Development of standard samples of magnesium alloy ML19

Karachevtsev F.N., Eroshkin S.G., Trofimov N.V., Leonov A.A., Popovnina N. A.
Karachevtsev F.N., Eroshkin S.G., Trofimov N.V., Leonov A.A., Popovnina N. A. Development of standard samples of magnesium alloy ML19 // Proceedings of VIAM. 2022. No. 1. DOI: 10.18577/2307-6046-2022-0-1-26-34. URL: https://viam-works.ru/en/journal/2022/1/3
Keywords
standard sample, magnesium alloys, spectroscopy, manufacturing technology, type approval, uncertainty
Abstract

The development of technology for the manufacture and production of reference materials (CRMs) of the composition of the magnesium alloy ML19 has been carried out. Manufactured material for CRM pipes with a diameter of 40 mm and a height of 30 mm. Tests of the material for CRM have been carried out in order to validate it. The metrological characteristics of the CRM were established, a metrological examination was carried out, and the conclusion on the verification of the CRM test results for the composition of the ML19 magnesium alloy.

Reference list
  1. Antipov V.V. Prospects for development of aluminium, magnesium and titanium alloys for aerospace engineering. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 186–194. DOI: 10.18577/2107-9140-2017-0-S-186-194.
  2. Kablov E.N., Ospennikova O.G., Vershkov A.V. Rare metals and rare-earth elements are materials for modern and future high technologies. Aviacionnye materialy i tehnologii, 2013, no. S2, pp. 3–10.
  3. Duyunova V.A., Volkova E.F., Uridiya Z.P., Trapeznikov A.V. Dynamics of the development of magnesium and cast aluminum alloys. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 225–241. DOI: 10.18577/2071-9140-2017-0-S-225-241.
  4. Karachevtsev F.N., Eroshkin S.G., Mos-tayev I.V., Akinina M.V., Slavin А.V. Development of standard samples of magnesium alloys VML20 and VMD16. Trudy VIAM, 2021, no. 5 (99), paper no. 04. Available at: http://www.viam-works.ru (accessed: September 16, 2021). DOI: 10.18577/2307-6046-2021-0-5-39-47.
  5. Kablov E.N., Chabina E.B., Morozov G.A., Muravskaya N.P. Conformity assessment of new materials using high-level RM and MI. Kompetentnost, 2017, no. 2, pp. 40–46.
  6. Lutsenko A.N., Perov N.S., Chabina E.B. The new stages of development of Testing Center. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 460–468. DOI: 10.18577/2071-9140-2017-0-S-460-468.
  7. Karpov Yu.A., Baranovskaya V.B. Analytical control is an integral part of material diagnostics. Zavodskaya laboratoriya. Diagnostika materialov, 2017, vol. 83, no. 1-I. pp. 5–12.
  8. Karpov Yu.A. Analytical control of metallurgical production. Moscow: Metallurgiya, 1995, pp. 97–107.
  9. Otto M. Modern methods of analytical chemistry: in 2 vols. Moscow: Technosfera, 2003, vol. 1. 416 p.
  10. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  11. Fariñas J.C., Rucandio I., Pomares-Alfonso M.S. et al. Determination of rare earth and concomitant elements in magnesium alloys by inductively coupled plasma optical emission spectrometry . Talanta, 2016, no. 154, pp. 53–62. DOI: 10.1016/j.talanta.2016.03.047.
  12. Dvoretskov R.M., Baranovskaya V.B., Karachevtsev F.N., Letov A.F. Determination of rare earth metals in magnesium alloys by inductively coupled plasma atomic emission spectrometry. Izmeritelnaya tekhnika, 2019, no. 4, pp. 62–66.
  13. State Standard 7728–79. Magnesium alloys. Methods of spectral analysis. Moscow: Publishing house of standards, 2004, 11 p.
  14. RMG 53–2002. Standard samples. Assessment of metrological characteristics using standards and exemplary measuring instruments. Moscow: Publishing house of standards, 2004, 8 p.
  15. State Standard 8.315–2019. Standard samples of the composition and properties of substances and materials. Basic provisions. Moscow: Standartinform, 2019, 33 p.