th Int. SAMPE Conference. Bourdeaux, 1983, pp. 49–61.
- Morgan P. Carbon Fibers and Their Composites. Florida: CRC Press, 2005, 1200 p.