Features of repair of welded structures of large thicknesses from titanium alloy VT6ch.

Sviridov A.V., Gribkov М.S.
Sviridov A.V., Gribkov М.S. Features of repair of welded structures of large thicknesses from titanium alloy VT6ch. // Proceedings of VIAM. 2021. No. 11. DOI: 10.18577/2307-6046-2021-0-11-34-43. URL: https://viam-works.ru/en/journal/2021/11/4
Keywords
electron beam welding, welding parameters, structure, mechanical properties, repair of welded joints, heat treatment.
Abstract

The technology of electron-beam welding (EBW) of structures of large thickness made of titanium alloy Ti–6Al–4V has been developed. A complex of metallographic studies of welded samples has been carried out. Tests to determine the mechanical characteristics of repair welded joints, that these joints made by EBW are equal in strength to the base material. The analysis of the level of residual stresses in various parts of the welded joint after repeated repair passes has been carried out. It was found that the subsequent vacuum annealing reduces the level of residual stresses in welded joints to 50 %. The analysis of the elemental composition showed that the elemental composition of the samples from the center of the weld to the base metal practically does not change for welding with the number of repeated passes up to 3.

Reference list
  1. Kablov E.N., Lukin V.I. Intermetallic compounds based on titanium and nickel for new technology products. Avtomaticheskaya svarka, 2008, no. 11, pp. 76–82.
  2. Kablov E.N., Kashapov O.S., Medvedev P.N., Pavlova T.V. Study of a α+β-titanium alloy based on a system of Ti–Al–Sn–Zr–Si–β-stabilizing alloying elements. Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 30–37. DOI: 10.18577/2071-9140-2020-0-1-30-37.
  3. Panteleev M.D., Bakradze M.M., Skupov A.A., Scherbakov A.V., Belozor V.E. Technological features of fusion welding of aluminum alloy V-1579. Aviacionnye materialy i tehnologii, 2018, no. 3 (52), pp. 11–17. DOI: 10.18577/2071-9140-2018-0-3-11-17.
  4. Skupov A.A., Panteleev M.D., Ioda E.N., Movenko D.A. The efficiency of rare earth metals for filler materials alloying. Aviacionnye materialy i tehnologii, 2017, no. 3 (48), pp. 14–19. DOI: 10.18577/2071-9140-2017-0-3-14-19.
  5. Kablov E.N., Lukin V.I., Ospennikova O.G. Welding and brazing in the aerospace industry. All-Rus. scientific-practical conf. "Welding and safety". Yakutsk, 2012. pp. 21–30.
  6. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  7. Nochovnaya N.A., Panin P.V. Residual Macrostress Analysis in Welded Junctions of Different Titanium Alloys. Trudy VIAM, 2014, no. 05, paper no. 02. Available at: http://www.viam-works.ru. (accessed: April 20, 2021). DOI: 10.18577/2307-6046-2014-0-5-2-2.
  8. Nochovnaya N.A., Panin P.V., Kochetkov A.S., Bokov K.A. VIAM experience in the field of development and research of economically alloyed titanium alloys of new generation. Trudy VIAM, 2016, no. 9, paper no. 05. Available at: http://www.viam-works.ru (accessed: March 2, 2021). DOI: 10.18577/2307-6046-2014-0-9-5-5.
  9. Tarasov Yu.M., Antipov V.V. The VIAM new materials – for perspective aviation engineering of production of JSC «OAK». Aviacionnye materialy i tehnologii, 2012, no. 2, pp. 5–6.
  10. Frolov V.A. Technology of fusion welding and thermal cutting of metals: textbook. Moscow: Alpha; Infra-M, 2011, 477 p.
  11. Lyasotskaya V.S. Heat treatment of welded joints of titanium alloys. Moscow: Ecomet, 2003, 352 p.
  12. Kablov E.N., Lukin V.I., Ospennikova O.G. Welding and brazing in the aerospace industry. All-Rus. scientific-practical conf. "Welding and Safety". Yakutsk, 2012. pp. 21–30.
  13. Zolotorevsky BB, Shubladze T.G., Tikhonova A.F. Residual stresses and deformations in welded joints of titanium alloy VT6. Svarochnoye proizvodstvo, 1982, no. 1, pp. 23–25.
  14. Martynov V.N., Khokhlovsky A.S., Sliva A.P. Electron beam welding of steels, aluminum and titanium alloys of great thickness. Svarochnoye proizvodstvo, 2009, no. 12, pp. 20–24.
  15. Nikolaev G.A. Welding in mechanical engineering: in 4 vols. Moscow: Mashinostroenie, 1978, vol. 3, pp. 85–89.
  16. Goncharov A.L., Sliva A.P., Portnov M.A., Terentyev E.V., Gribkov M.S. Investigation of welded joints of dissimilar steels of magnetic circuit parts made by ELW. Vestnik PNIPU. Mashinostroyenie, materialovedenie, 2013, vol. 15, no. 4, pp. 74–87.
  17. Nazarenko O.K., Kaidalov A.A., Kovbasenko S.N. et al. Electron beam welding. Ed. B.E. Paton. Kiev: Naukova Dumka, 1987, 256 p.
  18. Elkin V.N., Makarov S.V., Panfilov A.P. et al. Experience of electron-beam welding of large-sized products from titanium alloys. Materials and reports Intern. conf. "Electron beam welding and related technologies". Moscow, 2015, pp. 450–458.
  19. Terentyev E.V. Improving the quality of formation of welded joints in electron beam welding of fixed joints with through penetration: thesis abstracts, Cand. Sc. (Tech.). Moscow: MGTU im. N.E. Bauman, 2014, pp. 26–29.
  20. Terentyev E.V., Dragunov V.K., Sliva A.P., Shcherbakov A.V. Influence of welding speed on weld formation in EBW with through penetration. Svarochnoe proizvodstvo, 2014, no. 2, pp. 25–29.
  21. Dragunov V.K., Terentyev E.V., Sliva A.P., Goncharov A.L., Marchenkov A.Yu. Determination of welding speed with EBW of large thicknesses with through penetration. Svarochnoe proizvodstvo, 2016, no. 4, pp. 20–25.
  22. Gerasimenko A.V., Magnitov V.S., Shlyaev Yu.N. Electron beam welding of complex section parts. Elektronno-luchevaya svarka v sudovom mashinostroyenii, 1987, pp. 58–59.
  23. Solomatin V.E., Novosalov T.M. Experience in using the X-ray method for determining residual stresses in welded joints. Avtomaticheskaya svarka, 1982, no. 2, pp. 23–28.