Promising methods for production of electrochromic devices based on nanostructured coatings (review)

Schur P.A., Solovyanchik L.V., Kondrashov S.V.
Schur P.A., Solovyanchik L.V., Kondrashov S.V. Promising methods for production of electrochromic devices based on nanostructured coatings (review) // Proceedings of VIAM. 2021. No. 3. DOI: 10.18577/2307-6046-2021-0-3-99-108. URL: https://viam-works.ru/en/journal/2021/3/9
Keywords
electrochromic devices, electrochromic materials, electrochromic glazing, nanostructured coatings, smart glass, functional glazing.
Abstract

Paper presents the most common materials for nanostructured inorganic electrochromic coatings, describes the methods of their formation. The prospects for the use of electrochromic materials in various industries – construction, auto and aircraft construction are considered. The analysis of modern methods for the formation of nanostructured electrochromic materials used in various fields of science and technology is presented. The prospects for the use of tungsten oxide, as well as the possibility of its modification in order to improve its functional electrochromic properties, are shown.

Reference list
  1. Koktsinskaya E.M. «Smart» materials and their application (review). Videonauka, 2016, no. 1 (1), pp. 13.
  2. Schwartz M. Encydopedia of smart materials. New York: John Wiley and Sons Inc., 2002, 1193 c.
  3. Kablov E.N. New generation materials – the basis of innovation, technological leadership and national security of Russia. Intellekt i tekhnologii, 2016, no. 2 (14), pp. 16–21.
  4. Kablov E.N. What to make the future of? New generation materials, technologies for their creation and processing – the basis of innovations. Krylya Rodiny, 2016, no. 5, pp. 8–18.
  5. Kablov E.N., Semenova L.V., Bogatov V.A., Mekalina I.V. and other New electrically heated and bird-resistant polymer glazing of aircraft. Plasticheskiye massy, 2017, no. 5-6, pp. 48–52.
  6. Kondrashov S.V., Shashkeev K.A., Petrova G.N., Mekalina I.V. Constructional polymer composites with functional properties. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 405–419. DOI: 10.18577/2071-9140-2017-0-S-405-419.
  7. Kobasnyan S.S., Anisimov I.A. Intelligent system for regulating the level of light transmission of car glasses. Zhurnal mekhaniki XXI veka, 2012, no. 11, pp. 298–299.
  8. Kotok V., Kovalenko V., Solovov V., Yurlova O. The determination of electrolyte stability and conditions for electrochromic WO3 films deposition. Technology audit and production reserves, 2017, vol. 3, no. 3 (35), pp. 17–22.
  9. Kotok V., Kovalenko V. The electrochemical cathodic template synthesis of nickel hydroxide thin films for electrochromic devices: role of temperature. Eastern-European Journal of Enterprise Technologies, 2017, no. 2 (11), pp. 28–34.
  10. Somani P.R., Radhakrishnan S. Electrochromic materials and devices: present and future. Materials chemistry and physics, 2003, vol. 77, no. 1, pp. 117–133.
  11. Mortimer R. J. Electrochromic materials. Chemical Society Reviews, 1997, vol. 26, no. 3, pp. 147-156.
  12. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  13. Exarkhos G.J., Zhou X.-D. Discovery-based. Design of Transparent Conducting Oxide Films. Thin Solid Films, 2007, vol. 7025, pp. 515–521.
  14. Song X., Dong G., Xiao Y. et al. Properties of NiOx and its influence upon all-thin-film ITO/NiOx/ LiTaO3/WO3/ITO electrochromic devices prepared by magnetron sputtering. Vacuum, 2015, vol. 111, pp. 48–54.
  15. Mortimer R. J. Electrochromic materials. Annual Review of Materials Research, 2011, vol. 41, pp. 241–268.
  16. Prokopovich P.V., Kirillova E.S. Prospects for the use of a cellulose matrix as a solid polymer electrolyte for photo- and electrochromic devices. Trudy Kolskogo nauchnogo tsentra RAN, 2018, vol. 9, no. 2-2, pp. 1–6.
  17. Bogatov V.A., Krynin A.G., Popkov O.V., Khokhlov Yu.A. Influence of biaxial strain on the properties of the transparent conductive coating deposited on PET film by reactive magnetron sputtering. Trudy VIAM, 2016, no. 1 (37), paper no. 6. Available at: http://www.viam-works.ru (accessed: December 17, 2020). DOI: 10.18577/2307-6046-2016-0-1-42-49.
  18. Gorjanca T.C., Leonga D., Py C., Rotha D. Room temperature deposition of ITO using r.f. magnetron sputtering. Thin Solid Films, 2002, vol. 413, pp. 181–185.
  19. Bogatov V.A., Krynin A.G., Shchur P.A. Influence of the leakage value in the vacuum chamber on the parameters of reactive magnetron discharge and properties of titanium oxide coatings. Aviacionnye materialy i tehnologii, 2019, no. 1 (54), pp. 17–22. DOI: 10.18577/2071-9140-2019-0-1-17-22.
  20. Kuzmichev A.I. Magnetron sputtering systems. Introduction to physics and technology of magnetron sputtering. Kiev: Avers, 2008, 244 p.
