Abstract

A review of our own country and foreign papers in the field of high temperature metal matrix composite materials was conducted in this work. A classification of composite materials was considered. Main types of structures and characteristic properties were described. Matrix metals and alloys for obtaining high temperature composite materials were reviewed. Iron-and nickel-based composites and refractory metals and their compounds are considered in separate groups. Prospects for further research in the field of high-temperature composite materials were identified – for example, the use of composites in additive manufacturing.

Reference list
  1. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N., Svetlov I.L., Neiman A.V., Min P.G., Karachevtsev F.N., Karpov M.I. High-temperature composites based on the Nb–Si system reinforced with niobium silicides. Inorganic Materials: Applied Research, 2017, vol. 8, no. 4, pp. 609–617.
  3. Kablov E.N., Bondarenko Yu.A., Echin A.B. Development of technology of cast superalloys directional solidification with variable controlled temperature gradient. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 24–38. DOI: 10.18577/2071-9140-2017-0-S-24-38.
  4. Kablov E.N. What to make the future of? New generation materials, technologies for their creation and processing – the basis of innovations. Krylya Rodiny, 2016, no. 5, pp. 8–18.
  5. Portnoy K.I., Babich B.N. Advances in modern metal science. Moscow: Metallurgiya, 1974, 200 p.
  6. Kostikov V.I., Varenkov A.N. Ultra-high-temperature composite materials. Moscow: Intermet Inzhiniring, 2003, 506 p.
  7. Portnoy K.I., Salibekov S.E., Svetlov I.L., Chubarov V.M. Structure and properties of composite materials. Moscow: Mashinostroyenie, 1979, 255 p.
  8. Structural applications of mechanical alloying. Proceedings of an ASM International Conference, 1990, 320 p.
  9. Campbell F.C. Manufacturing Technology for Aerospace Structural Materials. Amsterdam: Elsevier, 2006, 616 p. DOI: 10.1016/B978-1-85617-495-4.X5000-8.
  10. Shallman R.E., Bishop R.J. Modern Alloy Developments. Modern Physical Metallurgy and Materials Engineering. 6th ed. Oxford: Butterworth-Heinemann, 1999, pp. 305–308. Available at: http://www.sciencedirect.com/science/article/pii/B9780750645645500094 (accessed: May 12, 2020).
  11. Svensson D.O. High Entropy Alloys: Breakthrough Materials for Aero Engine Applications?: diploma work. Gothenburg: Chalmers University of Technology, 2014. 70 p.
  12. Schafrik R.E., Ward D.D., Groh J.R. Application of alloy 718 in GE aircraft engines: past, present and next five years. 2001. Available at http://www.tms.org/superalloys/10.7449/2001/superalloys_ 2001_1_11.pdf (accessed: May 12, 2020).
  13. Williams J.C., Starke Jr. E.A. Progress in structural materials for aerospace systems. Acta Materialia, 2003, vol. 51 (19). P. 5775–5799. Available at http://www.sciencedirect.com/science/ article/pii/S1359645403005020 (accessed: May 12, 2020).
  14. Muktinutalapati N.R. Materials for gas turbines – an overview. Advances in Gas Turbine Technology. Available at: http://cdn.intechopen.com/pdfs-wm/22905.pdf (accessed: May 12, 2020).
  15. Group R.W. Turbine blade metallurgy. 2014. Available at: http://www.rwgroup.com/index/turbine-blade-metallurgy (accessed: May 12, 2020).
  16. Pollock T.M., Tin S. Nickel-based superalloys for advanced turbine engines: chemistry, microstructure and properties. Journal of propulsion and power, 2006, vol. 22 (2). P. 361–374. Available at: http://arc.aiaa.org/doi/abs/10.2514/1.18239 (accessed: May 12, 2020).
  17. MacKay R., Gabb T., Smialek J., Nathal M. A new approach of designing superalloys for low density. Journal of The Minerals, 2010, vol. 62 (1), p. 48–54. DOI: 10.1007/s11837-010-0011-0.
  18. Caron P., Khan T. Evolution of Ni-based superalloys for single crystal gas turbine blade applications. Aerospace Science and Technology, 1999, vol. 3 (8), pp. 513–523.
  19. Lasalmonie A. Intermetallics: Why is it so difficult to introduce them in gas turbine engines? Intermetallics. 2006, vol. 14 (10–11), pp. 1123–1129. Available at: http://www.sciencedirect.com/science/article/pii/S0966979506000835 (accessed: May 12, 2020).
