Effect of modifying zirconium oxide additive on the properties of ceramic materials of the Y2O3–Al2O3–SiO2 system obtained by the sol-gel method

Lebedeva Yu.E., Shchegoleva N.E., Voronov V.A., Kovaleva V.S., Chaynikova A.S.
Lebedeva Yu.E., Shchegoleva N.E., Voronov V.A., Kovaleva V.S., Chaynikova A.S. Effect of modifying zirconium oxide additive on the properties of ceramic materials of the Y2O3–Al2O3–SiO2 system obtained by the sol-gel method // Proceedings of VIAM. 2021. No. 10. DOI: 10.18577/2307-6046-2021-0-10-67-78. URL: https://viam-works.ru/en/journal/2021/10/7
Keywords
yttrium aluminosilicate system, zirconium oxide, ceramic materials, coatings, sintering, sol-gel method.
Abstract

The effect of the modifying additive ZrO2 on the rheological properties, the processes of structure and phase formation of the compositions of the Y2O3–Al2O3–SiO2 system obtained by the sol-gel method has been investigated. It was found that the temperature range of crystallization of the compositions of the Y2O3–Al2O3–SiO2 system with the addition of ZrO2 is 1020–1270 °C and with an increase in the concentration of zirconium oxide, the amount of the main crystalline phase of yttrium pyrosilicate (β-Y2Si2O7) decreases and the concentration of the zirconium-containing phase – the tetragonal modification of zirconium oxide and zirconium silicate ZrSiO4 -increases. 

