Prospects of the production of large-sized aircraft parts from polymer composite materials (review)

Goncharov V.A., Timoshkov P.N., Usacheva M.N.
Goncharov V.A., Timoshkov P.N., Usacheva M.N. Prospects of the production of large-sized aircraft parts from polymer composite materials (review) // Proceedings of VIAM. 2021. No. 12. DOI: 10.18577/2307-6046-2021-0-12-55-62. URL: https://viam-works.ru/en/journal/2021/12/7
Keywords
polymer composites materials, autoclave molding, vacuum infusion, aircraft wings, prepregs, resin, filler, automation.
Abstract

Today wings for Boeing 787 and Airbus A350 aircraft are made of polymer composite materials in the form of prepregs based on carbon fiber, the blanks of which are molded in an autoclave. It is expected that by 2025–2030 will actively use the vacuum infusion method, which will require global research on the selection of binding and reinforcing materials, development of the vacuum impregnation and curing process, automation and development of new technological methods for laying out workpieces of parts, accelerating the process and shortening the cycle time.

Reference list
  1. Putin noted the importance of holding MAKS-2021 online and offline. Available at: https://tass.ru/armiya-i-opk/11942899?utm_source=yxnews&utm_medium=desktop (accessed: August 20, 2021).
  2. Kablov E.N. New generation materials and digital technologies for their processing. Vestnik Rossiyskoy akademii nauk, 2020, vol. 90, no. 4, pp. 331–334.
  3. Kablov E.N. Formation of domestic space materials science. Vestnik RFFI, 2017, no. 3, pp. 97–105.
  4. Kablov E.N. VIAM: new generation materials for PD-14. Krylya Rodiny, 2019, no. 7-8, pp. 54–58.
  5. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  6. Tkachuk A.I., Donetsky K.I., Terekhov I.V., Karavaev R.Yu. The use of thermosetting matrices for the manufacture of polymer composite materials by the non-autoclave molding methods. Aviation materials and technology, 2021. no. 1 (62). paper no. 03. Available at: https://journal.viam.ru (accessed: August 19, 2021). DOI: 10.18577/2713-0193-2021-0-1-22-23.
  7. Goncharov V.A., Usacheva M.N., Khrulkov A.V. Features of the structure and reinforcement transmission shafts made of polymer composite materials (review). Trudy VIAM, 2021, no. 1 (95), paper no. 9. Available at: http://www.viam-works.ru (accessed: August 16, 2021). DOI: 10.18577/2307-6046-2021-0-1-85-96.
  8. Kudryavtseva A.N., Tkachuk A.I., Grigorieva K.N., Gurevich Ya.M. The use of epoxy resin system VSE-30, processed by the infusion technology, for the manufacture of low and medium loaded structural polymer composite materials. Trudy VIAM, 2019, no. 1 (73), paper no. 04. Available at: http://www.viam-works.ru (accessed: August 20, 2021). DOI: 10.18577/2307-6046-2019-0-1-31-39.
  9. Doneckij K.I., Karavaev R.Yu., Raskutin A.E., Panina N.N. Properties of carbon fiber and fiberglass on the basis of braiding preforms. Aviacionnye materialy i tehnologii, 2016, no. 4 (45), pp. 54–59. DOI: 10.18577/2071-9140-2016-0-4-54-59.
  10. Belinis P.G., Donetskiy K.I., Lukyanenko Yu.V., Rogozhnikov V.N., Mayer Yu., Bystrikova D.V. Volume reinforcing solid-woven preforms for manufacturing of polymer composite materials (review). Aviacionnye materialy i tehnologii, 2019, no. 4 (57), pp. 18–26. DOI: 10.18577/2071-9140-2019-0-4-18-26.
  11. Gusev Yu.A., Borshhev A.V., Khrulkov A.V. Features of prepregs intended for automated laying by ATL and AFP technologies. Trudy VIAM, 2015, no. 3, paper no. 06. Available at: http://www.viam-works.ru (accessed: August 18, 2021). DOI: 10.18577/2307-6046-2015-0-3-6-6.
