Valevin E.O., Startsev V.O., Zelenina I.V. Thermal aging, surface degradation and water transfer in carbon fiber reinforced plastic VKU-38TR // Proceedings of VIAM. 2020. No. 6-7 (89). Ст. 12. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2020-0-67-118-128.
Thermal aging, surface degradation and water transfer in carbon fiber reinforced plastic VKU-38TR
Abstract
Using the methods of thermogravimetry, analysis of 3D images of the surface topography and kinetics of moisture transfer, the mechanism of thermal aging and physicochemical transformations under the influence of elevated temperatures in carbon fiber reinforced plastic VKU-38TR is studied. According to the results of profilometry, it was proved that the degree of destruction of the surface layer of the studied carbon fiber reinforced plastic depends on the duration of exposure to the operating temperature and its value. The significant effect of thermal aging on the moisture absorption of carbon fiber reinforced plastic is shown.
Keywords
thermal aging, carbon fiber reinforced plastic, surface topography, thermal oxidative degradation, strength, moisture diffusion coefficient.
Reference list
- Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Kablov E.N. The strategic directions of development of materials and technologies of their processing for the period to 2030. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 7–17.
- Kablov E.N., Chursova L.V., Babin A.N., Mukhametov R.R., Panina N.N. Development of FSUE «VIAM» in the field of melt binders for polymer composite materials. Polimernye materialy i tekhnologii, 2016, vol. 2, no. 2, pp. 37–42.
- Raskutin A.E. Russian polymer composite materials of new generation, their exploitation and implementation in advanced developed constructions. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 349–367. DOI: 10.18577/2071-9140-2017-0-S-349-367.
- Zelenina I.V., Gulyaev I.N., Kucherovsky A.I., Mukhametov R.R. Features of the manufacture of heat-resistant carbon plastics and products made from them. Konstruktsii iz kompozitsionnykh materialov, 2016, no. 1, pp. 34–40.
- Gulyaev I.N. VIAM experience in the development of high-temperature PCM. Polymer composite materials and production technologies of a new generation: materials III All-Russian. scientific and technical conf. (Moscow, November 29, 2018). Moscow: VIAM, 2018, pp. 27–36.
- Mikhailin Yu.A. Structural polymer composite materials. Saint Petersburg: Nauchnye osnovy i tekhnologii, 2008, 822 p.
- Trostyanskaya E.B., Mikhailin Yu.A., Khokhlova L.F. et al. Carbon plastics based on polymerizing imides API-2. Voprosy aviatsionnoy nauki i tekhniki. Ser.: Aviatsionnye materialy. Moscow: VIAM, 1985, pp. 12–19.
- Domingues D.D., Jones H.N., Keller T.M. The effect of curing additive on the mechanical properties of phthalonitrile-carbon fiber composites. Polymer Composites, 2004, vol. 25, no. Five, pp. 554–561.
- Keller T.M., Dominguez D.D. High temperature resorcinol-based phthalonitrile polymer. Polymer, 2005, vol. 46, no. 13, pp. 4614–4618.
- Mikhailin Yu.A. Heat-resistant polymers and polymer materials. Saint Petersburg: Professiya, 2006, 624 p.
- Mukhametov R.R., Akhmadieva K.R., Chursova L.V. New heat-resistant heterocyclic binders and environmentally friendly technologies for obtaining composite materials. Rossiyskiy khimicheskiy zhurnal, 2010, vol. 54, no. 1, pp. 57–62.
- Sastri S.B., Keller T.M. Phthalonitrile cure reaction with aromatic diamines. Journal of Polymer Science, part A: Polymer Chemistry, 1998, vol. 36, pp. 1885–1890.
- Keller T.M. Phthalonitrile-based high temperature resin. Journal of Polymer Science, part A: Polymer Chemistry, 1988, vol. 26, pp. 3199–3212.
- Sastri S.B., Armistead J.P., Keller T.M., Sorathia U. Phtalonitrile-glass fabric composites. Polymer Composites, 1997, vol. 18, no. 1, pp. 816–822.
- Sastri S.B., Armistead J.P., Keller T.M. Phtalonitrile-carbon fiber composites. Polymer Composites, 1996, vol. 17, no. 6, pp. 816–822.
- Startsev V.O. Climatic resistance of polymer composite materials and protective coatings in a moderately warm climate: thesis, Dr. sc. (Tech.). Moscow: VIAM, 2018, 308 p.
