Heat-resistant fibers and non-woven materials based on them for use in filter elements of gas turbine engines (review)

Obraztsova E.P., Titkova Yu.M., Donskih I.N.
Obraztsova E.P., Titkova Yu.M., Donskih I.N. Heat-resistant fibers and non-woven materials based on them for use in filter elements of gas turbine engines (review) // Proceedings of VIAM. 2022. No. 3. DOI: 10.18577/2307-6046-2022-0-3-3-14. URL: https://viam-works.ru/en/journal/2022/3/1
Keywords
heat-resistant fibers, filter materials, needle-punched nonwovens, surface density, operating temperature, strength characteristics, water absorption
Abstract

Presented an overview of heat-resistant fibers and nonwovens based on them. Their comparative characteristics, description, advantages and disadvantages for use as a basis for the use of afterburner regulators of gas turbine engines as part of air filters. The conclusion is made about the possibility of using nonwovens and the prospects for their application, as well as about a possible way to improve the characteristics of nonwovens to adapt to operating conditions at elevated and lowered temperatures.

Reference list
  1. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N. Materials and chemical technologies for aviation equipmen. Vestnik Rossiyskoy akademii nauk, 2012, vol. 82, no. 6, pp. 520–530.
  3. Kablov E.N. Composites: today and tomorrow. Metally Evrazii, 2015, no. 1, pp. 36–39.
  4. Istomin A.V., Bespalov A.S., Babashov V.G. Adding increased resistance to heat and sound insulation of material based on mixture of inorganic and plant fibers. Aviacionnye materialy i tehnologii, 2018, no. 4 (53), pp. 74–78. DOI: 10.18577/2071-9140-2018-0-4-74-78.
  5. Ivakhnenko Yu.A., Baruzdin B.V., Varrik N.M., Maksimov V.G. High-temperature fibrous sealing materials. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 272–289. DOI: 10.18577/2071-9140-2017-0-S-272-289.
  6. Babachov V.G., Stepanova E.V., Zimichev A.M., Basargin O.V. Oxide continuous fibers as a part of flexible high temperature insulation. Aviation materials and technology, 2021. no. 1 (62). paper no. 04. Available at: http://www.journal.viam.ru (accessed: December 2, 2021). DOI: 10.18577/2713-0193-2021-0-1-34-43.
  7. Sevostyanov A.G., Osmin N.A., Shcherbakov V.P. Mechanical technology of textile materials. Moscow: Legprombytizdat, 1989, 512 p.
  8. Abdullin I.Sh., Igragimov R.G., Muzafarova G.Sh., Samatova E.M. Modern technologies for the production of nonwoven materials. Vestnik Kazanskogo tekhnologicheskogo universiteta, 2014, vol. 17, no. 19, pp. 114–119.
  9. Aviation materials: reference book: in 12 vols. Moscow: VIAM, 2011. Vol. 9: Heat-shielding, heat-insulating and composite materials, high-temperature non-metallic coatings, p. 31.
  10. Perepelkin K.E. Modern chemical fibers and prospects for their use in the textile industry. Rossiyskiy khimicheskiy zhurnal (Zhurnal rossiyskogo khimicheskogo obshchestva imeni D.I. Mendeleyeva), 2002, vol. XLVI, no. 1, pp. 31–48.
  11. Kukin G.N., Soloviev A.N. Textile materials science (original textile materials): textbook for universities. 2nd ed., rev. and add. Moscow: Legprombytizdat, 1985. 216 p.
  12. Budnitsky G.A. New in the field of heat-resistant polymers and fibers. Moscow: NIITEKhIM, 1978, 88 p.
  13. Bespalov A.S., Kuzmin V.V., Babashov V.G. Damping fibrous material on basis of heat-resistant synthetic fibers. Trudy VIAM, 2015, no. 1, paper no. 04. Available at: http://www.viam-works.ru (accessed: December 02, 2021). DOI: 10.18577/2307-6046-2015-0-1-4-4.
