Improvement of the tribotechnical characteristics of beryllium-containing steel VNS32-VI by surface modification

Sevalnev G.S., Druzhinina M.E., Dulnev K.V., Mosolov A.N., Fomina L.P., Chirkov I.A.
Sevalnev G.S., Druzhinina M.E., Dulnev K.V., Mosolov A.N., Fomina L.P., Chirkov I.A. Improvement of the tribotechnical characteristics of beryllium-containing steel VNS32-VI by surface modification // Proceedings of VIAM. 2022. No. 11. DOI: 10.18577/2307-6046-2022-0-11-3-15. URL: https://viam-works.ru/en/journal/2022/11/1
Keywords
beryllium, beryllium-containing steel, hardness, wear resistance, friction coefficient
Abstract

Microstructure, hardness and tribotechnical characteristics of beryllium-containing steel VNS32-VI were studied after strengthening heat treatment and final ion nitriding. It was found that the microstructure of samples processed according to various methods does not differ, and the thickness of the diffusion layer is 100 μm. The alloying element distribution study showed that the surface was dominated by Cr, Mo and Nb having a high affinity for nitrogen. The best tribotechnical properties were possessed by samples for which the dispersion hardening process was combined with final ion nitriding.

Reference list
  1. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N. What is the future to be made of? Materials of a new generation, technologies for their creation and processing – the basis of innovation. Krylya Rodiny, 2016, no. 5, pp. 8–18.
  3. Kablov E.N., Bakradze M.M., Gromov V.I., Voznesenskaya N.M., Yakusheva N.A. New high strength structural and corrosion-resistant steels for aerospace equipment developed by FSUE «VIAM» (review). Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 3–11. DOI: 10.18577/2071-9140-2020-0-1-3-11.
  4. Kablov E.N. New Generation Materials and Technologies for Their Digital Processing. Herald of the Russian Academy of Sciences, 2020, vol. 90, no. 2, pp. 225–228.
  5. Ospennikova O.G. Implementation results of the strategic directions on creation of new generation of heat-resisting cast and wrought alloys and steels for 2012–2016. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 17–23. DOI: 10.18577/2071-9140-2017-0-S-17-23.
  6. Papirov I.I. Beryllium in alloys: a reference book. Moscow: Energoatomizdat, 1986, 184 p.
  7. Zhubaev A.K., Bekturgan N.B., Kuvatbaeva K.K., Nurtazina A.S. Investigation of the phase-structural state of stainless steel with beryllium. Fundamentalnye problemy radioelektronnogo priborostroyeniya, 2014, vol. 14, no. 3, pp. 70–73.
  8. Dvoretskov R.M., Volkova O.S., Radzikovskaya V.N., Burova V.N. Determination of beryllium in modern aviation materials by atomic emission spectrometry with inductively coupled plasma. Trudy VIAM, 2016, no. 4, paper no. 5. Available at: http://www.viam-works.ru (accessed: June 14, 2022). DOI: 10.18577/2307-6046-2016-0-4-5-5.
  9. Naik B.G., Sivasubramanian N. Applications of beryllium and its alloys. Mineral Processing and Extractive Metullargy Review, 1994, vol. 13, no. 1, pp. 243–251.
  10. Papirov I.I. Structure and properties of beryllium alloys: a reference book. Moscow: Energoizdat, 1981, 368 p.
  11. Cherbakov A.I., Mosolov A.N., Kalicev V.A. Recovery of technology for the beryllium-containing steel VNS-32-VI obtaining. Trudy VIAM, 2014, no. 05, paper no. 01. Available at: http://www.viam-works.ru (accessed: February 1, 2022). DOI: 10.18577/2307-6046-2014-0-5-1-1.