Reference list
  1. Kablov E.N. New generation materials – the basis of innovation, technological leadership and national security of Russia. Intellekt i tekhnologii, 2016, no. 2 (14), pp. 16–21.
  2. Grashchenkov D.V. Strategy of development of non-metallic materials, metal composite materials and heat-shielding. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 264–271. DOI: 10.18577/2071-9140-2017-0-S-264-271.
  3. Evdokimov S.A., Shchegoleva N.E., Sorokin O.Yu. Ceramic materials aviation engineering (review). Trudy VIAM, 2018, no. 12 (72), paper no. 06. Available at: http://www.viam-works.ru (accessed: July 7, 2021). DOI: 10.18577/2307-6046-2018-0-12-54-61.
  4. Kablov E.N., Grashchenkov D.V., Shchegoleva N.E., Orlova L.A., Suzdaltsev E.I. Radiotransparent glass ceramics based on strontium aluminosilicate glass. Ogneupory i tekhnicheskaya keramika, 2016, no. 6, pp. 31–38.
  5. Evdokimov S.A., Solntsev S.St., Yermakova G.V., Davletchin D.I. High-temperature protective coating for C–C composite materials. Aviacionnye materialy i tehnologii, 2016, no. 3 (42), pp. 82–87. DOI: 10.18577/2071-9140-2016-0-3-82-87.
  6. Simonenko E.P., Simonenko N.P., Sevastianov V.G., Grashchenkov D.V., Kuznetsov N.T., Kablov E.N. Functionally gradient composite material SiC / (ZrO2 – HfO2 – Y2O3) obtained using the sol-gel method. Kompozity i nanostruktury, 2011, no. 4, pp. 52–64.
  7. Aparacio M., Duran A. Yttrium silicate Coatings for Oxidation Protection of Carbon-silicon Carbide Composites. Journal of American Ceramic Society, 2000, vol. 83, no. 6, pp. 1351–1355.
  8. Sun L., Shi X., Liu X., Fang J., Liu C., Zhang J. Joining of Cf/SiC composites and Si3N4 ceramic with Y2O3–Al2O3–SiO2 glass filler for high-temperature applications. Ceramic International, 2021, vol. 47, no. 11, pp. 15622–15630.
  9. Atkinson A., Segal D.L. Some Recent Developments in Aqueous Sol-Gel Processing. Journal of Sol-Gel Science and Technology, 1998, no. 13, pp. 133–139.
  10. Wang L., Fan S., Sun H. et al. Pressure-less joining of SiCf/SiC composites by Y2O3–Al2O3–SiO2 glass: Microstructure and properties. Ceramic International, 2020, vol. 46, no. 17, pp. 27046–27056.
  11. Zhou L., Huang J., Cao L. et al. A novel design of oxidation protective β-Y2Si2O7 nanowire toughened Y2SiO5/Y2O3–Al2O3–SiO2 glass ceramic coating for SiC coated carbon/carbon composites. Corrosion Science, 2018, vol. 135, pp. 233–242.
  12. Voronov Vs.A., Lebedeva Yu.E., Sorokin O.Yu., Vaganova M.L. Investigation of the high-temperature coatings properties on the basis of an yttrium-alumosilicate system for the protection of SiC materials from the action of an oxidizing environment. Aviacionnye materialy i tehnologii, 2018, no. 4 (53), pp. 63–73. DOI: 10.18577/2071-9140-2018-0-4-63-73.
  13. Simonenko E.P., Simonenko N.P., Kopitsa G.P., Almasy L., Gorobtsov F.Yu., Sevastyanov V.G., Kuznetsov N.T. Evolution during heat treatment of the mesostructure of highly dispersed Y3Al5O12 obtained by the sol-gel method. Zhurnal neorganicheskoy khimii, 2018, vol. 63, no. 6, pp. 661–669.
  14. Simonenko N.P., Simonenko E.P., Sevastyanov V.G., Kuznetsov N.T. Preparation of Nanostructured Thin Films of Yttrium Aluminum Garnet (Y3Al5O12) by Sol-Gel Technology. Russian Journal of Inorganic Chemistry, 2016, vol. 61, no. 6, pp. 667–673.
  15. Mackenzie J.D. Sol-Gel Research-Achievements Since 1981 and Prospects for the Future. Journal of Sol-Gel Science and Technology, 2003, no. 26, pp. 23–27.
  16. Zarzyki J. Past and Present of Sol-Gel Science and Technology. Journal of Sol-Gel Science and Technology, 1997, no. 8, pp. 17–22.
  17. Sainz М.A., Osendi M.I., Miranzo P. Protective Si–Al–O–Y glass coatings on stainless steel in situ prepared by combustion flame spraying. Surface & Coatings Technology, 2008, no. 202, pp. 1712–1717.
  18. Harrysson R., Vomacka P. Glass formation in the system Y2O3–Аl2О3–SiO2 under conditions of laser melting. Journal of the European Ceramic Society, 1994, no. 14, pp. 377–382.
  19. Kolitsch U., Seifert H.J., Ludwig T., Aldinger F. Phase equilibria and crystal chemistry in the Y2O3–Аl2О3–SiO2 system. Journal of Materials Research, 1999, vol. 14, no. 2, pp. 447–455.
  20. Nasiri N.A., Patra N., Horlait D. et al. Thermal properties of rare-earth monosilicates for EBC on Si-based ceramic composites. Journal of American Ceramic Society, 2016, vol. 99, pp. 589–596.
  21. Kolitsch U., Seifert H.J., Ludwig T., Aldinger F. Phase equilibria and crystal chemistry in the Y2O3–Аl2О3–SiO2 system. Journal of Materials Research, 1999, vol. 14. no. 2, pp. 447–455.
  22. Fernandez-Carrion A.J., Allix M., Becerro A.I. Thermal expansion of rare-earth pyrosilicates. Journal of American Ceramic Society, 2013, vol. 96, pp. 2298–2305.
  23. Lebedeva Yu.E., Grashhenkov D.V., Popovich N.V., Orlova L.A., Chajnikova A.S. Development and research of the thermostable coverings, received sol-gel method in Y2O3–Al2O3–SiO2system, for SiC-containing materials. Trudy VIAM, no. 12, paper no. 03. Available at: http://www.viam-works.ru (accessed: July 7, 2021).
  24. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.