Ceramics based on organosilicon polymers-precursors: microstructure and properties (review)

Part 1
Shestakov A.M.
Shestakov A.M. Ceramics based on organosilicon polymers-precursors: microstructure and properties (review). Part 1 // Proceedings of VIAM. 2021. No. 8. DOI: 10.18577/2307-6046-2021-0-8-21-33. URL: https://viam-works.ru/en/journal/2021/8/3
Keywords
silicon carbonitride, ceramics, ceramic foams, organosilicon polymers, silicon oxycarbide, pyrolysis.
Abstract

The paper considers the process of pyrolysis of polymers-precursors, and also shows the influence of various parameters of technological processes for obtaining ceramics on its composition, structure, and properties. The main types of binary, ternary and multicomponent silicon-based ceramics, methods of its preparation, features of structure and properties are considered, and promising directions of application of ceramics are determined. The possibility of obtaining porous ceramic materials (ceramic foams) with controlled porosity and ceramic composite materials with a given composition is noted.

Reference list
  1. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N. Composites: today and tomorrow. Metally Evrazii, 2015, no. 1, pp. 36–39.
  3. Grashchenkov D.V. Strategy of development of non-metallic materials, metal composite materials and heat-shielding. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 264–271. DOI: 10.18577/2071-9140-2017-0-S-264-271.
  4. Grashchenkov D.V., Evdokimov S.A., Zhestkov B.E., Solntsev S.St., Shtapov V.V. Research of thermochemical influence of the air plasma flow on high-temperature ceramic composite material. Aviacionnye materialy i tehnologii, 2017, no. 2 (47), pp. 31–40. DOI: 10.18577/2071-9140-2017-0-2-31-40.
  5. Kablov E.N., Nikiforov A.A., Demin S.A., Chesnokov D.V., Vinogradov S.S. Promising coatings for corrosion protection of carbon steels. Stal, 2016, no. 6, pp. 70–81.
  6. Grashchenkov D.V., Efimochkin I.Yu., Bolshakova A.N. High-temperature metal-matrix composite materials reinforced with particles and fibers of refractory compounds. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 318–328. DOI: 10.18577/2071-9140-2017-0-S-318-328.
  7. Kablov E.N., Grashchenkov D.V., Isaeva N.V., Solntsev S.S., Sevastianov V.G. High-temperature structural composite materials based on glass and ceramics for advanced aircraft products. Steklo i keramika, 2012, no. 4, pp. 7–11.
  8. Sorokin O.Yu., Grashhenkov D.V., Solntsev S.St., Evdokimov S.A. Ceramic composite materials with high oxidation resistance for the novel aircrafts (review). Trudy VIAM, 2014, no. 6, paper no. 8. Available at: http://www.viam-works.ru (accessed: April 12, 2021). DOI: 10.18577/2307-6046-2014-0-6-8-8.
  9. Minakov V.T., Solntsev S.S. Ceramic-matrix composites. Vse materialy. Entsiklopedicheskiy spravochnik, 2007. no. 2, pp. 5–9.
  10. Kablov E.N., Grashchenkov D.V., Isaeva N.V., Solntsev S.St. Promising high-temperature ceramic composite materials. Rossiyskiy khimicheskiy zhurnal, 2010, vol. LIV, no. 1, pp. 20–24.
  11. Сорокин О.Ю. К вопросу о механизме взаимодействия углеродных материалов с кремнием (обзор). Авиационные материалы и технологии. 2015. № 1 (34). С. 65–70. DOI: 10.18577/2071-9140-2015-0-1-65-70.
  12. Shvets N.I., Minakov V.T., Papkov V.S. et al. Investigation of thermochemical transformations of polycarbosilane precursors into a ceramic matrix. Zhurnal prikladnoy khimii, 2014, vol. 87, no. 6, pp. 793–799.
  13. Shestakov A.M., Minakov V.T., Shvets N.I. et al. Ceramic-forming polymeric precursors based on polycarbosilane and diallylbisphenol A. Zhurnal prikladnoy khimii, 2014, vol. 87, no. 11, pp. 1626–1635.