  12. Stainless PH steel: certificate of authorship 541374 USSR, no. 2120727/01; filed 03.04.75; publ. 15.05.91.
  13. Mosolov A.N., Sevalnev G.S., Krylov S.A., Skugorev A.V., Chirkov I.A. Study of the structure and properties of beryllium-containing steel VNS32-VI. Trudy VIAM, 2022, no. 5 (111), paper no. 01. Available at: http://www.viam-works.ru (accessed: June 01, 2022). DOI: 10.18577/2307-6046-2022-0-5-3-14.
  14. Kuksenova L.I., Gerasimov S.A., Alekseeva M.S., Gromov V.I. Influence of vacuum chemical and thermal processing on wear resistance of VKS-7 and VKS-10 steels. Aviacionnye materialy i tehnologii, 2018, no. 1 (50), pp. 3–8. DOI: 10.18577/2071-9140-2018-0-1-3-8.
  15. Czerwinski F. Heat treatment – Conventional and Novel Applications. London: IntechOpen, 2012, 422 p.
  16. Structural materials: a reference book. Ed. B.N. Arzamasov. Moscow: Mashinostroenie, 1990, 688 p.
  17. Aleksandrov V.G., Bazanov B.I. Reference book on aviation materials and technology of their application. Moscow: Transport, 1979, 263 p.
  18. Minkevich A.N. Chemical-thermal treatment of metals and alloys. Moscow: Mashinostroenie, 1965, 493 p.
  19. Minkevich A.N. Chemical-thermal treatment of steel. Moscow: Mashgiz, 1950, 432 p.
  20. Yao J., Yan F., Chen B. et al. Dual-strengthening of steel surface and bulk via synergistic effect of plasma nitriding: a case study of M50 steel. Surface and Coatings Technology, 2021, vol. 409, p. 126910.
  21. Ooi S., HKDH B. Duplex hardening of steels for aeroengine bearings. Iron and Steel Institute of Japan International, 2012, vol. 52, no. 11, pp. 1927–1934.
  22. Streit E., Trojahn W. Duplex Hardening for Aerospace Bearing Steels. ASTM special technical publication, 2002, vol. 1419, pp. 386–398.
  23. Sevalnev G.S., Sevalneva T.G., Kolmakov A.G., Dulnev K.V., Yazvitsky M.Yu. Influence of the phase composition of austenitic-martensitic trip-steel VNS9-Sh on the characteristics of dry sliding friction in tribocontact with steel ShKh15. Deformatsiya i razrushenie materialov, 2021, no. 10, pp. 20–27. DOI: 10.31044/1814-4632-2021-10-20-27.
  24. Arzamasov B.N., Bratukhin A.G., Eliseev Yu.S., Panayoti T.A. Ionic chemical-thermal treatment of alloys. Moscow: MSTU im. N.E. Bauman, 1999, 400 p.
  25. Goodremont E. Special steels: in 2 vols. 2nd ed., rev. Moscow: Metallurgiya, 1966, vol. 2. 532 p.
  26. Petrova L.G., Aleksandrov V.A., Zyuzin D.M. Regulated processes of nitriding of corrosion-resistant steels. Vestnik Moskovskogo avtomobilno-dorozhnogo instituta (gosudarstvennogo tekhnicheskogo universiteta), 2003, no. 1, pp. 20–26.
  27. Lakhtin Yu.M., Kogan Ya.D. Nitriding of steel. Moscow: Mashinostroenie, 1976, 256 p.
  28. Kuksenova L.I., Alekseeva M.S. Investigation of the structural state and wear resistance of nitrided iron alloys with different types of crystal lattice. Vestnik nauchno-tekhnicheskogo razvitiya, 2019, no. 9, pp. 21–29.
  29. Eliseev E.A., Sevalnev G.S., Doroshenko A.V., Druzhinina M.E. Influence of time-temperature parameters of long-duration exposure on transformations in structural steels (review). Aviation materials and technologies, 2021, no. 2 (63), paper no. 02. Available at: http://www.journal.viam.ru (accessed: June 14, 2022). DOI: 10.18577/2713-0193-2021-0-2-15-23.