Influence of technological parameters on characteristics of polymer composite materials in automated layup of prepregs (review)

Timoshkov P.N., Goncharov V.A., Usacheva M.N., Khrulkov A.V.
Timoshkov P.N., Goncharov V.A., Usacheva M.N., Khrulkov A.V. Influence of technological parameters on characteristics of polymer composite materials in automated layup of prepregs (review) // Proceedings of VIAM. 2021. No. 6. DOI: 10.18577/2307-6046-2021-0-6-46-55. URL: https://viam-works.ru/en/journal/2021/6/5
Keywords
technological parameters, automated layout, prepreg, polymer composite materials, defects, automated tape laying (ATL), automated fiber placement (AFP).
Abstract

The main technological factors when using ATL and AFP technologies are material temperature, laying speed, rolling pressure and no deviation from the required laying trajectory. The article discusses the influence of technological factors on some characteristics of polymer composite materials. The optimum laying temperature should provide the required adhesion. The rate of laying should provide heating of the material without its technological properties. The rolling pressure during laying should ensure optimal porosity and thickness of the material.

Reference list
  1. Dorey G. Carbon fibres and their applications. Journal of Physics D: Applied Physics, 1987, vol. 20, pp. 245–256.
  2. Grant C. Automated processes for composite aircraft structure. Industrial Robot, 2006, vol. 33(2), pp. 117–121.
  3. Composite tape laying machine with pivoting presser member: pat. US 4627886A; filed 06.04.71; publ. 09.12.86.
  4. Geodesic path length compensator for composite-tape placement method: pat. US 3810805A; filed 14.04.72; publ. 14.05.74.
  5. Timoshkov P.N. Equipment and materials for the technology of automated calculations prepregs. Aviacionnye materialy i tehnologii, 2016, no. 2, pp. 35–39. DOI: 10.18577/2071-9140-2016-0-2-35-39.
  6. Lossie M., van Brussel H. Design principles in filament winding. Composites Manufacturing, 1994, vol. 5 (1), pp. 5–13.
  7. Huber J. Automated lamination of production advanced composite aircraft structures. SAE International Congress and Exposition, 1981, vol. 90, pp. 1794–1803.
  8. Lukaszewicz D.H.J.A., Ward C., Potter K.D. The engineering aspects of automated prepreg layup: History, present and future. Composites. Part B: Engineering. 2012, vol. 43 (3), pp. 997–1009.
  9. Introduction to composite materials and smart structures. Structural health monitoring of composite structures using fiber optic methods. Ed. B.G. Prusty, G. Rajan. New York: CRC Press, 2016, 491 p.
  10. Mazumdar S.K. Composites manufacturing: materials, product, and process engineering. United States of America: CRC Press LLC, 2002. 416 p.
  11. Timoshkov P.N., Usacheva M.N., Khrulkov A.V. Stickiness and possibility of using prepregs for automated technologies (review). Trudy VIAM, 2018, no. 8 (68), paper no. 04. Available at: http://www.viam-works.ru (accessed: February 12, 2021). DOI: 10.18577/2307-6046-2018-0-8-38-46.
  12. Orlov E.V., Gusev Yu.A., Khrulkov A.V., Korotkov I.A. Comparative analysis of stickiness determination methods of prepreg. Trudy VIAM, 2016, no. 7, paper no. 09. Available at: http://www.viam-works.ru (accessed: February 12, 2021). DOI: 10.18577/2307-6046-2016-0-7-9-9.
  13. Béland S. High performance thermoplastic resins and their composites. Noyes Data Corp, 1990, 181 p.
  14. August Z., Ostrander G., Michasiow J., Hauber D. Recent development in automated fibre placement of Thermoplastic composites. SAMPE, 2014, vol. 50 (2), pp. 30–37.
  15. Stokes-Griffin C.M., Compston P. Laser-assisted tape placement of thermoplastic composites: The effect of process parameters on bond strength. Sustainable Automotive Technologies 2013. New York: Springer, 2014, pp. 295.