  14. Shestakov A.M., Shvets N.I., Khaskov M.A., Ponomarenko S.A., Minakov V.T. Compositions based on polycarbosilane and bismaleimide are precursors of ceramic-matrix composite materials. Zhurnal prikladnoy khimii, 2015, vol. 88, no. 9, pp. 1339–1347.
  15. Shestakov A.M., Khaskov M.A., Sorokin O.Yu. Organosilicon polymer compounds based inorganic fibers for high-temperature composite materials (review). Trudy VIAM, 2019, no. 1 (73), paper no. 09. Available at: http://viam-works.ru (accessed: April 12, 2021). DOI: 10.18577/2307-6046-2019-0-1-74-91.
  16. Shestakov A.M. Ceramics based on organosilicon polymers-precursors: methods of preparation and properties (review). Trudy VIAM, 2020, no. 11 (93), paper no. 9. Available at: http://www.viam-works.ru (accessed: April 12, 2021). DOI: 10.18577/2307-6046-2020-0-11-76-92.
  17. Colombo P., Mera G., Riedel R., Soraru G.D. Polymer-Derived Ceramics: 40 Years of Research and Innovation in Advanced Ceramics. Journal of the American Ceramic Society, 2010, vol. 93, no. 7, pp. 1805–1837.
  18. Blum Y.D., Schwartz K.B., Laine R.M. Preceramic Polymer Pyrolysis. Part 1: Pyrolytic Properties of Polysilazanes. Journal of Materials Science, 1989, vol. 24, no. 5, pp. 1707–1718.
  19. Wan J., Gasch M.J., Mukherjee A.K. Silicon Nitride-Silicon Carbide Nanocomposites Fabricated by Electric-Field-Assisted Sintering. Journal of the American Ceramic Society, 2003, vol. 86, no. 3, pp. 526–528.
  20. Esfehanian M., Oberacker R., Fett T., Hoffmann M.J. Development of Dense Filler-Free Polymer-Derived SiOC Ceramics by Field-Assisted Sintering. Journal of the American Ceramic Society, 2008, vol. 91, no. 11, pp. 3803–3805.
  21. Rapid thermal process for obtaining silica coatings: pat. US № 5059448; filed 18.06.90; publ. 22.10.91.
  22. Dzivenko D.A., Zerr A., Bulatov V.K. et al. High-Pressure Multianvil Synthesis and Structure Refinement of Oxygen-Bearing Cubic Zirconium(IV) Nitride. Advanced Materials, 2007, vol. 19, no. 14, pp. 1869–1873.
  23. Danko G.A., Silberglitt R., Colombo P. et al. Comparison of Microwave Hybrid and Conventional Heating of Preceramic Polymers to Form Silicon Carbide and Silicon Oxycarbide Ceramics. Journal of the American Ceramic Society, 2000, vol. 83, no. 7, pp. 1617–1625.
  24. Pivin J.C., Colombo P. Ceramic Coatings by Ion Irradiation of Polycarbosilanes and Polysiloxanes. Part I. Conversion Mechanism. Journal of Materials Science, 1997, vol. 32, no. 23, pp. 6163–6173.
  25. Pivin J.C., Colombo P. Ceramic Coatings by Ion Irradiation of Polycarbosilanes and Polysiloxanes. Part II. Hardness and Thermochemical Stability. Journal of Materials Science, 1997, vol. 32, no. 23, pp. 6175–6182.
  26. Pivin J.C., Colombo P., Soraru G.D. Comparison of Ion Irradiation Effects in Silicon-Based Preceramic Thin Films. Journal of the American Ceramic Society, 2000, vol. 83, no. 4, pp. 713–720.
  27. Kroke E., Li Y.-L., Konetschny C. et al. Silazane derived ceramics and related materials. Materials Science and Engineering, ser.: Reports, 2000, vol. 26, no. 4–6, pp. 97–199.
  28. Haug R., Weinmann M., Bill J., Aldinger F. Plastic forming of preceramic polymers. Journal of the European Ceramic Society, 1999, vol. 19, no. 1, pp. 1–6.