  14. Kondrashov E.K., Kuzmin V.V., Minakov V.T., Ponamoreva E.A. Nonwoven materials on the basis of heat-resistant polymeric fibres and intertiled sealings. Trudy VIAM, 2013, no. 7, paper no. 05. Available at: http://www.viam-works.ru (accessed: December 02, 2021).
  15. Lubin J. Handbook of composite materials: in 2 books. Moscow: Mashinostroenie, 1988, book 1, 440 p.
  16. Kablov E.N., Kulagina G.S., Zhelezina G.F., Lons-kii S.L., Kurshev E.V. Microstructure research of the unidirectional organoplastic based on Rusar-NT aramid fibers and epoxy-polysulfone binder. Aviacionnye materialy i tehnologii, 2020, no. 4 (61), pp. 19–26. DOI: 10.18577/2071-9140-2020-0-4-19-26.
  17. Sergeeva E.A., Kostina K.D. Analysis of the range of aramid fibers and their properties. Vestnik tekhnologicheskogo universiteta, 2015, vol. 18, no. 14, pp. 124–125.
  18. Doriomedov M.S. Aramid fiber market: types, properties, application. Trudy VIAM, 2020, no. 11 (93), paper no. 06. Available at: http://www.viam-works.ru (accessed: December 02, 2021). DOI: 10.18577/2307-6046-2020-0-11-48-59.
  19. Konkin A.A., Kudryavtsev G.I., Shchetinin A.M. Heat-resistant and non-combustible fibres. Moscow: Khimiya, 1978. 424 p.
  20. Buhler K.-U. Heat- and heat-resistant polymers: trans. from Germ. Ed. Ya.S. Vygodsky. Moscow: Khimiya, 1984, 1056 p.
  21. Andronova N.A., Bessonov M.I., Laius L.A., Rudakov A.P. Polyimides are a new class of heat-resistant polymers. Moscow: Nauka, 1968, 211 p.
  22. Perepelkin K.E. Structure and properties of fibers. Moscow: Chemistry, 1985. 208 p.
  23. Musina T.K., Volokhina A.V., Shchetinin A.M. Polyimide and aramid fibers and threads with special properties based on them. V mire oborudovaniya, 2010, no. 2 (91). pp. 4–8.
  24. Zefirov N.S. Chemical Encyclopedia: in 35 vols. Moscow: Bolshaya rossiyskaya entsiklopediya, 1998, vol. 5. 783 p.
  25. Konkin A.A. Carbon and other heat-resistant fibrous materials. Moscow: Khimiya, 1974. 376 p.
  26. Dokuchaev V.N. The use of polyoxadiazole and carbon fibers and threads of OAO Svetlogorskkhimvolokno in the production of technical textile materials. Grodno: GIAP, 2015, pp. 13–16.
  27. Non-woven material ANAT-FM-T and non-woven arselon material ANAT-FM. Available at: https://termiz.all.biz/my-goods/materialy-netkanye (accessed: December 2, 2021).
  28. Kalinowski E., Urbanchik G.V. Chemical fibers. Moscow: Light industry, 1966, 251 p.
  29. Timoshkov P.N., Sevastyanov D.V., Usacheva M.N., Khrulkov A.V. Existing and promising technologies for producing PAN fibers (review). Trudy VIAM, 2019, no. 11 (83), paper no. 08. Available at: http://www.viam-works.ru (accessed: December 1, 2021). DOI: 10.18577/2307-6046-2019-0-11-68-74.
  30. Ryauzov A.N., Gruzdev V.A., Vaksheev I.P. Technology of production of chemical fibers: textbook for technical schools. 3rd ed. Moscow: Khumiya, 1980, 448 p.
  31. Aviation material of needle-punched slow-burning grades "AOM" and "AVIKS-AOM". Available at: https://aviksnpf.ru/goods/24308060/material-igloprobivnoy-trudnogoryuchiy-marki-aom-tu-8276-007-17364404-03 (accessed: December 1, 2021)
  32. Ponomareva E.A., Kondrashov E.K., Minakov V.T., Polepkina N.A. Development of hydrophobization technological mode of the needle-punched nonwoven materials on the basis of heat resistant fibers. Aviacionnye materialy i tehnologii, 2014, no. S3. pp. 11–16. DOI: 10.18577/2071-9140-2014-0-s3-11-16.