  16. Stokes-Griffin C.M., Compston P. The effect of processing temperature and placement rate on the short beam strength of carbon fibre–PEEK manufactured using a laser tape placement process. Composites. Part A: Applied Science and Manufacturing, 2015, vol. 78, pp. 274–283.
  17. Chauncey Wu K., Stewart B.K., Martin R.A. ISAAC – A Testbed for Advanced Composites Research. The Second International Symposium on Automated Composites Manufacturing, 2015, pp. 1–10.
  18. Kablov E.N. New Generation Materials and Technologies for Their Digital Processing. Herald of the Russian Academy of Sciences, 2020, vol. 90, no. 2, pp. 225–228.
  19. Kablov E.N., Chursova L.V., Lukina N.F., Kutsevich K.E., Rubtsova E.V., Petrova A.P. A Study of Epoxide–Polysulfone Polymer Systems for High-Strength Adhesives of Aviation Purpose. Polymer Science, series D, 2017, vol. 10, no. 3, pp. 225–229.
  20. Kablov E.N., Shuldeshov E.M., Petrova A.P., Lapteva M.A., Sorokin A.E. Dependence of complex of sound-proof VZMK type material properties on concen-tration of hydrophobizing composition on the basis of organosilicon sealant. Aviacionnye materialy i tehnologii, 2020, no. 2 (59), pp. 41–49. DOI: 10.18577/2071-9140-2020-0-2-41-49.
  21. Tkachuk A.I., Donetsky K.I., Terekhov I.V., Karavaev R.Yu. The use of thermosetting matrices for the manufacture of polymer composite materials by the non-autoclave molding methods. Aviation materials and technologies, 2021, no. 1 (62), paper no. 3. Available at: http://www.journal.viam.ru (accessed: February 19, 2021). DOI: 10.18577/2713-0193-2021-0-1-22-33.
  22. Goncharov V.A., Usacheva M.N., Khrulkov A.V. Features of the structure and reinforcement transmission shafts made of polymer composite materials (review). Trudy VIAM, 2021, no. 1 (95), paper no. 9. Available at: http://www.viam-works.ru (accessed: March 1, 2021). DOI: 10.18577/2307-6046-2021-0-1-85-96.
  23. Timoshkov P.N., Hrulkov A.V., Grigoreva L.N. Сarbon fiber transmission shaft. Materials and technology (review). Trudy VIAM, 2020, no. 8 (90), paper no. 05. Available at: http://www.viam-works.ru (accessed: March 1, 2020). DOI: 10.18577/2307-6046-2020-0-8-46-53.
  24. Di Francesco M., Giddings P., Potter K. On the layup of convex corners using Automated Fibre Placement: an evaluation method. The Second International Symposium on Automated Composites Manufacturing, 2015, pp. 1–10.
  25. Woigka W., Halletta S.R., Jonesa M.I. et al. Experimental investigation of the effect of defects in Automated Fibre Placement produced composite laminates. Composite Structures. 2018, vol. 201, pp. 1004–1017.
  26. Croft K., Lessard L., Pasini D. et al. Experimental study of the effect of automated fiber placement induced defects on performance of composite laminates. Composites, part A: Applied Science and Manufacturing. 2011, vol. 42, is. 5, pp. 484–491.
  27. Pitchumani R., Gillespie Jr.J.W., Lamontia M.A. Design and optimization of a thermoplastic tow-placement process with in-situ consolidation. Journal of Composite Materials, 1997, vol. 31, is. 3, pp. 244–275.
  28. Qureshi Z., Swait T., Scaife R., El-Dessouky H.M. In situ consolidation of thermoplastic prepreg tape using automated tape placement technology: potential and possibilities. Composites. Part B: Engineering, 2014, vol. 66, pp. 255–267.
  29. Bendemra H., Vincent M.J., Compston P. Optimisation of compaction force for automated fibre placement. 8th Australasian Congress on Applied Mechanics (ACAM 8). Melbourne: Engineers Australia, 2014, pp. 957–965.