- Slavin A.V., Startsev O.V. Properties of aircraft glass- and carbonfibers reinforced plastics at the early stage of natural weathering. Trudy VIAM, 2018, no. 9 (69), paper no. 8. Available at: http://www.viam-works.ru (accessed: January 17, 2020). DOI: 10.18577 / 2307-6046-2018-0-9-71-82.
- Startsev O.V., Filistovich D.V., Kuznetsov A.A. Deformability of sheet glass-reinforced plastics based on adhesive prepregs under shear loads in a humid environment. Perspektivnyye materialy, 2004, no. 1, pp. 20–26.
- Kablov E.N., Startsev V.O. Climatic aging of polymer composite materials for aviation. I. Assessment of the influence of significant impact factors. Deformatsiya i razrusheniye materialov, 2019, no. 12, pp. 7–16.
- Kablov E.N., Startsev V.O. Climatic aging of polymer composite materials for aviation. II. Development of research methods for the early stages of aging. Deformatsiya i razrusheniye materialov, 2020, no. 1, pp. 15–21.
- Kirillov V.N., Efimov V.A. Problems of research of climatic resistance of aircraft non-metallic materials. 75 years. Aviation materials. Selected works of «VIAM». Moscow: VIAM, 2007, p. 379–388.
- Startseva L.T., Panin S.V., Startsev O.V., Krotov A.S. Moisture diffusion in glass-fiber-reinforced plastics after their climatic aging. Doklady Physical Chemistry, 2014, vol. 456, no. 1, pp. 77–81.
- Panin S.V., Startsev O.V., Krotov A.S. Initial stage environmental degradation of the polymer matrix composites evaluated by Water diffusion coefficient. Trudy VIAM, 2014, no. 7, paper no. 09. Available at: http://viam-works.ru (accessed: January 17, 2020). DOI: 10.18577/2307-6046-2014-0-7-9-9.
- Panin S.V. Study of changes in surface relief and moisture transfer in polymer composite materials during climatic aging: thesis, Cand. Sc. (Tech.). Moscow: VIAM, 2015, 131 p.
- Valevin E.O. Influence of heat and humidity impact on the properties of heat-resistant polymer composite materials based on phthalonitrile matrix: thesis, Cand. Sc. (Tech.). Moscow: MAI, 2018, 130 p.
- Kablov E.N., Startsev V.O. Systematical analysis of the climatics influence on mechanical properties of the polymer composite materials based on domestic and foreign sources (review). Aviacionnye materialy i tehnologii, 2018, no. 2 (51), pp. 47–58. DOI: 10.18577/2071-9140-2018-0-2-47-58.
- Bulmanis V.N., Startsev O.V. Prediction of changes in the strength of polymer fiber composites as a result of climatic effects. Yakutsk: Yakutsk Branch SB AS USSR; Institute of Physical and Technical Problems of the North, 1988, 32 p.
- Vapirov Yu.M., Krivonos V.V., Startsev O.V. Interpretation of the anomalous change in the properties of carbon-fiber-reinforced plastic KMU-1u during aging in different climatic regions. Mechanics of Composite Materials, 1994, vol. 30, no. 2, pp. 190–194.
- Nikolaev E.V., Kirillov V.N., Skirta A.A., Grashhenkov D.V. Study of moisture transport rules and development of a standard on measurement of the diffusion coefficient and moisture content limit to evaluate mechanical properties of carbon fiber reinforced plastics. Aviacionnye materialy i tehnologii, 2013, no. 3, pp. 44–48.
- Startsev O.V., Sortyakov E.D., Isupov V.V. et al. Acoustic spectroscopy of polymer composite materials exposed in open space. Experimental methods in the physics of structurally inhomogeneous media: Proceedings of the All-Russian. scientific and technical conf. Barnaul: ASU Publishing House, 1997, pp. 32–39.
- Issoupov V.V., Krotov A.S., Startsev O.V. et al. Moisture diffusion properties of carbon / epoxy and glass / epoxy composite materials after exposure to low earth orbit space environment. Water Transport in Synthetic Polymers. New York, 2003, pp. 179–189.
- Kablov E.N., Startsev O.V., Deev I.S., Nikishin E.F. Properties of polymer composite materials after exposure to outer space in near-earth orbits. Vse materialy. Entsiklopedicheskiy spravochnik, 2012, no. 11, pp. 2–16.
- Gulyaev I.N., Zelenina I.V., Valevin E.O., Shvedkova A.K. Investigation of the influence of elevated temperature and humidity on the properties of heat-resistant carbon plastics. Konstruktsii iz kompozitsionnykh materialov, 2015, no. 3 (139), pp. 55–61.