  21. Elinson V.M., Shchur P.A., Lyamin A.N. Nanostructuring of the Polyethyleneterephthalate Surface Using Ion-Plasma Technology with the Help of Fluorine-Containing Gas Mixtures. High Temperature Material Processes: An International Quarterly of High-Technology Plasma Processes, 2020, vol. 24, no. 3, pp. 173–182. DOI: 10.1615/HighTempMatProc.2020035843.
  22. Melnikov A.A., Shchur P.A. Transparent conductive antireflective coatings based on ITO, SiO2, TiO2. Trudy VIAM, 2019, No. 8 (80), paper no. 07. Available at: http://www.viam-works.ru (accessed: December 13, 2020). DOI: 10.18577 / 2307-6046-2019-0-8-56-66.
  23. Rougier A. Nickel oxide based electrochromic materials. Materiaux pour l'énergie. Amiens, 2009, pp. 26–30.
  24. Belousov A.L., Patrusheva T.N. Electrochromic oxide materials. Journal of the Siberian Federal University. Technics and techology, 2014, vol. 7, no. 6, pp. 698–709.
  25. Wang J., Khoo E., Lee P.S., Ma J. Synthesis, assembly, and electrochromic properties of uniform crystalline WO3 nanorods. The Journal of Physical Chemistry C, 2008, vol. 112, no. 37, pp. 14306–14312.
  26. Granqvist C.G. Electrochromic tungsten oxide films: review of progress 1993–1998. Solar Energy Materials and Solar Cells, 2000, vol. 60, no. 3, pp. 201–262.
  27. Granqvist C.G. Handbook of Inorganic Electrochromic Materials, second impression. Elsevier, 2002, 650 p.
  28. Dinh N.N., Oanh N.Th.T., Long P.D. et al. Electrochromic properties of TiO2 anatase thin films prepared by a dipping sol-gel method. Thin Solid Films, 2003, vol. 423, no. 1, pp. 70–76.
  29. Ninh D.H., Thao T.T., Vo-Van T. Mixed nanostructured Ti–W oxides films for efficient electrochromic windows. Journal of Nanomaterials, 2012, vol. 2012, p. 7.
  30. Handbook of inorganic electrochromic materials. Ed. C.G. Granqvist. Elsevier, 1995, 651 p.
  31. Monk P.M.S., Mortimer R.J., Rosseinsky D.R. Electrochromism and electrochromic device. Cambridge: Cambridge University Press, 2007, 512 p.
  32. Porqueras I., Person C., Corbella C., Vives M. Characteristics of e-beam deposited electrochromic CeO2 thin films. Solid State Ionics, 2003, vol. 165, no. 1-4, pp. 131–137.
  33. Shchegolkov A.V., Chudov K.A. Obtaining thin, highly efficient electrochromic films based on nanostructured materials. Materials of All-Rus. Scientific Conf. “Technologies and materials for extreme conditions (predictive research and innovative development)”. Zvenigorod, 2018, pp. 66–70.
  34. Shchegolkov A.V., Tugolukov E.N., Shchegolkov A.V. Overview of Electrochromic Materials and Devices: Scope and Development Prospects. Advanced Materials and Technologies, 2020, no. 2, pp. 66–73.
  35. Vroon Z.A.E.P., Spee C.I.M.A. Sol-gel coatings on large area glass sheets for electrochromic devices. Journal of Non-Crystalline Solids, 1997, vol. 218, pp. 189–195.
  36. Yanovskaya M.I., Obvintseva I.E., Kessler V.G. et al. Hydrolysis of molybdenum and tungsten alkoxides: sols, powders and films. Journal of Non-Crystalline Solids, 1990, vol. 124, no. 2-3, pp. 155–166.
  37. Meda L., Breitkopf R.C., Haas T.E., Kirss R.U. Investigation of electrochromic properties of nanocrystalline tungsten oxide thin film. Thin Solid Films, 2002, vol. 402, no. 1-2, pp. 126–130.
  38. Richardson T.J., Rubin M.D. Liquid phase deposition of electrochromic thin films. Electrochimica Acta, 2001, vol. 46, no. 13-14, pp. 2119–2123.
  39. Nagayama H., Honda H., Kawahara H. A new process for silica coating. Electrochemical Society, 1988, vol. 135, pp. 2013–2016.
  40. Zöller A., Götzelmann R., Matl K., Cushing, D. Temperature-stable bandpass filters deposited with plasma ion-assisted deposition. Applied Optics, 1996, vol. 35, no. 28, pp. 5609–5612.
  41. Elinson V.M., Shchur P.A., Kirillov D.V. et al. Study of the Mechanical Characteristics of Single-Layer and Multilayer Nanostructures Based on Carbon and Fluorocarbon Coatings. Journal of Surface Investigation: X-ray, Synchrotron and Neutron Techniques, 2018, vol. 12, no. 2, pp. 357–360. DOI: 10.1134/S1027451018020246.
  42. Elinson V.M., Shchur P.A., Deshevaya E.A., Kravets L.I. Antimicrobial antiadhesive properties of nanostructured fluorocarbon films obtained under transient conditions using two-component gas mixtures. Journal of Physics: Conference Series, 2019, vol. 1313, art. no. 012016. DOI: 10.1088/1742-6596/1313/1/012016.
  43. Sleptsov V., Diteleva A. Thin-film technology for creating flexible supercapacitor electrodes based on a carbon matrix. High Temperature Material Processes: An International Quarterly of High-Technology Plasma Processes, 2020, vol. 24, no. 3, pp. 167–171
  44. Macrelli G., Poli E. An all solid state inorganic thin film electrochromic device: device fabrication optical and electrochromical characterization. The Electrochemical Society Proceeding Series, 1996, vol. 5, no. 96-24, p. 338.