Estimation of defect depth in multilayer PCM honeycomb during impedance testing with serial detectors

Chertishchev V.Yu., Boychuk A.S., Dikov I.A., Gorbovets M.A.
Chertishchev V.Yu., Boychuk A.S., Dikov I.A., Gorbovets M.A. Estimation of defect depth in multilayer PCM honeycomb during impedance testing with serial detectors // Proceedings of VIAM. 2022. No. 12. DOI: 10.18577/2307-6046-2022-0-12-107-120. URL: https://viam-works.ru/en/journal/2022/12/10
Keywords
acoustic impedance technique, mechanical impedance, acoustic control methods, honeycomb constructions, polymer composite materials, carbon fiber reinforced plastic
Abstract

Presents studies aimed at creating a methodology for assessing the depth of defects in multilayer honeycomb parts made of polymer composite materials during impedance testing with serial flaw detectors with the construction of C-scans. There are methods for estimating depth based on data with two independent parameters, which require special equipment and software. The study is aimed at creating a technique based on the analysis of only one parameter due to the knowledge of the mechanisms of the influence of the depth of defects on the impedance value and understanding the nature of the change in the signal of the flaw detector when the load changes.

Reference list
  1. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N. The key problem is materials. Trends and guidelines for Russia's innovative development. Moscow: VIAM, 2015, pp. 458–464.
  3. Kablov E.N., Ospennikova O.G., Kudinov I.I., Golovkov A.N., Generalov A.S., Knyazev A.V. Estimation of the probability of detecting operational defects in aircraft parts made of heat-resistant alloys using domestic and foreign flaw detection liquids. Defectoscopiya, 2021, no. 1, pp. 64–71. DOI: 10.31857/S0130308221010073.
  4. Kablov E.N. New generation materials. Zashchita i bezopasnost, 2014, no. 4, pp. 28–29.
  5. Murashov V.V. Control and diagnostics of multilayer structures made of polymer composite materials by acoustic methods. Moscow: Spektr, 2016, 244 p.
  6. Non-destructive testing: a reference book in 7 vols. General ed. V.V. Klyuev. Moscow: Mashinostroenie, 2004, vol. 3: Ultrasonic testing. Ed. I.N. Ermolov, Yu.V. Lange, 864 p.
  7. Murashov V.V., Generalov A.S. Control of multilayer adhesive structures operating in severe climatic condition. Aviacionnye materialy i tehnologii, 2014, no. 2, pp. 59–67. DOI: 10.18577/2071-9140-2014-0-2-59-67.
  8. Murashov V.V. Research and improvement of acoustic low-frequency control methods of products from layered plastics and multilayered glued of constructions. Aviacionnye materialy i tehnologii, 2018, no. 4 (53), pp. 87–93. DOI: 10.18577/2071-9140-2018-0-4-87-93.
  9. Shershak P.V., Yakovlev N.O., Shokin G.I., Kutsevich K.E., Popkova E.A. Evaluation method and factors influencing the bonding quality between face and honey-comb cores in floor and interior aircraft panels. Aviacionnye materialy i tehnologii, 2020, no. 2 (59), pp. 81–88. DOI: 10.18577/2071-9140-2020-0-2-81-88.
  10. Chertishchev V.Yu., Boychuk A.S., Dikov I.A., Yakovleva S.I., Generalov A.S. Determination of the Defect Depth in Multilayer PCM Structures by Acoustic Methods Based on the Mechanical Impedance. Defektoskopiya, 2018, no. 8, pp. 21–34. DOI: 10.1134/50130308218080031.
  11. Chertishchev V.Yu., Ospennikova O.G., Boichuk A.S., Dikov I.A., Generalov A.S. Determina-tion of the size and depth of defects in multilayer PCM honeycomb structures based on the mechanical impedance value. Aviaсionnye materialy i tehnologii, 2020, no. 3 (60), pp. 72–94. DOI: 10.18577/2071-9140-2020-0-3-72-94.
  12. Starikovsky G.P., Zhovner P.B. Non-destructive testing of three-layer integral structures made of polymer composite materials. Kontrol. Diagnostika, 2012, no. 6, pp. 58–62.
  13. Nondestructive Evaluation System Reliability Assessment: Handbook. Military and Government Specs & Standards (Naval Publications and Form Center), 2009, 171 p.
  14. Krasnov I.S., Lozhkova D.S., Dalin M.A. Evaluation of deficiency of titanium alloy forgings for probabilistic calculation of gas turbine engine disks fracture risk. Aviation materials and technologies, 2021, no. 2 (63), paper no. 12. Available at: https: //journal.viam.ru (accessed: June 01, 2022). DOI: 10.18577/2713-0193-2021-0-2-115-122.
  15. Lange Yu.V. Acoustic low-frequency methods and means of non-destructive testing of multilayer structures. Moscow: Mashinostroenie, 1991, 272 p.