Ultrasonic testing of spesimens at the development and testing process of new CFRP grades

Boychuk A.S., Dikov I.A., Generalov A.S., Chertishchev V.Yu.
Boychuk A.S., Dikov I.A., Generalov A.S., Chertishchev V.Yu. Ultrasonic testing of spesimens at the development and testing process of new CFRP grades // Proceedings of VIAM. 2021. No. 12. DOI: 10.18577/2307-6046-2021-0-12-86-95. URL: https://viam-works.ru/en/journal/2021/12/10
Keywords
carbon fiber reinforced plastics, flat panels, curved beam, nondestructive testing, ultrasonic testing, pulse-echo technique.
Abstract

Nondestructive testing results of carbon fiber reinforced plastics (CFRP) specimens at the development and testing process are given at that paper. Ultrasonic pulse-echo technique is the most applicable for CFRP monolithic panels and curved beam specimens testing. It is shown that ultrasonic testing allows optimizing the mode in the process of developing molding modes for new CFRP grades. At the test stages it allows to exclude defective specimens from the testing process and estimate the sorts and damage sizes after the tests.

Reference list
  1. Raskutin A.E. Russian polymer composite materials of new generation, their exploitation and implementation in advanced developed constructions. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 349–367. DOI: 10.18577/2071-9140-2017-0-S-349-367.
  2. Kablov E.N. What to make the future of? New generation materials, technologies for their creation and processing - the basis of innovation. Krylya Rodiny, 2016, no. 5, pp. 8–18.
  3. Kablov E.N. New generation materials – the basis of innovation, technological leadership and national security of Russia. Intellekt i tekhnologii, 2016, no. 2 (14), pp. 16–21.
  4. Kablov E.N. VIAM: new generation materials for PD-14. Krylya Rodiny, 2019, no. 7-8, pp. 54–58.
  5. Zhelezina G.F., Solovyeva N.A., Makrushin K.V., Rysin L.S. Polymer composite materials for manufacturing engine air particle separation of advanced helicopter engine. Aviacionnye materialy i tehnologii, 2018, no. 1 (50), pp. 58–63. DOI: 10.18577/2071-9140-2018-0-1-58-63.
  6. Timoshkov P.N. Equipment and materials for the technology of automated calculations prepregs. Aviacionnye materialy i tehnologii, 2016, no. 2, pp. 35–39. DOI: 10.18577/2071-9140-2016-0-2-35-39.
  7. Ivanov N.V., Gurevich Ya.M., Khaskov M.A., Akmeev A.R. Mode studying curing binding VSE-34 and its influences on mechanical properties. Aviacionnyye materialy i tehnologii, 2017, no. 2, pp. 50–55. DOI: 10.18577 / 2071-9140-2017-0-2-50-55.
  8. Kablov E.N. The strategic directions of development of materials and technologies of their processing for the period to 2030. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 7–17.
  9. Boychuk A.S., Generalov A.S., Dalin M.A., Dikov I.A. Inspection of monolithic parts and structures of aviation equipment made of PCM by ultrasonic non-destructive testing using phased arrays. Main trends, directions and prospects for the development of non-destructive testing methods in the aerospace industry: Collection of articles. Proceedings of the X All-Russia. conf. "TestMat". Moscow: VIAM, 2018, pp. 18–31. Available at: https://conf.viam.ru/sites/default/files/uploads/proceedings/1063.pdf (accessed: May 07, 2021).
  10. Papa I., Lopresto V., Langella A. Ultrasonic inspection of composites materials: Application to detect impact damage. International Journal of Lightweight Materials and Manufacture, 2021, vol. 4, is. 1, pp. 37–42. DOI: 10.1016/j.ijlmm.2020.04.002.
  11. Bossi R.H., Georgeson G.E. Nondestructive testing of aerospace composites. Polymer Composites in the Aerospace Industry, second edition, 2020, pp. 461–489. DOI: 10.1016/B978-0-08-102679-3.00016-2.
  12. Starikovsky G.P., Karabutov A.A., Kuryatin A.A. Non-destructive testing of integral structures made of polymer composite materials. V mire nerazrushayushchego kontrolya, 2011, no. 4, pp. 61–65.
  13. Non-destructive testing: reference book in 7 vols. Ed. V.V. Klyuev. Moscow: Mashinostroenie, 2004. Vol. 3: Ultrasonic control, 864 p.
  14. Kosarina E.I., Stepanov A.V. Radiographic control of honeycomb structures. V mire nerazrushayushchego kontrolya, 2003, no. 3, pp. 12–15.
  15. Boytsov B.V., Vasiliev S.L., Gromashev A.G. Non-destructive testing methods used for structures made of advanced composite materials. Trudy MAI, 2011, no. 49, pp. 63–74.
  16. Troitsky V.A., Karmanov M.N., Troitskaya N.V. Non-destructive quality control of composite materials. Tekhnicheskaya diagnostika i nerazrushayushchiy kontrol, 2014, no. 3, pp. 29–33.
  17. Dikov I.A., Boychuk A.S., Dalin M.A., Chertishchev V.Yu., Generalov A.S. Relationship between strength characteristics, porosity and ultrasonic control data for PCM samples obtained by autoclave and infusion technologies. Kontrol. Diagnostika, 2018, no. 11, pp. 40–51.
  18. Boychuk A.S. Development of technologies for non-destructive testing of monolithic structures made of carbon fiber using ultrasonic antenna arrays: thesis, Cand. Sc. (Tech.). Moscow, 2016, 203 p.