Inquiry of the properties of detection media for magnetic particle inspection
UDC
620.179.119
DOI
10.18577/2307-6046-2022-0-2-122-132
Article PDF (Russian)
(1021.26 KB)
How to cite
Lednev I.S. Inquiry of the properties of detection media for magnetic particle inspection // Proceedings of VIAM. 2022. No. 2. DOI: 10.18577/2307-6046-2022-0-2-122-132. URL: https://viam-works.ru/en/journal/2022/2/10
Keywords
non-destructive testing, magnetic particle inspection, dispersion medium, magnetic powder, magnetic indicator, flaw detection material, control technology, magnetic coagulation, detecting ability, concentration of magnetic powder
Abstract
The article presents the main properties of flaw detection materials for conducting magnetic particle inspection based on the analysis of GOST R ISO 9934-2–2011. A description of the verification of each parameter of flaw detection materials is presented and it is established how their nonconformity affects the effectiveness of control. The types of tests and which subjects should conduct them are shown. An experimental check of the detectability of defects depending on the particle sizes of flaw-detecting materials was carried out and it was found that the highest detectability is characteristic of a flaw-detecting material with a particle size of magnetic powder in the range of 0–15 microns.
Reference list
- Kablov E.N. Quality control of materials – guarantee of safety of aircraft operation. Aviacionnye materialy i tehnologii, 2001, no. 1, pp. 3–8.
- Kablov E.N. Aviation Materials Science in the XXI century. Prospects and tasks. Aviation materials. Selected Works VIAM 1932–2002. Moscow: MISIS – VIAM, 2002, pp. 23–47.
- Krasnov I.S., Lozhkova D.S., Dalin M.A. Evaluation of deficiency of titanium alloy forgings for probabilistic calculation of gas turbine engine disks fracture risk. Aviation materials and technologies, 2021, no. 2 (63), paper no. 12. Available at: https: //journal.viam.ru (accessed: October 3, 2021). DOI: 10.18577/2713-0193-2021-0-2-115-122.
- The concept of the development of the national standardization system of the Russian Federation for the period up to 2020 (approved by the order of the Government of
- the Russian Federation No. 1762-p from 24.09.2012). Available at:
- http://standard.gost.ru/wps/portal/!ut/p/c4/04_SB8K8xLLM9MSSzPy8xBz9CP0os3gLHzeXUFNLYwMLD1dLA09vR39DD68g4-BAI_2CbEdFACiQY_Q!/ (accessed: October 3, 2021).
- On standardization in the Russian Federation. Available at: https://docs.cntd.ru/document/ 420284277 (accessed: October 3, 2021).
- Standardization and technical regulation in the quality quality aspect: allowance. Ed. 3rd., rev. and add. Ulyanovsk: UlGTU, 2011, 258 p.
- About technical regulation. Available at: https://docs.cntd.ru/document/901836556 (accessed: October 3, 2021).
- Chesnokov A.G. On the issue of harmonization of standards. Moscow: Institute of Glass, 2003. Available at: https://glassinfo.ru/articles/2003_01_k_voprosu_o_garmonizaci_standartov.pdf (accessed: October 3, 2021).
- Chertishchev V.Yu., Ospennikova O.G., Boichuk A.S., Dikov I.A., Generalov A.S. Determina-tion of the size and depth of defects in multilayer PCM honeycomb structures based on the mechanical impedance value. Aviaсionnye materialy i tehnologii, 2020, no. 3 (60), pp. 72–94. DOI: 10.18577/2071-9140-2020-0-3-72-94.
- Boychuk A.S., Dikov I.A., Generalov A.S., Slavin A.V. Automated non-destructive inspection of three-layer honeycomb structures’ samples by ultrasonic through-transmission technique. Aviacionnye materialy i tehnologii, 2020, no. 2 (59), pp. 74–80. DOI: 10.18577/2071-9140-2020-0-2-74-80.
- Kablov E.N., Podzhivov N.Yu., Lutsenko A.N. On the need to create a single information and analytical center of aviation materials of the Russian Federation. Problemy mashinostroyeniya i avtomatizatsii, 2019, no. 3, pp. 28–34.
- Kosarina E.I., Generalov A.S., Demidov A.A. Questions of x-ray non-destructive testing in Russian State standardization system. Trudy VIAM, 2018, no. 11 (71), paper no. 10. Available at: http://viam-works.ru (accessed: October 3, 2021). DOI: 10.18577/2307-6046-2018-0-11-86-92.
- Shershak P.V. National standardization specifics of polymer composites materials tests methods. Trudy VIAM, 2019, no. 2 (74), paper no. 08. Available at: http://www.viam-works.ru (accessed: October 3, 2021).DOI: 10.18577/2307-6046-2019-0-2-77-88.
- State Standard R 56512-2015. Control non-destructive. Magnetic powder method. Typical technological processes. Mosocw: Starotinform, 2016, 56 p.
- State Standard R 1.0-2012. Standardization in the Russian Federation. Basic provisions. Moscow: Starotinform, 2013, 19 p.
- Shelikhov G.S. Magnetic solo flaw detection of parts and nodes. Moscow: Expert, 1995, 224 p.
- State Standard R ISO 9934-1-2011. Control non-destructive. Magnetic powder method. Part 1. Basic requirements. Moscow: Starotinform, 2019, 16 p.