Effect of heat treatment of sintered Pr–Dy–Fe–Co–B magnets on their coercivity
Korolev D.V., Valeev R.A., Morgunov R.B., Piskorsky V.P. Effect of heat treatment of sintered Pr–Dy–Fe–Co–B magnets on their coercivity // Proceedings of VIAM. 2022. No. 12. DOI: 10.18577/2307-6046-2022-0-12-39-48. URL: https://viam-works.ru/en/journal/2022/12/4
Keywords
gyroscopes, ring magnets with radial texture, coercive force, thermal stability
Abstract
The coercive force of sintered Pr–Dy–Fe–Co–B magnets plays a decisive role for the quality and accuracy of gyroscopes and other navigation devices. The residual magnetization also plays an important role in determining the sensitivity threshold and the accuracy of the such systems. The chemical design of magnets, i. e. the selection of chemical composition, does not fully realize the best characteristics. Therefore, some success can be achieved by applying heat treatment. The article shows that the selection of the heat treatment mode of sintered magnets allows to improve their characteristics to technically acceptable values, which greatly simplifies the manufacturing technology of such magnets.
Reference list
- Buzenkov A.V., Valeev R.A., Piskorsky V.P., Morgunov R.B. The effect of the content of yttrium on the properties of the sintered Magnets Nd–Dy–Y–Fe–Co–B. Trudy VIAM, 2022, no. 4 (110), paper no. 11. Available at: http://www.viam-works.ru (accessed: July 15, 2022). DOI: 10.18577/2307-6046-2022-0-4-108-117.
- Piskorsky V.P., Valeev R.A., Korolev D.V., Morgunov R.B., Rezchikova I.I. Terbium and gadolinium dopin influence on thermal stability and magnetic properties of sintered magnets Pr–Tb–Gd–Fe–Co–B. Trudy VIAM, 2019, no. 7 (79), paper no. 07. Available at: http://www.viam-works.ru (accessed: July 15, 2022). DOI: 10.18577/2307-6046-2019-0-7-59-66.
- Korolev D.V., Stolyankov Yu.V., Piskorsky V.P., Valeev R.A., Bahmetiev M.V., Dvorezkaya E.V., Koplak O.V., Morgunov R.B. Magnetic properties and magnetic strip domains in micro stripes PrDyFeCoB. Aviation materials and technologies, 2021, no. 3 (64), paper no. 08. Available at: http://www.journal.viam.ru (accessed: July 15, 2022). DOI: 10.18577/2713-0193-2021-0-3-86-93.
- Morgunov R.B., Piskorskiy V.P., Valeev R.A., Korolev D.V. The thermal stability of rare-earth magnets supported by means of the magnetocaloric effect. Aviacionnye materialy i tehnologii, 2019, no. 1 (54), pp. 88–94. DOI: 10.18577/2071-9140-2019-0-1-88-94.
- Mezentsev G.M. Analysis of a two-mass model of linear motion of a dynamically tuned gyroscope. Miass: South Ural State Univ., 2019, 94 p.
- Vasilevsky N.I. Development of a dynamically tuned gyroscope taking into account its vibrational characteristics. Miass: South Ural State Univ., 2018, 77 p.
- Chirkin D.S., Roslovets P.V., Tatarinov F.V., Novikov L.Z. Reducing the drift of a dynamically tuned gyroscope from run to run. Inzhenernyi zhurna: nauka i innovatsii, 2017, no. 1, pp. 1–14. DOI: 10.18698/2308-6033-2017-01-1579.
- Topilskaya S.V., Borodulin D.S., Kornyukhin A.V. Experimental evaluation of allowable mechanical impacts on a dynamically adjustable gyroscope. Vestnik MGTU im. N.E. Baumana. Ser.:Instrumentation, 2018, no. 4, pp. 69–79.
- Golovanov V.A. Gyroscopic orientation. St. Petersburg, 2004, 92 p.
- Kablov E.N., Ospennikova O.G., Piskorskij V.P. et al. Ring magnets with radial texture for dynamically tuned gyroscopes. Aviacionnye materialy i tehnologii, 2014, no. S5, pp. 89–94. DOI: 10.18577/2071-9140-2014-0-S5-89-94.
- Fuerst C.D., Herbst J.F., Alson E.A. Magnetic properties of Nd2(CoxFe1–x)14B. Journal of Magnetism and Magnetic Materials, 1986, vol. 54–56, pp. 567–569.
- Sinnema D.B., Radwanski R.J., Franse J.J.M. et al. Magnetic properties of ternary rare-earth compounds of the type R2Fe14B. Journal of Magnetism and Magnetic Materials, 1984, vol. 44, nо. 3. P. 333–341.
- Pedziwiatr A.T., Wallace W.E. Structure and magnetism of the R2Fe14–xCoxB (R = Dy and Er). Journal of Magnetism and Magnetic Materials, 1987, vol. 66, nо. 3, pp. 63–68.
- Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Knyazev A.V., Suleimanov E.V. Fundamentals of X-ray phase analysis. N. Novgorod, 2005, 23 p.
- Boyarkina O.V., Zotov M.I., Kyashkin V.M. et al. Physical methods for studying solids: electron microscopy and X-ray diffraction analysis. Saransk: Mordovia Univ., 2012, 96 p.
- Grossinger R., Krewenka R., Kirchmayr H.R. et al. Magnetic anisotropy in Pr2(Fe1–xCox)14 B compounds. Journal of the Less-Common Metals, 1987, vol. 132, pp. 265–272.
- Abache C., Oesterreicher H. Magnetic properties of compounds R2Fe14B. Journal Applied Physics, 1985, vol. 57, pp. 4112–4114.
- Pedziwiatr A.T., Wallace W.E. Structure and magnetism of the R2Fe14–xCoxB ferromagnetic systems (R = Dy and Er). Journal of Magnetism and Magnetic Materials, 1987, vol. 66, pp. 63–68.
- Pedziwiatr A.T., Chen H.Y., Wallace W.E. Magnetism of the Tb2Fe14–xCoxB system. Journal of Magnetism and Magnetic Materials, 1987, vol. 67, pp. 311–315.
- Abache C., Oesterreicher H.J. Magnetic anisotropies and spin reorientations of R2Fe14B-type compounds. Journal Applied Physics, 1986, vol. 60, pp. 3671–3679.
- Zhi-dong Z., Sun X.K., Zhen-Chen Z. et al. Effects of partial Co substitution on structural and magnetic properties of (Pr, Gd)2Fe14B compounds. Journal of Magnetism and Magnetic Materials, 1991, vol. 96, pp. 215–218.
- Perigo E.A., Takiishi H., Motta C.C., Faria R.N. On the squareness factor behavior of RE–Fe–B (RE = Nd or Pr). IEEE Transactions on Magnetics, 2009, vol. 45, nо. 10, pp. 4431–4434.
- Faria R.N., Takiishi H., Lima L.F.C.P., Costa I. Praseodymium-based HD-sintered magnets produced using a mixture of cast alloys. Journal of Magnetism and Magnetic Materials, 2001, vol. 237, pp. 261–266.
- Musalimov V.M., Rotts Yu.A., Astafiev S.A., Amvrosyeva A.V. Calculation of reliability of elastic elements of micromechanical gyroscopes. St. Petersburg: St. Petersburg State Univ. of information, technologies, mechanics and optics, 2009, 128 p.
- Dynamically adjustable gyroscope: pat. 2687169 Rus. Federation; filed 17.04.18; publ. 07.05.19.