Materials based on phenolformaldehyde oligomers of resol and novolac tipes (review)
Part 2
Zastrogina O.B., Sinyakov S.D., Serkova E.A. Materials based on phenolformaldehyde oligomers of resol and novolac tipes (review). Part 2 // Proceedings of VIAM. 2021. No. 11. DOI: 10.18577/2307-6046-2021-0-11-55-65. URL: https://viam-works.ru/en/journal/2021/11/6
Keywords
phenol-formaldehyde binders, resole-type resin, novolac-type resin, foam plastic, laminated plastic, vulcanization, sealing.
Abstract
Describes compositions based on a mixture of phenol-formaldehyde oligomers of the resole and novolac types, used to create foams, laminated plastics for electrical purposes, friction materials, press compositions, sealing putties, as well as for vulcanization of rubbers. Detailed information on the composition and physicochemical properties of the compositions and their technological characteristics are given. The main advantages of resole-novolac materials are shown: strength, heat resistance, reduced flammability, low moisture absorption, good dielectric properties.
Reference list
- Kablov E.N. Marketing Materials Science, Aircraft and Industry: Present and Future. Direktor po marketingu i sbytu, 2017, no. 5-6, pp. 40–44.
- Kablov E.N. The materials of the new generation are the basis of innovation, technological leadership and national security of Russia. Intellekt i tekhnologii, 2016, no. 2, pp. 16–22.
- Raskutin A.E. Development strategy of polymer composite materials. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 344–348. DOI: 10.18577/2071-9140-2017-0-S-344-348.
- Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Raskutin A.E. Russian polymer composite materials of new generation, their exploitation and implementation in advanced developed constructions. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 349–367. DOI: 10.18577/2071-9140-2017-0-S-349-367.
- Mukhametov R.R., Petrova A.P. Thermosetting binders for polymer composites (review). Aviacionnye materialy i tehnologii, 2019, no. 3 (56), pp. 48–58. DOI: 10.18577/2071-9140-2019-0-3-48-58.
- Tkachuk A.I., Donetsky K.I., Terekhov I.V., Kara-vaev R.Yu. The use of thermosetting matrices for the manufacture of polymer composite materials by the non-autoclave molding methods. Aviation materials and technology, 2021. no. 1 (62). paper no. 03. Available at: https://journal.viam.ru (accessed: June 15, 2021). DOI: 10.18577/2713-0193-2021-0-1-22-23.
- Pilato. L. Phenolic resins: A century of progress. Springer, 2010. 545 p.
- Gardziella A., Pilato L.A., Knop A. Phenolic resins: chemistry, applications, standardization, safety and ecology. 2nd completely rev. Springer, 2000. 562 p.
- Knop A., Pilato L. Phenolic resins. Springer, 1985. 315 p.
- Knop A., Shab V. Phenolic resin and materials based on them. Trans. from Engl. Moscow: Khimiya, 1983, 280 p.
- Martin R.V. Chemistry of phenolic resins. Trans. from Engl. Moscow: NIIPM, 1962, 168 p.
- Encyclopedia of polymers. Ed. V.A. Kabanov. Moscow: Sovetskaya Entsyklopedia, 1977, vol. 3, pp. 710–720.
- Losev I.P., Trostyanskaya E.B. Chemistry of synthetic polymers. Ed. 3rd. Moscow: Khimiya, 1971, 616 p.
- Technology of plastics. Ed. V.V. Korshak. Moscow: Khimiya, 1972, 616 p.
- Method for producing polystyrene: pat. 333844 USSR. No. 1440024/23-5; filed 04.06.70; publ. 25.05.76.
- A method of producing foams based on liquid novolac phenol-formaldehyde resin: pat. 335966 USSR. No. 1453094/23-05; filed 06.07.70; publ. 15.05.84.
- A method of producing foams based on liquid resole phenol-formaldehyde resin: pat. 448744 USSR. No. 1436621/23-5; filed 08.06.70; publ. 23.06.85.
- A method of producing foams based on liquid phenol-formaldehyde oligomers of the novolach type: pat. 448745 USSR. No. 1445873/23-05; filed 08.06.70; publ. 30.10.84.
- Composition for obtaining foam: pat. 548037 USSR. No. 1965061/23-05; filed 08.10.73; publ. 15.05.84.
- A method of producing foam: pat. 519442 USSR. No. 1734328/05; filed 04.01.72; publ. 30.06.76.
- Valgin V.D. Domestic energy-saving technology of thermal insulation of building structures using a new generation of foam. Energobezopasnost v dokumenty i faktakh, 2005, no. 1, pp. 20–26.
- Valgin V.D. Data for the design of production of thermal insulation of building structures using a new generation of foam. Energobezopasnost v dokumenty i faktakh, 2005, no. 4, pp. 22–28.
- Catalyst for obtaining phenol-formaldehyde foam and composition for obtaining phenol-formaldehyde foam: pat. 2451550 Ros. Federation. No. 2010139112/04; filed 23.09.10; publ. 27.05.12.
- Composition for producing foam: pat. 2477734 Rus. Federation. No. 2011141873/05; filed 17.10.11; publ. 20.03.13.
- Polymer molding composition: pat. 1733445 USSR. No. 4811128/05; filed 02.21.90; publ. 15.05.92.
- Polymer composition: pat. 2100390 Rus. Federation. No. 95121369/04; filed 19.12.95; publ. 27.12.97.
- Binder based on synthetic oligomers for fiberglass for electrical purposes: pat. 2320039 Rus. Federation. No. 2006130494/09; filed 08.24.06; publ. 20.03.08.
- Composition for the manufacture of a compacting composition:pat. 2198189 Rus. Federation. No. 2000116777/04; filed 29.06.00; publ. 10.02.03.
- Frictional composition: pat. 2101305 Rus. Federation. No. 64036316/04; filed 28.09.94; publ. 10.01.98.
- Frictional composition: pat. 2298707 Rus. Federation. No. 2005130672/11; filed 04.10.05; publ. 10.05.07.
- Polymer press composition: pat. 1016335 USSR. No. 3372956/23-05; filed 29.12.81; publ. 07.05.83.
- Phenol-formaldehyde putty: pat. 1735336 USSR. No. 4804951/05; filed 31.01.90; publ. 23.05.92.
- Adhesive underlayer for attaching rubbers to metal during vulcanization: pat. 2637239 Rus. Federation. No. 2016132657; filed 08.08.16; publ. 01.12.17.