Structure of a single crystalline intermetallic alloy based on Ni3Al after deformatoin-heat treatment

Bazyleva O.A., Karashaev M.M., Shestakov A.V., Dmitriev N.S.
Bazyleva O.A., Karashaev M.M., Shestakov A.V., Dmitriev N.S. Structure of a single crystalline intermetallic alloy based on Ni3Al after deformatoin-heat treatment // Proceedings of VIAM. 2022. No. 4. DOI: 10.18577/2307-6046-2022-0-4-3-12. URL: https://viam-works.ru/en/journal/2022/4/1
Keywords
Ni3Al
Abstract

Examines the study of the effect of deformation and subsequent heat treatment on the structure of single-crystal samples from a heat-resistant intermetallic alloy based on the Ni3Al compound. It is shown that at a degree of deformation (upsetting in a closed container) ≤40 %, no cracks are formed in the structure of the material under study. Subsequent thermal annealing after deformation promotes the process of recrystallization and the formation of a grain structure in deformed samples of an intermetallic alloy based on the Ni3Al compound.

Reference list
  1. Kablov E.N., Ospennikova O.G., Lomberg B.S. Strategic Directions for the Development of Structural Materials and Technologies for Their Processing for Aircraft Engines. Avtomaticheskaya svarka, 2013, no. 10, pp. 23–32.
  2. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  3. Kablov E.N., Bondarenko Yu.A., Echin A.B. Development of technology of cast superalloys directional solidification with variable controlled temperature gradient. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 24–38. DOI: 10.18577/2071-9140-2017-0-S-24-38.
  4. Kablov E.N. We really need a breakthrough. Izvestia, 2018. 6 Sept.
  5. Kablov E.N. VIAM materials and technologies for Aviadvigatel. Permskiye aviatsionnye dvigateli, 2014, no. 31, pp. 43–47.
  6. Svetlov I.L. High-temperature Nb–Si-composites. Materialovedenie, 2010, no. 9, pp. 29–38.
  7. Svetlov I.L. High-temperature Nb-Si-composites – replacement of single-crystal nickel heat-resistant alloys. Dvigatel, 2010, no. 5 (71). pp. 36–37.
  8. Kablov E.N. Formation of domestic space materials science. Vestnik RFFI, 2017, no. 3, pp. 97–105.
  9. Letnikov M.N., Lomberg B.S., Ovsepyan S.V. Investigation experimental alloys based on Ni–Al–Co ternary system for development a new high-temperature intermetallic alloy for disk application. Trudy VIAM, 2013, no. 10, paper no. 01. Available at: http://www.viam-works.ru (accessed: November 23, 2021).
  10. Ping Li, Shu-suo Li, Ya-fang Han. Influence of solution heat treatment on microstructure and stress rupture properties of a Ni3Al base single crystal superalloy IC6SX. Intermetallics, 2011, no. 19, pp. 182–186.
  11. Bazyleva O.A., Efimochkin I.Yu., Arginbaeva E.G., Kuptsov R.S., Karashaev M.M. Composite material based on an intermetallic alloy of the VKNA type, reinforced with oxides. Perspektivnye materialy, 2020, no. 10, pp. 19–27.
  12. Jozwik P., Polkowski W., Bojar Z. Applications of Ni3Al based intermetallic alloys – current stage and potential perceptivities. Materials, 2015, no. 8, pp. 2537–2568. DOI: 10.3390/ma8052537.
  13. Bolshakova A.N., Efimochkin I.Yu., Murasheva V.V. Mechanically alloyed dispersion-strengthened composite materials. Konstruktsii iz kompozitsionnykh materialov, 2015, no. 1 (137). pp. 36–40.
  14. Intermetallic alloy based on the nickel-aluminum-cobalt system: pat. RU 2603415 C1; filed 15.08.15; publ. 27.11.16.
  15. Povarova K.B., Lomberg B.S., Filin S.A., Kazanskaya N.K., Shkolnikov D.Yu., Bespalova M.D. Structure and properties of (β + γ)-alloys of the Ni–Al–Co system. Metally, 1994, no. 3, pp. 77–81.
  16. Povarova K.B., Kazanskaya N.K., Lomberg B.S., Shkolnikov D.Yu., Filin S.A., Bespalova M.D. Phase composition and structure of alloys based on NiAl of the Ni–Al–Co–M system, where M is Ti, Zr, Hf, V, Nb, Ta, Cr, Mo. Metally, 1996, no. 3, pp. 85–94.
  17. Povarova K.B., Filin S.A., Maslenkov S.B. Phase equilibria with the participation of the β-phase in Ni–Al–Me (Me – Co, Fe, Mn, Cu) systems at 900 and 1100 °C. Metally, 1993, no. 1, pp. 191–205.
  18. Povarova K.B., Kazanskaya N.K., Lomberg B.S., Bondarenko Yu.A., Shkolnikov D.Yu. Structural heat-resistant (β + γ)-alloys based on NiAl with increased low-temperature plasticity. Metallurg, 1996, no. 5, pp. 1.
  19. Kucheryaev V.V., Mironova N.A., Shishkov S.U. Research of technological features of Ni–Al–Co system ingots deformation. Trudy VIAM, 2016, no. 3 (39), paper no. 01. Available at: http://viam-works.ru (accessed: November 23, 2021). DOI: 10.18557/2307-6046-2016-0-3-1-1.
  20. Bazyleva O.A., Karashaev M.M., Shestakov A.V., E.G. Arginbaeva. Effect of annealing temperature on the homogeneity of inter-metallic alloy based on Ni3Al compound. Trudy VIAM, 2020, no. 8 (90), paper no. 01. Available at: http://www.viam-works.ru (accessed: November 23, 2021). DOI: 10.18577/2307-6046-2020-0-3-10.