  29. Greil P. Polymer derived engineering ceramics. Advanced Engineering Materials, 2000, vol. 2, no. 6, pp. 339–348.
  30. Konetschny C., Galusek D., Reschke S. et al. Dense silicon carbonitride ceramics by pyrolysis of cross-linked and warm pressed polysilazane powders. Journal of the European Ceramic Society, 1999, vol. 19, no. 16, pp. 2789–2796.
  31. Yu S.H., Riman R.E., Danforth S.C., Leung R.Y. Pyrolysis of Titanium-Metal-Filled Poly(siloxane) Preceramic Polymers: Effect of Atmosphere on Pyrolysis Product Chemistry. Journal of the American Ceramic Society, 1995, vol. 78, no. 7, pp. 1818–1824.
  32. Breval E., Hammond M., Pantano C.G. Nanostructural Characterization of Silicon Oxycarbide Glasses and Glass-Ceramics. Journal of the American Ceramic Society, 1994, vol. 77, no. 11, pp. 3012–3018.
  33. Liew L.-A., Saravanan R.A., Bright V.M. et al. Processing and characterization of silicon carbon-nitride ceramics: application of electrical properties towards MEMS thermal actuators. Sensors and Actuators. A: Physical, 2003, vol. 103, no. 1–2, pp. 171–181.
  34. Colombo P., Martucci A., Fogato O., Villoresi P. Silicon Carbide Films by Laser Pyrolysis of Polycarbosilane. Journal of the American Ceramic Society, 2001, vol. 84, no. 1, pp. 224–226.
  35. Yoon T.-H., Park S.-H., Min K.-I. et al. Novel inorganic polymer derived microreactors for organic microchemistry applications. Lab on a Chip, 2008, vol. 8, no. 9, pp. 1454–1459.
  36. Method for coating a surface: pat. US № 6316057B1; filed 26.05.98; publ. 03.12.98.
  37. Fu Sh., Zhu M., Zhu Y. Organosilicon polymer-derived ceramics: An overview. Journal of Advanced Ceramics, 2019, vol. 8, no. 4, pp. 457–478.
  38. Wang Y., Xiao P., Zhou W. et al. Microstructures, dielectric response and microwave absorption properties of polycarbosilane derived SiC powders. Ceramics International, 2018, vol. 44, no. 4, pp. 3606–3613.
  39. Mishra M.K., Kumar S., Ranjan A., Prasad N.E. Processing, properties and microstructure of SiC foam derived from epoxy-modified polycarbosilane. Ceramics International, 2018, vol. 44, no. 2, pp. 1859–1867.
  40. Eick B.M., Youngblood J.P. SiC nanofibers by pyrolysis of electrospun preceramic polymers. Journal of Materials Science, 2009, vol. 44, no. 1, pp. 160–165.
  41. Hu T.-J., Li X.-D., Li G.-Y. et al. SiC fibers with controllable thickness of carbon layer prepared directly by preceramic polymer pyrolysis routes. Materials Science and Engineering: B, 2011, vol. 176, no. 9, pp. 706–710.
  42. Ma Y., Wang S., Chen Z.-H. Effects of high-temperature annealing on the microstructures and mechanical properties of Cf/SiC composites using polycarbosilane. Materials Science and Engineering: A, 2011, vol. 528, no. 7–8, pp. 3069–3072.
  43. Mu Y., Zhou W., Luo F., Zhu D. Effects of BN/SiC dual-layer interphase on mechanical and dielectric properties of SiCf/SiC composites. Ceramics International, 2014, vol. 40, no. 2, pp. 3411–3418.
  44. Fu X., Zhu N., Peng Zh. One-step synthesis and characterization of tree-like branched α-Si3N4 nano/submicron-structures by pyrolysis of a polymer precursor. Solid State Sciences, 2012, vol. 14, no. 9, pp. 1267–1272.
  45. Peng Zh., Zhu N., Fu X. et al. Growth and Mechanism of Network-Like Branched Si3N4 Nanostructures. Journal of the American Ceramic Society, 2010, vol. 93, no. 8, pp. 2264–2267.
  46. Zhu N., Peng Zh., Fu X. et al. A simple approach to controllably grow network-like branched single-crystalline Si3N4 nanostructures. Solid State Sciences, 2010, vol. 12, no. 7, pp. 1076–1079.
