Kolobkov A.S. Polymer composite materials for various aircraft structures (review) // Proceedings of VIAM. 2020. No. 6-7 (89). Ст. 05. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2020-0-67-38-44.
Polymer composite materials for various aircraft structures (review)
Abstract
The article describes the new polymer composite materials developed recently in FSUE «VIAM», which are used in various aviation equipment, using a variety of reinforcing fillers and polymer binders. These developments are associated with the development of a new technological structure, the emergence of new requirements for aviation products and increasing requirements for existing ones, which in turn creates certain requirements for materials. The brands of materials, their application areas and operating temperatures are also presented.
Keywords
carbon fiber, fiberglass, organoplastics, binder, polymer composite materials, high-temperature carbon fiber plastics.
Reference list
- Kablov E.N. The sixth technological order. Nauka i zhizn, 2010, no. 4, pp. 2–7.
- Borshchev A.V., Gusev Yu.A. Polymer composite materials in automotive industry. Aviacionnye materialy i tehnologii, 2014, no. S2, pp. 34–38.
- Kochurov D.V. High-strength polymer composite materials. International student scientific bulletin. 2018, no. 5. Available at: http://eduherald.ru/article/view?id=19200 (accessed: March 20, 2020).
- Bekturov KB, Zaripov R.Yu., Medvedev AS, Kaerbekov D.Z. Prospects for the use of composite materials in freight car building. Nauka i tekhnika Kazakhstana, 2017, no. 1–2, pp. 25–33.
- Molchanov B.I., Gudimov M.M. Properties of carbon plastics and their application. Aviatsionnaya promyshlennost, 1997, no. 3–4, pp. 22–26.
- Kablov E.N. VIAM: new generation materials for PD-14. Krylya Rodiny, 2019, no. 7-8, pp. 54–58.
- Kablov E.N., Chursova L.V., Babin A.N., Mukhametov R.R., Panina N.N. Development of FSUE «VIAM» in the field of melt binders for polymer composite materials. Polimernyye materialy i tekhnologii, 2016, vol. 2, no. 2, pp. 37–42.
- Raskutin A.E. Russian polymer composite materials of new generation, their exploitation and implementation in advanced developed constructions. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 349–367. DOI: 10.18577/2071-9140-2017-0-S-349-367.
- Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Davydova I.F., Kavun N.S. Fibreglasses ‒ multipurpose composite materials. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 253–260.
- Davydova I.F., Kablov E.N., Kavun N.S. Heat-resistant non-combustible polyimide glass fiber laminates for aircraft and rocket technology. Vse materialy. Entsiklopedicheskiy spravochnik, 2009, no. 7, pp. 2–11.
- Aviation regulation 25. Standards of airworthiness of transport category aircraft. 3rd ed. Moscow: Aviaizdat, 2009, 267 p.
- Gunyayeva A.G., Sidorina A.I., Kurnosov A.O., Klimenko O.N. Polymeric composite materials of new generation on the basis of binder VSE-1212 and the filling agents alternative to ones of Porcher Ind. and Toho Tenax. Aviacionnye materialy i tehnologii, 2018, no. 3 (52), pp. 18–26. DOI: 10.18577/2071-9140-2018-0-3-18-26.
- Mishurov K.S., Mishkin S.I. Environmental effect on properties of CFRP (Carbon Fiber Reinforced Plastic) VKU-39. Trudy VIAM, 2016, no. 12 (48), paper no. 08. Available at: http://www.viam-works.ru (accessed: June, 10 2020). DOI: 10.18577/2307-6046-2016-0-12-8-8.
- PD-14: five facts about the new Russian engine. Available at: https://rostec.ru/news/pd-14-pyat-faktov-o-novom-rossiyskom-dvigatele/ (accessed: October 03, 2020).
- Merkulova Yu.I., Muhametov R.R., Dolgova E.V., Ahmadieva K.R. Polycyanurates binding for composites production by impregnation under pressure. Trudy VIAM, 2016, no. 11 (47), paper no. 05. Available at: http://www.viam-works.ru (accessed: April 11, 2020). DOI: 10.18577/2307-6046-2016-0-11-5-5.
- Zelenina I.V., Gulyayev I.N., Kucherovskiy A.I., Mukhametov R.R. Heat-resistant CFRP for the impulse wheel of the centrifugal compressor. Trudy VIAM, 2016, no. 2 (38), paper no. 08. Available at: http://www.viam-works.ru (accessed: April 11, 2020). DOI: 10.18577/2307-6046-2016-0-2-8-8.
- Zhelezina G.F., Voinov S.I., Chernykh T.E., Chernykh K.Yu. New aramid fibers Rusar-NT for reinforcement of structural organoplastics. Voprosy materialovedeniya, 2015, no. 1 (81), pp. 60–72.
- Zhelezina G.F., Gulyaev I.N., Soloveva N.A. Aramide organic plastics of new generation for aviation designs. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 368–378. DOI: 10.18577/2071-9140-2017-0-S-368-378.