  30. Senthil K., Arockiarajan A., Palaninathan R. et al. Defects in composite structures: Its effects and prediction methods – a comprehensive review. Composite Structures. 2013, vol. 106, pp. 139–149.
  31. Bolotin V.V. Delaminations in composite structures: Its origin, buckling, growth and stability. Composites, Part B: Engineering, 1996, vol. 27, is. 2, pp. 129–145.
  32. Nixon-Pearson O.J., Belnoue J.P.-H., Ivanov D.S., Hallett S.R. The compaction behavior of un-cured prepregs. The 20th International Conference on Composite Materials. Copenhagen, 2015. Available at: https://www.researchgate.net/publication/303880867_THE_COMPACTION_BEHAVIOUR_ OF_UN-CURED_PREPREGS (accessed: March 29, 2021).
  33. Sun H., Godin D., Dong A. et al. Effect of Process Parameters on the Quality of Laminates made by Automated Fiber Placement (AFP) Using Out-Ofautoclave (OOA) Prepregs. 17th European Conference on Composite Materials, 2016. pp. 1–12.
  34. Khan M.A., Mitschang P., Schledjewski R. Identification of some optimal parameters to achieve higher laminate quality through tape placement process. Advances in Polymer Technology, 2010, vol. 29, is. 2, pp. 98–111.
  35. Çelik O., Peeters D., Dransfeld S., Teuwen J. Intimate contact development in laser assisted fiber placement. Microstructure and effect of process parameters. Composites, Part A: Applied Science and Manufacturing, 2020, vol. 134, pp. 1–13.
  36. Ivanov D., Li Y., Ward C., Potter K. Transitional behaviour of prepregs in Automated fibre deposition processes. The 19th International Conference on Composite Materials, 2013, pp. 1–11.
  37. Ilcewicz L.B., Murphy B. Safety & Certification Initiatives for Composite Airframe Structure. 46th AIAA/ASME/ASCE/AHS/ASC Structures, Structural Dynamics & Materials Conference, 2005, pp. 1–12.
  38. Chauncey Wu K. Design and Analysis of Tow-Steered Composite Shells Using Fiber Placement. American Society for Composites 23rd Technical Conference, 2008. Available at: https://www.researchgate.net/publication/273144777_Design_and_Analysis_of_Tow-Steered_Composite_Shells_Using_Fiber_Placement (accessed: March 30, 2021).
  39. Measom R., Sewell K. Fiber placement low-cost production for complex composite structures. Proceedings. American Helicopter Society International Annual Forum. Washington, 1996, vol. 52, is. 1, pp. 611–622.
  40. Wu K., Tatting B., Smith B. et al. Design and Manufacturing of Tow-Steered Composite Shells Using Fiber Placement. 50th AIAA/ASME/ASCE/AHS/ASC Structures, Structural Dynamics, and Materials Conference. Boston, 2009, pp. 1–18.
  41. Tatting B.F., Gürdal Z. Automated finite element analysis of elastically-tailored plates. NASA Scientfic and Technical Information, 2003, pp. 1–47.
  42. Kim B.C., Hazra K., Weaver P., Potter K. Limitations of fibre placement techniques for variable angle tow composites and their process-induced defects. 18th International Conference on Composite Materials, 2011. Available at: https://www.researchgate.net/publication/259267107_Limitations_ of_fibre_placement_techniques_for_variable_angle_tow_composites_and_their_process-induced_defects (accessed: March 30, 2021).
  43. Oromiehie E., Prusty B.G., Compston P., Rajan G. Automated fibre placement based composite structures: Review on the defects, impacts and inspections techniques. Composite Structures, 2019, vol. 224, pp. 1–14.
  44. Langley P. Finite element modeling of tow-placed variable-stiffness composite laminates. Virginia Polytechnic Institute and State University, 1999, 127 p.