  47. Jiang Y.G., Zhang C.R., Cao F. et al. Effects of thermal load on mechanical properties and microstructures of 3D SiO2f/Si3N4–BN composites using polyborosilazane. Materials Science and Engineering: A, 2008, vol. 487, no. 1–2, pp. 597–600.
  48. Sasikumar P.V.W., Zera E., Graczyk-Zajac M. et al. Structural Design of Polymer-Derived SiOC Ceramic Aerogels for High-Rate Li Ion Storage Applications. Journal of the American Ceramic Society, 2016, vol. 99, no. 9, pp. 2977–2983.
  49. Vakifahmetoglu C., Zeydanli D., de Mello Innocentini M.D., dos Santos Ribeiro F., Lasso P.R.O., Soraru G.D. Gradient-hierarchic-aligned porosity SiOC ceramics. Scientific Reports, 2017, vol. 7. Publ. 41049.
  50. Colombo P., Arcaro A., Francesconi A. et al. Effect of hypervelocity impact on microcellular ceramic foams from a preceramic polymer. Advanced Engineering Materials, 2003, vol. 5, no. 11, pp. 802–805.
  51. Iwamoto Y., Völger W., Kroke E. et al. Crystallization Behavior of Amorphous Silicon Carbonitride Ceramics Derived from Organometallic Precursors. Journal of the American Ceramic Society, 2001, vol. 84, no. 10, pp. 2170–2178.
  52. Mera G., Riedel R., Poli F., Müller K. Carbon-rich SiCN ceramics derived from phenyl-containing poly(silylcarbodiimides). Journal of the European Ceramic Society, 2009, vol. 29, no. 13, pp. 2873–2883.
  53. Nangrejo M.R., Bao X., Edirisinghe M.J. Preparation of silicon carbide-silicon nitride composite foams from pre-ceramic polymers. Journal of the European Ceramic Society, 2000, vol. 20, no. 11, pp. 1777–1785.
  54. Degenhardt U., Stegner F., Liebscher C. et al. Sintered silicon nitride/nano-silicon carbide materials based on preceramic polymers and ceramic powder. Journal of the European Ceramic Society, 2012, vol. 32, no. 9, pp. 1893–1899.
  55. Graczyk-Zajac M., Fasel C., Riedel R. Polymer-derived-SiCN ceramic/graphite composite as anode material with enhanced rate capability for lithium ion batteries. Journal of Power Sources, 2011, vol. 196, no. 15, pp. 6412–6418.
  56. Bernardo E., Colombo P., Pippel E., Woltersdorf J. Novel Mullite Synthesis Based on Alumina Nanoparticles and a Preceramic Polymer. Journal of the American Ceramic Society, 2006, vol. 89, no. 5, pp. 1577–1583.
  57. Griggio F., Bernardo E., Colombo P., Messing G.L. Kinetic Studies of Mullite Synthesis from Alumina Nanoparticles and a Preceramic Polymer. Journal of the American Ceramic Society, 2008, vol. 91, no. 8, pp. 2529–2533.
  58. Bernardo E., Colombo P., Hampshire S. SiAlON-Based Ceramics from Filled Preceramic Polymers. Journal of the American Ceramic Society, 2006, vol. 89, no. 12, pp. 3839–3842.
  59. Schlier L., Fu Z., Harris J. et al. Crack healing of ferrosilicochromium-filled polymer-derived ceramic composites. Journal of the European Ceramic Society, 2018, vol. 38, no. 6, pp. 2495–2501.
  60. Riedel R., Passing G., Schönfelder H., Brook R.J. Synthesis of dense silicon-based ceramics at low temperatures. Nature, 1992, vol. 355, pp. 714–717.
  61. Kleebe H.-J., Störmer H., Trassl S., Ziegler G. Thermal stability of SiCN ceramics studied by spectroscopy and electron microscopy. Applied Organometallic Chemistry, 2001, vol. 15, no. 10, pp. 858–866.
  62. Mera G., Tamayo A., Nguyen H., Sen S., Riedel R. Nanodomain Structure of Carbon-Rich Silicon Carbonitride Polymer-Derived Ceramics. Journal of the American Ceramic Society, 2010, vol. 93, no. 4, pp. 1169–1175.