Influence of non-oxid additives on the properties of glass-ceramic coating for parts made of heat-resistant alloys (review)

Malinina G.A., Solntsev St.S., Denisova V.S.
Malinina G.A., Solntsev St.S., Denisova V.S. Influence of non-oxid additives on the properties of glass-ceramic coating for parts made of heat-resistant alloys (review) // Proceedings of VIAM. 2021. No. 3. DOI: 10.18577/2307-6046-2021-0-3-109-117. URL: https://viam-works.ru/en/journal/2021/3/10
Keywords
glass-ceramic coatings, modifying additives, boride, silicide, lanthanum, heat resistance, formation of the coating.
Abstract

A review of the scientific and technical literature is presented, which provides examples of improving glass-based coatings by introducing non-oxide modifying additives. The main groups of chemical compounds that are used to improve the properties of glass-ceramic coatings are considered. Such substances include compounds based on boron, silicon and rare earth metals. It is concluded that these additives have a positive effect on the following properties of coatings: heat resistance, heat resistance, mechanical strength, coating formation temperature, temperature coefficient of linear expansion and adhesion strength to the protected material.

Reference list
  1. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Ospennikova O.G., Podieiachev V.N., Stoliankov Yu.V. Refractory alloys for innovative equipment. Trudy VIAM, 2016, no. 10, paper no. 5. Available at: http://www.viam-works.ru (accessed: November 18, 2020). DOI: 10.18577/2307-6046-2016-0-10-5-5.
  3. Kablov E.N., Solntsev S.S., Rosenenkova V.A., Mironova N.A. Modern polyfunctional high-temperature coatings for nickel alloys, sealing metal materials and beryllium alloys. Novosti materialovedeniya. Nauka i tekhnika, 2013, no. 1, paper no. 05. Available at: http://www.materialsnews.ru (date accessed: November 23, 2020).
  4. Grashchenkov D.V. Strategy of development of non-metallic materials, metal composite materials and heat-shielding. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 264–271. DOI: 10.18577/2071-9140-2017-0-S-264-271.
  5. Kablov E.N., Grashchenkov D.V., Isaeva N.V., Solntsev S.S. Promising high-temperature ceramic composite materials. Rossiyskiy khimicheskiy zhurnal, 2010., vol. LIV, no. 1, pp. 20–24.
  6. Kablov E.N., Grashchenkov D.V., Isaeva N.V., Solntsev S.S., Sevastianov V.G. High-temperature structural composite materials based on glass and ceramics for advanced aircraft products. Steklo i keramika, 2012, no. 4, pp. 7–11.
  7. Zhitnyuk S.V. Oxygen-free ceramic mate-rials for the space technics (review). Trudy VIAM, 2018, no. 8 (68), paper no. 08. Available at: http://www.viam-works.ru (accessed: November 11, 2020). DOI: 10.18577/2307-6046-2018-0-8-81-88.
  8. Wang G., Jiang W., Bai G., Wu Li. Effect of Addition of Oxides on Low-Temperature Oxidation of Molybdenum Disilicide. Journal of American Ceramic Society, 2003, vol. 86, no. 4, pp. 731–734.
  9. Titov D.D., Kargin Yu.F., Popov N.A., Lysenkov A.S. New composite materials based on molybdenum disilicide. Perspektivnye materialy, 2011, no. S13, pp. 493–499.
  10. Han X., Wang Y.-L., Xiong X., Li H. Microstructure, sintering behavior and mechanical properties of SiC / MoSi2 composites by spark plasma sintering. Transaction of Nonferrous Metals Sosiety of Chaina, 2018, no. 28, pp. 957–965. DOI: 10.1016/S1003-6326 (18) 64730-2.
  11. Gnesin I.B. Experimental study of the structure and properties of solid solutions of molybdenum and tungsten silicides and their application: thesis, Cand. Sc. (Tech.). Chernogolovka: Institute of Solid State Physics RAS, 2005, 24 p.
  12. Gnesin I.B., Gnesin B.A., Nekrasov A.N. Investigation of the effect of carbon impurity on microhardness, chemical and phase compositions of double silicide eutectics Me5Si3–MeSi2 of the Mo–W–Si system on cast samples. Materialovedenie, 2008, no. 8, pp. 21–35.
  13. Armor for «Buran». Materials and technologies of VIAM for the ISS «Energiya–Buran». Ed. E.N. Kablov. Moscow: Nauka i zhizn, 2013, 128 p.
  14. Kablov E.N. Materials for «Buran» spaceship – innovative solutions of formation of the sixth technological mode. Aviacionnye materialy i tehnologii, 2013, no. S1, pp. 3–9.