  12. Timoshkov P.N., Goncharov V.A., Usacheva M.N., Khrulkov A.V. The development of automated laying: from the beginning to our days (review). Part 1. Automated Tape Laying (ATL). Aviation materials and technologies, 2021, no. 2 (63), paper no. 06. Available at: http://www.journal.viam.ru (accessed: August 17, 2021). DOI: 10.18577/2713-0193-2021-0-2-51-61.
  13. Dushin M.I., Hrulkov A.V., Muhametov R.R. A choice of technological parameters of autoclave formation of details from polymeric composite materials. Aviacionnye materialy i tehnologii, 2011, no. 3, pp.20–26.
  14. Minakov V.T., Postnov V.I., Khulkov A.V., Postnov A.V., Pletin I.I. Peculiarities of gluing PCM parts using polymer equipment. Klei. Germetiki. Tekhnologii, 2008, no. 5, pp. 24–29.
  15. Hrulkov A.V., Dushin M.I., Popov Yu.O., Kogan D.I. Researches and development autoclave and out-of-autoclave technologies of formation of PCM. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 292–301.
  16. Dushin M. I., Hrulkov A.V., Muhametov R.R., Chursova L.V. Features of manufacturing of products from PCM impregnation method under pressure. Aviacionnye materialy i tehnologii, 2012, no. 1, pp. 18–26.
  17. Timoshkov P.N., Usacheva M.N., Khrulkov A.V., Grigorieva L.N. Prospects for the use of polymer composite materials in the manufacture of prostheses (review). Plasticheskiye massy, 2021, no. 5-6. S. 40–43.
  18. Veshkin E.A., Postnov V.I., Postnova M.V., Barannikov A.A. Experience of using vacuum-infusion technologies in the production of structures from PCM. Izvestiya Samarskogo nauchnogo tsentra Rossiyskoy akademii nauk, 2018, vol. 20, no. 4 (3), pp. 344–350.
  19. Timoshkov P.N., Goncharov V.A., Grigoreva L.N., Usacheva M.N., Hrulkov A.V. Robotic laying out of prepregs as an alternative to technology to ATL and AFP (review). Trudy VIAM, 2021, no. 3 (97), paper no. 08. Available at: http://www.viam-works.ru (accessed: August 13, 2021). DOI: 10.18577/2307-6046-2021-0-3-87-98.
  20. Large, high-volume, infused composite structures on the aerospace horizon. Available at: https://www.compositesworld.com/articles/large-high-volume-infused-composite-structures-on-the-aerospace-horizon (accessed: August 18, 2021).
  21. Rajan S., Sutton M.A., Wehbe R. et al. Experimental investigation of prepreg slit tape wrinkling during automated fiber placement process using StereoDIC. Composites. Part B: Engineering, 2019, vol. 160, pp. 546–557.
  22. Boeng 787-8. AirlinesInfo. Available at: https://www.airlines-inform.ru/commercial-aircraft/boeing-787.html (accessed: August 20, 2021).
  23. Yavuz H. Materials Selection for Aircraft Skin Panels by Integrating Multiple Constraints Design with Computational Evaluations. Procedia Structural Integrity, 2019, vol. 21, pp. 112–119.
  24. Thermoplastic composites: Poised to step forward. Composites world: офиц. сайт. Available at: https://www.compositesworld.com/articles/thermoplastic-composites-poised-to-step-forward (accessed: August 20, 2021).
  25. Baker A., Dutton S., Kelly D. Composite materials for aircraft structures. 2nd ed. AIAA, 2004. 602 p.
  26. Chahroudi D. Low cost manufacture of laminar wings. Technical Soaring, 1997, vol. 21, no. 2. P. 55–61.
  27. The spread of spread tow. Available at: https://www.compositesworld.com/articles/the-spread-of-spread-tow (accessed: August 20, 2021).
  28. Update: Lower wing skin, Wing of Tomorrow. Available at: https://www.compositesworld.com/articles/update-lower-wing-skin-wing-of-tomorrow (accessed: August 20, 2021).