  20. Emelyanov V.S., Evstyukhin A.I., Shulepov V.I. et al. Molybdenum in nuclear power. Moscow: Atomizdat, 1977, 160 p.
  21. Batienkov R.V., Efimochkin I.Yu., Kolyshev S.G., Khudnev A.A. The effect of heat treatment on the structure and mechanical properties of an alloy of the Mo–Ti–Zr–C system obtained by electric pulse plasma sintering. Trudy VIAM, 2020, no. 4–5 (88), paper no. 01. Available at: http://www.viam-works.ru (accessed: June 1, 2020). DOI: 10.18577/2307-6046-2020-0-45-3-12.
  22. Ershova I.O. Physical and mechanical properties of industrial refractory alloys. Tsvetnye metally, 1997, no. 7, pp. 49–54.
  23. Ershova I.O., Manegin Yu.V. Refractory powder materials for high-temperature technology. Tsvetnye metally, 1998, no. 3, pp. 36–39.
  24. Ershova I.O., Fedotenkova O.B. Influence of the modes of extrusion and annealing on the mechanical properties of powder alloys of the Mo–Zr–B system. Materialovedeniye i termicheskaya obrabotka metallov, 2000, no. 7, pp. 13–19.
  25. Ershova I.O. Influence of nitrides of refractory metals on the properties of sintered tungsten and molybdenum. Materialovedeniye i termicheskaya obrabotka metallov, 2003, no. 2, pp. 26–30.
  26. Ohser-Wiedemann R., Weck Ch., Martin U. et al. Spark plasma sintering of TiC partical-reinforced molybdenum composites. International Journal Refractory Metals and Hard Materials, 2012, vol. 32, pp. 1–6.
  27. Hu P., Wang K., He H. et al. Preparation and properties of La–TZM alloy plates. Applied Mechanics and Materials, 2013, vol. 320, pp. 350–353.
  28. Wang Y.K., Miao S., Xie Z.M. et al. Thermal stability and mechanical properties of HfС dispersion strengthened W alloys as plasma-facing components in fusion devices. Journal of Nuclear Materials, 2017, vol. 492, pp. 260–268.
  29. Grashchenkov D.V., Shchetanov B.V., Efimochkin I.Yu. Development of powder metallurgy of refractory materials. Vse materialy. Entsiklopedicheskiy spravochnik, 2011, no. 5, pp. 13–26.
  30. Grashchenkov D.V., Shchetanov B.V., Efimochkin I.Yu. Development of powder metallurgy of refractory materials. Vse materialy. Entsiklopedicheskiy spravochnik, 2011, no. 6, pp. 10–22.
  31. Grashchenkov D.V., Shchetanov B.V., Efimochkin I.Yu., Sevostyanov N.V. Composite materials based on refractory metals. Konstruktsii iz kompozitsionnykh materialov, 2016, no. 4, pp. 16–22.
  32. Efimochkin I.Yu., Shchetanov B.V., Paegle S.V., Dvoretskov R.M. Research of peculiarities of mechanical decomposition in synthesis of in-situ composites based on refractory metals. Trudy VIAM, 2018, no. 4 (64), paper no. 05. Available at: http//www.viam-works.ru (accessed: June 1, 2020). DOI: 10.18577/2307-6046-2018-0-4-38-50.
  33. Balasubramanian M. Composite materials and processing. LLC CRC Press, 2014, 648 р.
  34. Kovtunov A.I., Myamin S.V., Semistenova T.V. Layered composite materials. Tolyatti: TSU Publishing House, 2017, 1 CD.
  35. Seemüller H.C.M. Evaluation of Powder Metallurgical Processing Routes for Multi-Component Niobium Silicide-Based High-Temperature Alloys. Materials Science, 2016. DOI: 10.5445/IR/1000054464.
  36. Goulon J.-M. Hybrid Silicide-Based Lightweight Components for Turbine and Energy Applications: Final Report Summary. Available at: https://cordis.europa.eu/project/id/266214 (accessed: 20.10.2019).
  37. Yueling Guo, Lina Jia, Bin Kong et al. Improvement in the oxidation resistance of Nb–Si based alloy by selective laser melting. Corrosion Science, 2017, vol. 127, pp. 1–10.
  38. Dicks R., Wang F., Wu X. The manufacture of a niobium/niobium-silicide-based alloy using direct laser fabrication. Journal of Materials Processing Technology, 2009, vol. 209, pp. 1752–1757. DOI: 10.1016/j.jmatprotec.2008.04.042.