Investigation of hot isostatic pressing and heat treatment effect on structure and mechanical properties of 3D-printed samples made from VT6-PS grade material

Vasilev A.I., Panin P.V., Putyrskiy S.V., Rogalev A.M.
Vasilev A.I., Panin P.V., Putyrskiy S.V., Rogalev A.M. Investigation of hot isostatic pressing and heat treatment effect on structure and mechanical properties of 3D-printed samples made from VT6-PS grade material // Proceedings of VIAM. 2021. No. 7. DOI: 10.18577/2307-6046-2021-0-7-22-30. URL: https://viam-works.ru/en/journal/2021/7/3
Keywords
selective laser melting, additive manufacturing, hot isostatic pressing (HIP), vacuum annealing, tensile mechanical properties, microstructure.
Abstract

Presents the results of the investigation of the influence of hot isostatic pressing and heat treatment on the structure and mechanical properties during tension of synthesized workpieces obtained by selective laser alloying from a metal-powder composition of VT6 alloy. The blanks were subjected to heat treatment at various temperatures in the state after synthesis, as well after HIP. The influence of different heat treatment modes was assessed by the results of tensile tests and structural researches.

Reference list
  1. Onishchenko G.G., Kablov E.N., Ivanov V.V. Scientific and technological development of Russia in the context of achieving national goals: problems and solutions. Innovatsii, 2020, no. 6 (260), pp. 3–16.
  2. Kablov E.N. What to make the future of? New generation materials, technologies for their creation and processing - the basis of innovations. Krylya Rodiny, 2016, no. 5, pp. 8–18.
  3. Gu D.D., Meiners W., Wissenbach K., Poprawe R. Laser additive manufacturing of metallic components: Materials, processes and mechanisms. International Materials Reviews, 2012, no. 57 (3), pp. 133–164.
  4. Graf B., Gook SE, Gumenyuk AV, Retmayer M. Combined laser additive technologies for the production of turbine blades of complex geometric shape. Globalnaya yadernaya bezopasnost, 2016, no. 3 (20), pp. 34–42.
  5. Garibov G.S. Metallurgy of granules – the basis for creating new materials for advanced aircraft engines. Permskie aviatsionnye dvigateli, 2012, no. 26, pp. 58–63.
  6. Shishkovsky I.V. Fundamentals of High Resolution Additive Technologies. Saint Petersburg: Peter, 2016, 400 p.
  7. Zlenko M.A., Popovich A.A., Mutylina I.N. Additive technologies in mechanical engineering. Saint Petersburg: Publishing house of Polytech University, 2013, 210 p.
  8. Sufiyarov V.Sh., Popovich A.A., Borisov E.V., Polozov I.A. Selective laser melting of heat-resistant nickel alloy. Tsvetnye metally, 2015, no. 1, pp. 79–84.
  9. Evgenov A.G., Rogalev A.M., Nerush S.V., Mazalov I.S. A study of properties of EP648 alloy manufactured by the selective laser sintering of metal powders. Trudy VIAM, 2015, no. 2, paper no. 02. Available at: http://www.viam-works.ru (accessed: May 12, 2021). DOI: 10.18577/2307-6046-2015-0-2-2-2.
  10. Inozemtsev A.A., Bashkatov I.G., Koryakovtsev A.S. Titanium alloys in products developed by Aviadvigatel OJSC. Sovremennyye titanovyye splavy i problemy ikh razvitiya. Moscow: VIAM, 2010, pp. 43–46.
  11. Dudikhin D.V., Saprykin A.A. Methods for producing spherical powders for additive laser technologies. Masters Journal, 2016, no. 1, pp. 51–55.
  12. Dzunovich D.A., Lukina E.A., Yakovlev A.L. Influence of heat treatment parameters on producibility and mechanical properties of sheets made from high-strength titanium alloy VT23. Aviacionnye materialy i tehnologii, 2018, no. 3 (52), pp. 3–10. DOI: 10.18577/2071-9140-2018-0-3-3-10.
  13. Kablov E.N. Present and future of additive technologies. Metally Evrazii, 2017, no. 1, pp. 2–6.
  14. Gelchinsky B.R., Merkushev A.G., Dolmatov A.V. Application of protective coatings by plasma spraying on VT6 alloy products obtained by selective laser fusion. IV International Conference "Additive Technologies: Present and Future". Moscow, 2018, pp. 18–28.
  15. Vasilev A.I, Putyrskiy S.V., Korotchenko A.Yu., Anisimova A.Yu. MIM technology as a method of manufacturing precision parts from metal-powder compositions, including titanium alloys (review). Trudy VIAM, 2021, no. 3 (97), paper no. 02. Available at: http://www.viam-works.ru (accessed: May 12, 2021). DOI: 10.18577/2307-6046-2021-0-3-16-27.
  16. Peskova A.V., Sukhov D.I., Mazalov P.B. Exami-nation of the formation of the titanium alloy VT6 structure obtained by additive manufacturing. Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 38–44. DOI: 10.18577/2071-9140-2020-0-1-38-44.
  17. Ahlfors M., Bahbou F., Eklund A. HIP for AM – Optimized Material Properties by HIP. Proceedings of 12th International Conference on Hot Isostatic Pressing. Sydney, 2017, pp. 1–10.
  18. Yamomoto Y., Fujikawa T. Mechanical Properties of Ti – 6Al – 4V Materials Prepared by Additive Manufacturing. Technology and HIP Process. Proceedings of 11th International Conference on Hot Isostatic Pressing. Stockholm, 2014, pp. 398–404.
  19. Hjärne J., Ahlfors M. Hot Isostatic Pressing for AM parts. Quintus Technologies. Västerås, 2016, pp. –5.
  20. Lukina E.A., Filonova E.V., Treninkov I.A. The microstructure and preferential crystallographic orientation of nickel superalloy, synthesized by SLM method, depending of the energy impact and heat treatment. Aviacionnye materialy i tehnologii, 2017, no. 1 (46), pp. 38–44. DOI: 10.18577/2071-9140-2017-0-1-38-44.