  15. Kablov E.N., Solntsev S.S. Oxythermosynthesis – a new step towards materials for advanced aerospace technology. Aviation materials. Selected works of VIAM 1932–2002. Moscow: VIAM, 2002, pp. 131–137.
  16. Goldstein H.E., Leiser D.B., Katvala V. Reaction cured borosilicate glass coating for low density fibrous silica insulation. Borate Glasses. Materials science research: plenum press. New York; London, 1978, vol. 12, pp. 623–634.
  17. Goldstein N.V. et al. Reaction cured borosilicate glass coating for low-density fibrous insulation. Borate glasses. Structure, properties, application: plenum press. New York, 1978, pp. 623–634.
  18. Garofalini S.H., Banas R., Creedon J. Development of high viscosity coatings for advances Space Shuttle application. 11th National SAMPE technical conference. Boston, 1979, pp. 114–124.
  19. Stratiychuk D.A. Impregnation of amorphous boron with silicon melt under conditions of high pressures and temperatures. Dopovidi Nacionalnoi akademii nauk Ukraini, 2011, no. 3, pp. 94–99.
  20. Matsushita J., Komarneni S. High temperature oxidation of silicon hexaboride ceramics. Materials Research Bulletin, 2001, vol. 36, no. 5-6, pp. 1083–1089.
  21. Tong Ch., Cheng L., Yin X. et al. Oxidation behavior of 2D C/SiC composite modified by SiB4 particles in inter-bundle pores. Composites Science and Technology, 2008, vol. 68, pp. 602–607.
  22. Pryamilova E.N., Lyamin Yu.B. Ultra-high-temperature ceramics based on borides. Collection of materials of the V Internat. conf. with elements of scientific schools for young people «Functional nanomaterials and high-purity substances». Suzdal, 2014, pp. 447–448.
  23. Pryamilova E.N., Poilov V.Z., Lyamin Yu.B. Thermochemical stability of ceramics based on zirconium and hafnium borides. Vestnik Permskogo natsionalnogo issledovatelskogo politekhnicheskogo universiteta, 2014, no. 4, pp. 55–67.
  24. Mazilin I.V., Baldaev L.Kh., Drobot D.V., Akhmetgareeva A.M., Zhukov A.O., Khismatullin A.G. Thermal and thermophysical properties of heat-protective coatings based on lanthanum zirconate. Perspektivnye materialy, 2013, no. 7, pp. 21–30.
  25. Merkushkin A.O., Zaw Ye Maw Oo. Obtaining and properties of ceramics from lanthanum and gadolinium aluminates. Scientific Researches and Their Practical Application, 2012, vol. 32, no. 3, pp. 8–9.
  26. Stefanovskiy S.V., Stefanovskaya O.I., Semenova D.V. Phase composition and structure of sodium-aluminum phosphate-based glass materials containing oxides of rare-earth elements. Radioaktivnye otkhody, 2018, no. 1 (2), pp. 97–101.
  27. Galasso F.S. Structure, properties and preparation of perovskite-type compounds. Oxford: Pergamon Press, 1969, 209 p.
  28. Vitkalova I.A., Torlova A.S., Pikalov E.S. Influence of lanthanum oxide on the properties of chemically resistant ceramics obtained using galvanic sludge. Mezhdunarodnyy nauchno-issledovatelskiy zhurnal, ser.: Technical sciences, 2019, no. 10, pp. 35–39. DOI: 10.23670/IRJ.2019/88/10/006.
  29. Dudkin B.N., Bugaeva A.Yu., Zainullin G.G. Features of sintering xerogel of the composition «lanthanum hexaaluminate – yttrium oxide» obtained by the sol-gel method. Izvestiya Komi nauchnogo tsentra UrO RAN, 2011, no. 2, pp. 19–24.
  30. Pyachin A.S., Ershova T.B., Burkov A.A., Vlasova N.M., Komarova V.S. The use of titanium aluminides for the creation of electrospark coatings. Poroshkovaya metallurgiya i funktsional'nyye pokrytiya. Izvestiya vuzov, 2015, no. 1, pp. 55–61.
  31. Karashaev M.M., Lomberg B.S., Bakradze M.M., Letnikov M.N. On technological approaches to the creation of composite materials based on nickel monoaluminide NiAl (review). Trudy VIAM, 2019, no. 12 (84), paper no. 07. Available at: http://www.viam-works.ru (accessed: December 18, 2020). DOI: 10.18577/2307-6046-2019-0-12-55-66.
  32. Bankovskaya N.V. Creation of a new generation of high-temperature glass-ceramic compositions and study of their physical and chemical properties: thesis, Dr. Sc. (Chem.). Saint Petersburg: Order of the Red Banner of Labor Institute of silicates named after I.V. Grebenshchikov Russian Academy of Sciences, 2006, 297 p.
  33. Vasenev V.V. Development of composite materials based on Al–Si–Ni systems with low thermal expansion coefficient and technology for producing semi-finished products for rocket and space technology: thesis, Cand. Sc. (Tech.). Moscow: Moscow Institute of Aviation Materials, 2017, 135 p.